Disposing electronic plastic waste into construction materials is an eco-friendly and energy efficient solution to protect the environment. This work is aimed at enhancing the strength of self-compacting concrete (SCC) replacing sand with electronic waste, namely, High Impact polystyrene (HIPS) plastic granules and cementitious material with fly ash. SCC is designed with the optimized binder content of 497 kg/m3 using Fly Ash (30% by weight of cement) and 0.36 as water-to-binder ratio for all the mixtures. High Impact Polystyrene granules are replaced with sand up to 40% (by volume) at a regular interval of 10%. Rheological behavior is observed with the slump flow test for slump diameter, V-funnel test for flow time, and the L-box test for heights ratio, respectively. Strength behavior is studied by performing split tensile strength, and compressive strength tests after a period of 7, 28, and 90 days, respectively. Both fly ash and HIPS aggregate in addition to SCC up to 30% exhibits a minimal strength reduction with a promising performance in workability. Hence incorporation of both fly ash and HIPS granules up to 30% in SCC is a viable eco-friendly technique, with the beneficial economic impact on the construction industry.
This investigation is focused on durability studies of binary blended self-compacting concrete (SCC) with the replacement effect of electronic plastic waste, namely high-impact polystyrene (HIPS) granules as partial sand. In the current investigation, for all the SCC mixes, cement is replaced with pozzolanic material fly ash in the binder content of 497 kg/m3 and an adopted water-to-binder ratio of 0.36. Durability properties such as porosity, water absorption, and sorptivity are assessed for the curing periods of 28 and 90 days on SCC specimens produced with HIPS (0%–40% replacement by volume of sand). Both surface and internal water absorption rates were found to be minimal for SCC with HIPS. Replacement of HIPS up to 30% in SCC exhibited improved trends for all tests results. Reported durability parameter values were within permissible limits and revealed the excellent performance of HIPS in SCC. The optimum durability values can be attributed to the dense microstructure of SCC obtained with the combined effect of HIPS and fly ash. The continuous gradation of aggregates in the matrix reduced porosity due to the spherical shape of HIPS; additionally, the hydrophobicity of HIPS inhibits moisture migration in SCC. The additional benefits of fly ash, such as pozzolanic action and the filler effect at the interfacial transition zone (ITZ) are also major contributions to the long-term performance of durability. Electronic plastic waste replacement for fine aggregates in concrete compensates for the disposal problem and conserves natural sand.
Utilization of various mineral admixtures in producing mortar decreases the porosity and capillarity, hence improves the durability in opposition to water and competitive solutions. In this research work, Ground Granulated Blast Furnace Slag is used to replace 30 percent, 60 percent, and 70% of ordinary Portland cement (OPC) (GGBFS). Mechanical property (compressive strength) and durability properties (permeability, porosity, and sorptivity) of high‐performance concrete (HPC) are tested. Water permeability of M85 is measured using three cell permeability apparatus. Compressive strength, porosity, and sorptivity of the same mixes are also found. According to the test results of HPC, 30% replacement level of GGBFS gives higher compressive strength than 60% and 70% replacement levels of GGBFS. An equation is developed for permeability of HPC based on mechanical strength and porosity. It is found that coefficient of permeability of water for HPC mixes ranges from 5.1 × 10‐11 cm/sec to 7.8 × 10‐11 cm/sec. It is concluded that 30% GGBFS used in HPC produces less porosity, less permeability, and less sorptivity than compared to other replacement levels.
In this current work, gold nanoparticles (AuNPs) that were biosynthesized from the leaves of the Royal Poinciana Tree (Delonix regia) were experimentally investigated for their photocatalytic decomposition and antioxidant properties. Using plant extracts as reducing and stabilizing agents, the synthesis of AuNPs was carried out sustainably. Advanced methods for assessing the dimension, structure, and crystallization of the resulting gold nanomaterials included transmission electron microscopy (TEM), Fourier-transform infrared spectroscopy (FTIR), X-ray diffraction (XRD), and UV–visible spectroscopy. The RP-AuNPs were mostly spherical, and the average particle size was 22.36 nm, according to the TEM images. The potential of the biosynthesized AuNPs photocatalytic activities to break down 4-nitrophenol (4-NP) pollutants when exposed to sunlight was assessed. The nanoparticles also showed good ultrarapid catalytic capacity for the 10-min, 0.337-min⁻1 rate of reactions and a consistent decrease in 4-nitrophenol to p-aminophenol in a solution of NaBH4. The pseudo-first-order kinetic model was used to describe the photodegradation process. These findings support the notion that royal poinciana is a promising bioresource for producing AuNPs with various uses. This research also tested the antioxidant power of RP-based AuNPs by scavenging DPPH radicals. Their IC50 value was 55.32 µg/ml using a sigmoidal curve-fitting model, which means they are excellent at eliminating free radicals.
Steel connection is utilized to link the beam and column. It moves the plastic hinge structure away at a predetermined distance from the face of the column. To lower the cross-sectional area of the beam flanges, several shape cuts (uniform, radius, taper, and straight cut) are available, and a piece of the beam flanges at the column face is purposefully intended to yield and plastic hinge. The use of a lowered beam section connection reduces stress absorption since the criteria for a strong column–weak beam are met. The ANSYS 14.5 software was used to model four types of reduced beam sections by decreasing the beam flange. In various patterns, fatigue behaviour was studied. The objective of this project is to evaluate the deformations, stresses and transient temperatures deformations, and stresses of the reduced beam section at static structural analysis. In comparison to other connections, steel connection reduced beam section ductile and dissipated energy more. A nonlinear finite element software was used, along with a static study of exhaustion responsiveness transient temperatures. The analysis is carried out to identify the thermal effects on the behaviour of material properties in the elastic and plastic regions. The members with cuts have performed superior in comparison with members without cuts.