In this study, the continuous evolution of the second-phase particles across as-cast, homogenization, multi-directional forging (MDF), and solution-aging treatment and their effect on tensile fracture behavior of 2219 aluminum alloys with different Cu contents was examined by optical microscopy (OM), scanning electron microscopy (SEM), and tensile tests. The results showed that the microstructure of as-cast 2219 aluminum alloy consisted of the α-Al matrix, Al2Cu coarse phase, and Fe-rich impurity phase. Severe segregation of Cu existed, and eutectic networks can be observed in the ingot. With an increase in Cu content, the eutectic networks became coarsen and thicker. During the complex improved process, the refinement mechanisms were fragmentation, dissolution, and diffusion of Al2Cu particles. Most fine Al2Cu particles were fully dissolved into the matrix and partial coarse particles were still retained after solution-aging treatment. Thus, the elongations of all the samples, undergoing solution treatment followed by water quenching, increased evidently. Then, the elongations decreased slightly due to the increase of precipitates. The fractography analysis of peak aged condition samples indicated that the fracture mode was diverted from a typical inter-granular fracture to a mainly trans-granular fracture with increase in Cu content from 5.56% to 6.52%. Fracture initiation mainly occurred by original microcrack propagation and microvoid nucleation at the coarse constituents.
The Fe-rich intermetallic phases have a broadly detrimental effect on the mechanical properties of Al–Cu alloy. In this paper, the continuous evolution of Fe-rich intermetallics and their effects on mechanical properties, especially the tensile fracture behavior of 2219 wrought Al–Cu alloys as a function of Fe content against different processing approaches (i.e., as-cast, homogenization, multidirectional forging, and solution-peak aging treatment) were investigated using optical microscopy, scanning electron microscopy, and tensile tests. The results indicated that needle-like Al7Cu2Fe or Al7Cu2(Fe, Mn) intermetallics mainly presented in the final microstructures of all alloys with various Fe contents. The size and number of Al7Cu2Fe/Al7Cu2(Fe, Mn) intermetallics increased with the increase of Fe content. The increase of Fe content had little influence on the ultimate tensile strength and yield strength, while obvious deterioration in the elongation, because fracture initiators mainly occurred at the Al7Cu2Fe/Al7Cu2(Fe, Mn) particles or particles–matrix interface. Therefore, the 2219 Al–Cu alloy with 0.2 wt.% Fe content presented relatively low tensile ductility. The tensile fracture mechanism has been discussed in detail.
In this study, three kinds of coatings, AlTiN, AlTiN–Ni, and AlTiN–Cu were deposited via the cathodic arc evaporation method. The microstructure, mechanical properties, oxidation resistance, and cutting behavior of these coatings were then investigated. The incorporation of Cu(Ni) into AlTiN eliminated its columnar structure and led to an increase in the growth defects of its macroparticles. The addition of Cu and Ni decreased the hardness of the coatings, their elastic moduli, and their friction coefficients. All of the AlTiN, AlTiN–Ni, and AlTiN–Cu coatings presented sufficient adhesion strength values. The oxidation resistance of these three coatings was determined to be in the following order: AlTiN > AlTiN–Ni > AlTiN–Cu. Titanium turning experiments indicated that the cutting force was reduced and the tool life was improved through doping with Cu(Ni) elements, dependent on cutting speed. The AlTiN–Ni coating showed the best performance at a high cutting speed, whereas the AlTiN–Cu coating was more successful at a lower cutting speed.
28 August 2021 in Metals and Materials International
In the present work, the influence of Cu content on microstructure, mechanical properties and exfoliation corrosion behaviors of Al-Zn-Mg-xCu alloy extrusions has been investigated in longitudinal-transverse (L-T) and short-longitudinal (S-L) directions by means of mechanical tensile and exfoliation corrosion testing combined with optical microscopy (OM), scanning electron microscopy (SEM) and transmission electron microscopy (TEM). The results showed that a higher Cu content significantly decreased the fracture toughness and ductility of the alloy in S-L direction compared with L-T direction. Concomitant with the increase in Cu content, a transition in fracture mode was observed from transgranular dimpled rupture to intergranular rupture in S-L direction. Moreover, the exfoliation corrosion (EXCO) resistance of the alloy decreased as the Cu content increased and the exfoliation corrosion resistance of the alloy in short-transverse (S-T) direction was better than that of L-T direction. These results were mainly associated with the large number of coarse intermetallics caused by high Cu content in the L-T direction of alloy.