To enhance the cutting performance of TiAlSiN coated cemented carbide tools by inserting Ti interlayers and to explore their mechanism, TiAlSiN/Ti multilayer coatings with different Ti thicknesses, including 0 nm, 25 nm, 50 nm, 100 nm, and 150 nm, were deposited onto cemented carbide (WC-10 wt%, Co) substrates by high power impulse magnetron sputtering (HiPIMS). The microstructure, hardness, grain orientation, residual stress, adhesion, and toughness of those coatings were measured, and the cutting performance against Inconel 718 was analyzed. Meanwhile, finite element method (FEM) indentation simulations were performed to gain detailed insight into the effects of Ti interlayer thickness on mechanical properties of TiAlSiN/Ti multilayer coatings. Results demonstrated that mechanical properties of TiAlSiN multilayer coatings were significantly changed after the Ti interlayer was introduced, and the multilayer coating #M2 with 25 nm Ti layer showed the excellent toughness and adhesion without sacrificing hardness too much. As Ti interlayer thickness increased, both toughness and adhesion decrease owing to the plastic mismatch between individual layers, and these changes were discussed detailedly with finite element method. Moreover, the result of the cutting experiment also revealed that the tool flank wear Vb can be reduced by the multilayer structure. This improvement is believed to be due to the increasing toughness, which alleviated the damage caused by the continuous impact load of hard phases generated by Inconel 718 during cutting.
TiAlSiN coatings were deposited on YT 15 cemented carbide substrate by reactive direct current magnetron sputtering (DCMS) in a Plasma Immersion Ion Implantation and Deposition (PIII&D) system. The pre-implantation step and the coating deposition were carried out in the same experimental facility. In this article the effects of pre-implantation of several different elements (N, C, and O) were investigated. The adhesion strength, hardness, micro-structure, element concentration, depth profile, and the formation of coatings after the PIII experiments were characterized by a wide variety of techniques such as Rockwell indentation, scratch test, nano-indentation measurement, X-ray diffraction, energy dispersive spectroscopy, and Auger electron spectroscopy. The results showed that the adhesive strength of TiAlSiN coatings was significantly improved on samples pre-implanted with N and O whereas only slightly improved with pre-implantation of C. Additionally, the microstructure and mechanical properties of the TiAlSiN coatings were also altered through pre-implantation. The improved adhesion could be explained by the grain refinement and surface energy enhancement of the substrate by pre-implantation.
Tungsten carbide (WC) and Tungsten carbonitride (WCN) coatings are deposited by reactive high-power impulse magnetron sputtering (HiPIMS) with various nitrogen gas flow rates. The characteristics of discharge current and plasma optical emission of HiPIMS are recorded by oscilloscope (OSC) and optical emission spectroscopy (OES). The results exhibit that the peak discharge currents and the intensities of optical emission spectra lines are significantly influenced by the addition of nitrogen. The elemental concentration, microstructure, mechanical and tribological properties in ambient temperature and high temperature of deposited coatings are investigated by a wide variety of techniques such as energy dispersive spectroscopy (EDS), X-ray diffraction (XRD), nano-indentation measurement, scanning electron microscope (SEM), atomic force microscopy (AFM), X-ray photoelectron spectroscopy (XPS), and ball-on-disk tribometer. The results show that WC/WCN coatings with different microstructures, mechanical properties and tribological properties have been produced by controlling the flow rate of N2. Meanwhile, with the N2 flow rate increasing from 0 sccm to 24 sccm, (101) diffraction peak shifts to low angle. Moreover, (102) and (110) peaks’ intensities and the angle of (101) peak of β-W2C phase of the deposited WCN coatings decrease and disappear, and the average grain size decreases from 8.9 nm to 6.4 nm. XPS results show that the intensities of C=N, W–N, W–C–N, and N–O peaks increase while the intensity of C–W peak decreases. The deposited coatings change from slight columnar type to a typically dense and featureless structure, and the surface roughness decreases from Ra 11.6 nm at 0 sccm to Ra 5.7 nm at 24 sccm. The variation of nitrogen flow also plays a role in the mechanical properties of the coatings. It is found that the maximum hardness and elastic modulus of 35.6 GPa and 476.5 GPa appear at 16 sccm N2 flow rate. The results of wear tests demonstrate the addition of nitrogen slightly deteriorates tribological properties at room temperature (25 °C), but can remarkably improve tribological properties at high temperature (400 °C) of WC/WCN coatings deposited with an appropriate flow rate of nitrogen.