The 080A15 and 30CrMnMo steels were cut by precision sawing machine. The microscopic characteristic of the chip surface and the chip failure microscopic mechanism have been studied. The studies show that the formation of saw-tooth chip is mainly a function of the strength and thermal conductivity. For 080A15 steel, the strength is low and the thermal conductivity is high, the plastic work was absorbed continuously by the process of plastic deformation, and the heat was dissipated at any moment. The heat energy did not reach the critical value causing thermal softening. The chip is more prone to ductile fracture. For 30CrMnMo steel, the bonding ability is stronger among atoms, and thermal conductivity is smaller. The plastic deformation is extremely fast and the instantaneous temperature rise was very high because the heat energy reached the critical value causing thermal softening. Therefore, the chip is more prone to adiabatic shear failure to form the saw-tooth chip divided uniformly by adiabatic shear band. The research results help to provide the basis for selecting materials with different adiabatic shearing sensitivities in the process of high-speed cutting by studying the energy barrier on the influence of chip failure mechanism.
13 September 2019 in The International Journal of Advanced Manufacturing Technology
During high-speed cutting, a white layer is often produced on the machined surfaces after mechanical machining, seriously affecting the mechanical properties. These properties are related to the material structure and the defects induced by cutting. However, there is a lack of research on the atomic-scale defects of the white layer. This paper studied the influence of cutting parameters, namely the feed rate, cutting speed and cutting depth, on atomic-scale defects induced by high-speed cutting in GCr15 steel. Positron annihilation studies showed typical plastically deformed or tempered carbon steel defects with additional vacancy cluster components. The quantity of these clusters changed with cutting parameters. Furthermore, significant changes were observed in the subsurface region up to 1 µm, occurring as a result of simultaneous phase transformations, deformation and thermal impacts. The predominant accumulation of only one type of atomic-scale defect was not observed.