The metallic tantalum powder was successfully synthesized via reduction of tantalum pentoxide (Ta2O5) with magnesium gas at 1073~1223 K for 10 h inside the chamber held under an argon atmosphere. The powder obtained after reduction shows the Ta–MgO mixed structure and that the MgO component was dissolved and removed fully via stirring in a water-based HCl solution. The particle size in the tantalum powder obtained after acid leaching was shown to be in a range of 50~300 nm, and the mean internal crystallite sizes measured by the Scherrer equation varied from 11.5 to 24.7 nm according to the increase in reduction temperatures. The temperature satisfactory for a maximal reduction effect was found to be 1173 K because the oxygen content was minimally saturated to about 1.3 wt %.
In this study, a fabrication of nickel nanoparticles from LNO(LiNiO2), which is a cathode active material, was synthesized by the liquid reduction process of NiSO4, obtained through a leaching and purification process. Hydrazine monohydrate (N2H4·H2O) was used as a liquid reducing agent and it was added to NiSO4 at a volume ratio of NiSO4:N2H4·H2O = 10:3 and reacted for 10 min to synthesize the nickel hydrazine complex. Sodium hydroxide was added to the nickel hydrazine complex at the weight ratio of NiSO4:NaOH = 10:1.25–1.5 and the reduction reaction was performed at 80 °C for 15 min to synthesize nickel particles. Synthesized nickel particles were agglomerated and had a mean size of 200 nm to 300 nm. Ultrasonic dispersion, which is a physical dispersion method, was conducted. The nickel had particles of 100 nm or less when dispersed for 2 h at an ultrasonic intensity of 40 kHz. In order to prevent the agglomeration of the dispersed particles again, polyvinylpyrrolidone (PVP), an interfacial stabilizer, was added to stabilize the dispersed particles. It was confirmed that the nanoparticles were stably retained when PVP was added in an amount of 1 to 2 wt % based on the weight of the nickel. The purity of nickel recovered was found to be 99.62 wt %.
Hexane is a safe, efficient, and cost-effective alternative to other commercial hydrocarbons for gaseous carburization; however, commercial hexane is not sufficiently pure. Titanium powder can remove oxygen-containing impurities from commercial hexane; however, research on the use of titanium powder remains limited. We investigated the purification of hexane using titanium, copper, and aluminum powders and used the purified hexane for the gaseous carburization of tantalum. Ti exhibited lower activation energy for oxidation (1.55 kJ/mol) than Cu (91.09 kJ/mol) and Al (150.25 kJ/mol) and a significantly higher oxidation rate (0.0269 g/h) in hexane at room temperature than Cu (0.0018 g/h) and Al (0.0001 g/h). The carbon content in tantalum carburized using the purified hexane was comparable to that carburized using unpurified hexane (approximately 6.22%); however, its oxygen content was significantly lower (1.39%), which indicates that the produced tantalum carbide has a higher purity. X-ray diffraction results revealed that the oxidation products of tantalum, such as Ta2O, TaO2, Ta0.8O2, and Ta2O5, were absent in the sample carburized using the purified hexane. Therefore, Ti powder can effectively remove oxygen-containing impurities from commercial hexane and facilitate its use as an effective carburizing medium for the synthesis of high-purity tantalum carbide.
Nb-Ti binary alloys are widely employed as high value-added materials in the manufacture of super heat-resistant alloys, biomaterials, and superconductors. Therefore, there is significant interest to produce Nb-Ti master alloys in a cost-effective manner. In this study, we investigated the magnesiothermic reduction of Nb2O5 and Ti2Nb10O29 over the temperature range of 1073 to 1223 K and comparatively evaluated the reaction outcomes. The reduction product was composed of metal (Nb or Nb-Ti) particles and MgO, which covered the surface of the reduced metal particles. After the reduction reaction, the surface MgO phase was removed by pickling with hydrochloric acid (HCl) to finally recover the Nb metal or Nb-Ti alloy as a pure product. Scanning electron microscopy and X-ray diffraction analyses of the pure Nb metal and Nb-Ti alloy powders revealed that the reduction of both raw materials was successful at temperatures exceeding 1173 K. Reaction kinetics analysis revealed that the activation energy for the reduction of the mixed metal oxide (Ti2Nb10O29) is lower than that of Nb2O5 reduction. This is because of the different reaction mechanism behaviors during reduction and the different thermodynamic stabilities of the precursors.
Tantalum carbide (TaC) is a highly refractory material with a melting point of 4153 K, making it attractive for applications requiring excellent hardness and thermal stability. In this study, we investigated the carburization behavior of high-purity tantalum metal powder synthesized by magnesium thermal reduction of Ta2O5, using activated carbon and graphite as carbon sources under high vacuum. Carburization was conducted at 1100–1400 °C for durations of 5–20 h. Carbon contents were analyzed via combustion analysis, and activation energies were calculated based on Arrhenius plots. The results showed that the activated carbon significantly enhanced carbon uptake compared to graphite due to its higher porosity and surface reactivity. The formation and transformation of carbide phases were confirmed via X-ray diffraction, revealing a progression from Ta to Ta2C and eventually to single-phase TaC with increasing carbon content. Scanning electron microscopy (SEM) analysis showed that fine particles formed on the surface as carbon content increased, indicating local nucleation of TaC. Although the theoretical carbon content of stoichiometric TaC (6.22 wt.%) was not fully achieved, the near-theoretical lattice parameter (4.4547 Å) was approached. These findings suggest that activated carbon can serve as an effective carburizing agent for the synthesis of TaC under vacuum conditions.