The resource utilization of phosphogypsum is confronted with great challenge. Of all the different methods for phosphogypsum resource utilization, using phosphocypsum to fabricate calcium fluoride (CaF2) is an effective resource utilization method. In this work, high-quality nano-calcium fluoride was successfully prepared in aqueous solution using calcined phosphogypsum by direct precipitation method. A series of orthogonal experiments were carried out in study. Here, the calcined phosphogypsum powder was mixed with NH4F to react at 40°C for 70 min according to the optimum molar ratio (Ca/ F=0.4). Meanwhile, the residue obtained by separating the mixture reacted was dried at 120°C for 90min. After preparation, the nano-calcium fluoride was analyzed by X-ray diffraction and scanning electron microscope, results found that the average particle diameter of calcium fluoride was around 70 nm. This work could increase the industrial chain of phosphogypsum application and apply a method to solve the fluorite resource shortage.
A precipitation reaction method was employed to prepare mesopore calcium carbonate (CaCO3) using rape flower pollen as the template. CaCO3 adsorbent was characterized using X-ray diffraction (XRD), scanning electronic microscopy (SEM), and Brunner−Emmet−Teller measurements (BET). The equilibrium adsorption data on amoxicillin were explained using Langmuir, Freundlich, and Temkin adsorption isotherm models. The pseudo-first order, second order, pseudo-second order, and intra-particle diffusion kinetic models were used to explore adsorption kinetics. Equilibrium adsorption of as-prepared CaCO3 was better depicted using the Langmuir adsorption model with an R2 of 0.9948. The separation factor (RL) was found to be in the range of 0 < RL < 1, indicating the favorable adsorption of amoxicillin. The adsorption capacity of mesopore CaCO3 reached 13.49 mg·g−1 in 0.2 g∙L−1 amoxicillin solution. The values of adsorption thermodynamic parameters (ΔHθ, ΔSθ, ΔGθ) were obtained. In addition, the adsorption process turned out to be endothermic and spontaneous for the CaCO3 product at 298 K, 308 K, and 318 K.
The acid-etching behavior and mechanism of basalt fiber in an acid solution determine the modification and application of basalt fiber. The effects of acid etching time, sulfuric acid concentration, acid etching temperature, and liquid–solid ratio on the acid etching process of basalt fiber were studied using a single-factor experiment. The chemical composition, phase, structure, and morphology of basalt fiber before and after acid etching were analyzed by XRF, XRD, SEM-EDS, and spectrophotometry. The dissolution mechanism of the iron component was speculated. The results showed that the dissolution of iron components could be promoted by increasing the acid etching time, sulfuric acid concentration, acid etching temperature, and liquid–solid ratio. When the sulfuric acid concentration was 1 mol L −1 , the acid etching temperature was 90°C, the liquid–solid ratio was 20 mL g −1 , and the reaction time was 4 h, the dissolution rate of iron components could reach 1.66%. During the acid etching process, the phase change of the basalt fiber was not obvious. Due to the dissolution of the iron component, the surface of the fiber could be chapped, resulting in the phenomenon of ravines and delamination, reducing the lattice distortion rate of the material.