In this study, the cationic Poly[Styrene-Butyl acrylate-(P-vinylbenzyl trimethyl ammonium chloride)] P(St-BA-VBT) nanospheres with N+(CH3)3 functional groups were successfully synthesized by soap-free emulsion polymerization and applied to different fabrics by pad-cure process. After the pad-cure process, the nanospheres were deposited on the surface of the modified cotton fibers successfully without forming a continuous film structure. The X-ray Photoelectron Spectroscopy (XPS) and the Fourier transform infrared (FTIR) results demonstrated that P(St-BA-VBT) nanospheres were adsorbed on the surface of cotton fibers successfully. The excellent color strength value and outline sharpness of the plain, twill, and honeycomb fabrics can be achieved when the nanosphere concentration, sodium bicarbonate, and steaming time were 1 g/L, 10 g/L, and 6 min, respectively. The plain fabrics exhibited the smallest color strength (K/S) values and the best outline sharpness, followed by twill and honeycomb fabrics, which displayed the largest K/S values and the worst outline sharpness after the same treatment. Besides, all the three fabrics showed excellent rubbing fastness and washing fastness. The cationic P(St-BA-VBT) nanospheres modification of the cotton fabrics provides a novel potential approach to obtain good printing efficiency without affecting the tensile breaking strength of cotton fabrics significantly.
The Poly[Styrene-Butyl acrylate-(P-vinylbenzyl trimethyl ammonium chloride)] P(St-BA-VBT) nanospheres with N+(CH3)3 functional groups were successfully prepared and applied to modify cotton fabrics using a pad-dry process. The obtained cationic cotton fabrics were dyed with pad-steam dyeing with reactive dye. The results show that the appropriate concentration of nanospheres was 4 g/L. The sodium carbonate of 25 g/L and steaming time of 3 min were suitable for dyeing cationic cotton with 25 g/L of C.I. Reactive Blue 222. The color strength and dye fixation rates of dyed cationic cotton fabrics increased by 39.4% and 14.3% compared with untreated fabrics. Moreover, sodium carbonate and steaming time were reduced by 37.5% and 40%, respectively. The rubbing and washing fastness of dyed fabrics were equal or higher 3 and 4–5 grades, respectively. Scanning electron microscopy (SEM) images revealed that the P(St-BA-VBT) nanospheres randomly distributed and did not form a continuous film on the cationic cotton fiber surfaces. The X-ray photoelectron spectroscopy (XPS) analysis further demonstrated the presence of cationic nanospheres on the fiber surfaces. The cationic modification did not affect the breaking strength of cotton fabrics.