This study focused on understanding the effect of various media (such as vacuum, argon and air) on the formation, structure, composition and properties of electrospark coatings deposited on the nickel alloy EP 718-ID (an equivalent of Inconel 718). The ZrB2 — 20% Si electrodes were produced by self-propagating high-temperature synthesis. A hand tool with a vibrating electrode was used to form the coatings in air or argon, whereas the coatings deposited in vacuum were produced with the help of an automatic tool with a rotating electrode. It was established that when electrospark alloying is carried out in vacuum or argon a consistent weight gain is observed on the cathode, and the resultant coatings are uniform and have minimum drawbacks. Coatings deposited in air are associated with eroded substrate material and a high degree of imperfection. The coatings deposited on the nickel alloy have a thickness of 20–25 μm, a hardness of 12.6–18.8 GPa, and a Young modulus of 237.8–351.4 GPa. The roughness of the coatings is 5.8–7.4 μm. The coatings deposited in argon and in vacuum were found to have the maximum hardness and Young modulus. The following compounds dominate in coatings depending on the medium: zirconium diboride ZrB2 for argon, nickel silicide Ni(1 — x)Si(x) and zirconium diboride ZrB2 for vacuum, and zirconium dioxide ZrO2 and nickel silicide Ni(1 — x)Si(x) for air. The coatings deposited in vacuum have the maximum oxidation resistance. It is demonstrated that for quality coatings deposited on nickel alloys the electrode materials Zr–Si–B should be used for ESA in argon or vacuum. This work was carried out with financial support from the Ministry of Education and Science of the Russian Federation in the framework of state assignment No.11.7172.2017/8.9. The authors would like to thank N.V. Shvyndina, T. A. Sviridova, A. N. Sheveiko for their support during the study.
1 September 2019 in Surface Engineering and Applied Electrochemistry
The electrospark deposition of coatings onto SPKhN–60 white cast iron samples has been undertaken in two stages. A barrier sublayer has been deposited at the first stage, using chromium and...
6 September 2022 in Powder Metallurgy аnd Functional Coatings
Protective coatings were applied by electrospark deposition (ESD) using zirconium electrodes to improve the performance of the Ni-containing alloy obtained using the selective laser melting (SLM) technology. The kinetics of mass transfer was studied in 5 different frequency-energy processing modes. An analog-to-digital converter was used to determine the average number of pulse discharges, single-pulse energy, and the total energy of pulse discharges for 1 min of processing (ΣЕ) for all the modes used. In low-energy processing modes (ΣЕ= 1459÷2915 J), a weak mass transfer was observed, and the cathode weight gain was recorded only in the first minutes. As the processing time increased, a decrease in the substrate weight was observed. The roughness of coatings (Ra) varied in the range of 3.9–7.2 μm. In high-energy modes (ΣЕ= 5197÷17212 J), due to intense electrode heating, a steady cathode weight gain was observed, but the formed coatings featured by increased roughness: Ra = 7.4÷8.6 μm. The Ra parameter for the original SLM samples was 10.7 μm. The formed coatings featured by a thickness of 15–30 μm, high continuity (up to 100 %), hardness of 9.0–12.5 GPa, elastic modulus of 122–145 GPa, and friction coefficient of 0.36–0.49. The ESD processing promoted an increase in wear resistance of the SLM alloy by 7.5–20 times, and oxidation resistance by 10–20 % (t = 1150 °C, τ = 30 h). It was found that the coating obtained in the low-energy ESD mode with energy ΣЕ= 2915 J featured the best performance (hardness, modulus of elasticity, roughness, wear resistance and oxidation resistance).
1 July 2019 in Surface Engineering and Applied Electrochemistry
Electrospark deposition on samples made of SPHN-60 white cast iron is carried out in two stages. During the first stage, a barrier sublayer was applied, and during the second stage, a...
1 September 2018 in Surface Engineering and Applied Electrochemistry
Electrospark treatment of OT4-1 titanium alloy was performed sequentially with a STIM-20N hard-alloy electrode (TiC–20% Ni) and carbon-containing material (graphite and carbon-based composite...
9 September 2019 in Bulletin of Bryansk state technical university
At metallurgical enterprises the worn out rollers of BCCM are reduced by means of a surfacing technology. In most cases the rollers of BCCM are made of heat-resistant steel of 20H13 and 25H1M1F grades and others and their reduction is carried out by surfacing with the use of powder wire, for instance PP-Np-25H5FMS. Life increase of the reduced rollers of BCCM twice as many and more is an urgent problem requiring the use of more wear-resistant materials. The paper reports the results of X-ray structural, phase, structural, tribological, thermocyclic investigations directed to the analysis of the possibility in use of ASM 4603-SA filler modified with 3% of refractory components of tungsten carbide (TC) and 0.2% hexagonal boron nitride (BN) for roller reduction of blank continuous casting machines. It is defined that ASM 4603-SA powder wire application with the refractory component addition is promising for roller surfacing reduction in BCCM. As a result of mentioned material electro arc surfacing on the roller surface of BCCM there is formed a wear-resistant layer with hardness up to 57 HRC resistant to a crack formation and burn back grid as a result of cyclic hightemperature impacts characterized with the decreased friction coefficient in comparison with the layer surfaced with the basic material.