Yajie Li

Dr. Yajie Li

orcid

Research Focus & Metrics

Academic Career Length

11Years (2016-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
20 February 2019 in Materials
Verified
Journal Article
Open access
PDF file
YLYajie Li
Yajie Li
HWHaibo Wu
Haibo Wu
XLXuejian Liu
Xuejian Liu
ZHZhengren Huang
Zhengren Huang
Porous liquid-phase-sintered SiC (L-SiC) ceramics were successfully fabricated by hot press sintering (HP) at 1800 °C in argon, using Al2O3 and Y2O3 as oxide additions. By varying the starting coarse SiC particle size, the relationships between pore microstructures and flexural strength as well as gas permeability of porous L-SiC were examined. All the as-sintered samples possessed homogeneous interconnected pores. The porosity of porous L-SiC decreased from 34.0% to 25.9%, and the peak pore size increased from 1.1 to 3.8 μm as the coarse SiC particle sizes increased. The flexural strengths of porous L-SiC ceramics at room temperature and 1000 °C were as high as 104.3 ± 7.3 MPa and 78.8 ± 5.1 MPa, respectively, though there was a decrease in accordance with their increasing pore sizes and particle sizes. Moreover, their gas permeability increased from 1.4 × 10−14 m2 to 4.6 × 10−14 m2 with the increase of pore size in spite of their decreased porosity.

12 May 2021 in Materials
Verified
Journal Article
Open access
PDF file
QMQuan Mao
Quan Mao
MLMeng Liu
Meng Liu
YLYajie Li
Yajie Li
YWYuquan Wei
Yuquan Wei
Yong YangYong Yang
Yong Yang
ZHZhengren Huang
Zhengren Huang
Titanium oxide is widely applied as a photocatalyst. However, its low efficiency and narrow light absorption range are two main disadvantages that severely impede its practical application. In this work, black TiOx films with different chemical compositions were fabricated by tuning target voltage and controlling O2 flow during reactive DC magnetron sputtering. The optimized TiOx films with mixed phases (TiO, Ti2O3, Ti3O5, and TiO2) exhibited fantastic photothermal and photocatalytic activity by combining high light-absorptive Ti2O3 and Ti3O5 phases with the photocatalytic TiO2 phase. The sample prepared with oxygen flow at 5.6 ± 0.2 sccm and target voltage near 400 V exhibited excellent optical absorbance of 89.29% under visible light, which could improve surface temperature to 114 °C under sunlight. This film could degrade Rhodamine-B up to 74% after 150 min of UV irradiation. In a word, this work provides a guideline for fabricating black TiOx films with photothermal-assisted photocatalytic activity by reactive DC magnetron sputtering, which could avoid the usage of hydrogen and is convenient for quantity preparation.