Drying shrinkage of alkali-activated slag concrete (AASC) is significantly greater than that of concrete made with ordinary Portland cement (OPC). It limits the large-scale application of AASC in field engineering. This study investigates the effect of early age-curing methods, including water curing, curing in elevated-temperature water, and CO2 curing, on drying shrinkage of AASC. Scanning electron microscopy (SEM), X-ray diffraction (XRD), thermogravimetric (TG-DTG), and mercury intrusion porosimetry (MIP) were carried out to analyze the composition and microstructure of hydration products, to provide deeper understanding of drying shrinkage of AASC. The results show that water curing decreased drying shrinkage of both C30 and C50 AASC moderately compared to air curing, while it was more effective for C30 AASC. Curing in water of elevated temperature and CO2 curing were very beneficial to mitigate drying shrinkage of AASC. Heat curing decreased drying shrinkage of AASC up to 80%. SEM and TG-DTG results show that denser microstructure formed because of the accelerated hydration, resulting in lower porosity and lower proportion of pores smaller than 25 nm that contributed to the reduction of drying shrinkage. In addition, under high-temperature curing, most autogenous shrinkage of AASC occurred in the first few days because hydration was accelerated. After measurement of drying shrinkage was started, recorded autogenous shrinkage of AASC cured in elevated-temperature water should be much less than that of AASC cured at normal temperature. It is another important reason for the reduction of drying shrinkage. Carbonation occurring in the CO2 curing period led to the decalcification of C-(A)-S-H gel; it coarsened the pore-size distribution and decreased the total porosity. Therefore, drying shrinkage of C30 and C50 AASC was declined by 49% and 53% respectively.
This study investigates the long-term durability and crystallization-induced degradation mechanisms of alkali-activated slag (AAS) mortars with varying water-to-binder ratios (w/b, 0.4, 0.45, 0.5) under semi-immersion in 5 wt.% sodium sulfate solution. Through 360 d of exposure, the evolution of physical–mechanical properties (mass change, open porosity, compressive/flexural strength) and ion migration patterns (SO42−, Na+, Ca2+) were analyzed to unravel the interplay between pore structure, ion transport, and crystallization-induced deterioration. Results demonstrated that higher w/b ratios exacerbated surface crystallization and spalling due to accelerated ion transport and pore coarsening. Early-stage strength gains (up to 25.15% at 120–180 d) stemmed from pore refinement via sulfate deposition and continued slag hydration. However, prolonged exposure triggered microstructural degradation, with open porosity increasing by 58.9% and strength declining by 30.6% at 360 d for a w/b of 0.5 compared to a w/b of 0.4. This was driven by crystallization pressure and the decalcification of hydration products. Ion migration analysis revealed SO42− enrichment in evaporation area and outward Na+ diffusion, establishing supersaturation gradients that aligned with crystallization damage progression. These findings provide critical insights for optimizing AAS mortar formulations to mitigate sulfate crystallization risks in semi-immersed environments.
Ultra-high-performance concrete (UHPC) exhibits exceptional mechanical properties and durability but faces challenges such as high heat of hydration and limited stiffness. Incorporation of coarse aggregates offers a potential solution; however, it alters the dispersion of steel fibers, thereby affecting the mechanical performance of UHPC under different loading conditions. This study systematically investigates the influence of coarse aggregates on UHPC performance under different loading conditions, including four-point bending, uniaxial compression, and triaxial compression tests. The spatial distribution of steel fibers was quantitatively analyzed via image analysis to elucidate changes induced by CA incorporation. Results reveal that with 20 vol% coarse aggregate (10 mm), UHPC’s flexural strength is essentially unchanged (≈23 MPa), whereas flexural toughness decreases by about one-third. This toughness loss is linked to a slight increase in the fiber orientation angle (from 48.77° to 48.90°) and reduced continuity, which together weaken crack-bridging. Moreover, both flexural strength and toughness are governed primarily by the local steel-fiber content within the tensile zone. Under triaxial compression, confinement dominates: as confining pressure rises from 0 to 30 MPa, compressive strength increases by approximately 32.6%, 52.6%, and 71.3%. Due to crack-suppression by confinement overlapping with fiber bridging, the contribution of fibers to strength gains decreases with increasing confinement, and the competing and complementary interaction between coarse aggregate and steel fibers correspondingly weakens. These findings clarify the coupled effects of coarse aggregate and fibers in UHPC-CA, guide mix-design optimization for improved mechanical performance, and support broader practical adoption.