Ruhul Khan

Dr. Ruhul Khan


Research Focus & Metrics

Academic Career Length

19Years (2008-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
15 August 2024 in Discover Applied Sciences
Verified
Journal Article
Open access
PDF file
MRMd. Mostafizur Rahman
Md. Mostafizur Rahman
Md. Abdus ShahidMd. Abdus Shahid
Md. Abdus Shahid
THTanvir Hossain
Tanvir Hossain
SSSohan Sheikh
Sohan Sheikh
SRSunjidur Rahman
Sunjidur Rahman
Imam HossainImam Hossain
Imam Hossain
Alginate, a naturally sourced bio-polymer derived mainly from brown seaweed, has gained incredible attention due to its versatile properties and wide range of applications. This review outlines alginate regarding sources, extraction methods, classifications, and critical characteristics. The critical development of alginate, focusing on its application in 3D bioprinting in fields such as vascular tissue formation, bone printing, and cartilage printing, has been discussed. Recent trends regarding the application of alginate in different sectors, from cosmetic textiles to wastewater treatment, wound dressing, and preparation of intelligent materials, have also been probed. The techniques used, benefits, and limitations form the discussion of each application. In addition, future alginate perspectives are discussed by considering current research with potential innovations that can expand its utility. Particular attention is devoted to the promising role of alginate in these emerging technologies that hold promise for radical changes in many industries due to its biocompatibility, biodegradability, and unique physicochemical properties. This review seeks to lay down basic knowledge on alginate by synthesizing the state of the art and, in this way, brings out the gaps that might inspire further studies and development in this dynamic field.

23 June 2009 in Journal of Reinforced Plastics and Composites
Verified
Journal Article
Closed access
RKRuhul Khan
Ruhul Khan
MKMubarak A. Khan
Mubarak A. Khan
HZHaydar U. Zaman
Haydar U. Zaman
SPShamim Pervin
Shamim Pervin
NKNuruzzaman Khan
Nuruzzaman Khan
AMA.I. Mustafa
A.I. Mustafa
Jute fiber (hessian cloth)-reinforced polypropylene matrix composites (50 wt% fiber) were fabricated by compression molding. Tensile strength, tensile modulus, bending strength, bending modulus, and impact strength of the composites were found to be 48 MPa, 2.5 GPa, 56 MPa, 4.5 GPa, and 18 kJ/m2, respectively. Then E-glass fiber (woven)-reinforced polypropylene-based composites (50 wt% fiber) were fabricated and the mechanical properties were compared with those of the jute-based composites. It was revealed that E-glass fiber-based composites had almost double the mechanical properties as compared to jute composites. The interfacial shear strength of the jute and E-glass fiber-based systems was investigated and found to be 2.13 and 4.66 MPa, respectively, measured using the single-fiber fragmentation test. Fracture sides after flexural testing of both types of the composites were studied by scanning electron microscope and the results revealed poor fiber matrix adhesion for jute-based composites when compared to that of the E-glass fiber composites.

21 July 2011 in Journal of Thermoplastic Composite Materials
Verified
Journal Article
Closed access
PDF file
SNS. Nahar
S. Nahar
RKRuhul Khan
Ruhul Khan
KDK. Dey
K. Dey
BSB. Sarker
B. Sarker
ADA.K. Das
A.K. Das
Sushanta GhoshalSushanta Ghoshal
Sushanta Ghoshal
Jute and bamboo fiber-reinforced polypropylene (PP) based composites (50 wt% fiber) were fabricated by compression molding. Tensile strength (TS), bending strength (BS), tensile modulus (TM), and bending modulus (BM) of the jute-reinforced PP composite were found to be 48, 56, 900, and 1500 MPa, respectively. Then, bamboo fiber-reinforced PP-based composites (50 wt% fiber) were fabricated and the mechanical properties evaluated. The TS, BS, TM, and BM of bamboo-reinforced PP composites were found to be 60, 76, 4210, and 6210 MPa, respectively. It was revealed that bamboo fiber-based composites had higher TS, BS, TM, and BM compared to jute-based composites. Degradation tests of the composites (jute fiber/PP and bamboo fiber/PP) were performed in soil at ambient conditions for up to 24 weeks. It was revealed that bamboo fiber/PP composite retained its original mechanical properties higher than that of jute fiber/PP composite. The interfacial shear strength of the jute and bamboo fiber-based composites was investigated using the single-fiber fragmentation test and it was found to be 2.14 and 4.91 MPa, respectively. Fracture sides of the composites were studied by scanning electron microscope, and the results revealed poor fiber matrix adhesion for jute fiber-based composites compared to that of the bamboo fiber-based composites.

5 November 2012 in Journal of Thermoplastic Composite Materials
Verified
Journal Article
Closed access
NANousin Akter
Nousin Akter
RKRuhul Khan
Ruhul Khan
MTMohammad O Tuhin
Mohammad O Tuhin
MHM Emdadu Haque
M Emdadu Haque
MNMohammad Nurnabi
Mohammad Nurnabi
RIRafiqul Islam
Rafiqul Islam
Chitosan-reinforced starch-based biodegradable composite films were prepared by solution casting. The chitosan content in the films was varied from 20% to 80% (w/w). Tensile strength (TS) and tensile modulus (TM) of the starch-based composites were improved significantly with the addition of chitosan. Water vapor permeability (WVP) and oxygen transmission rate (OTR) of chitosan-reinforced starch-based films showed a significant reduction compared to native chitosan film and indicated better barrier properties to water vapor and oxygen. The water uptake of the films pointed out better hydrophobic character due to the incorporation of chitosan in starch-based films. Thermal stability was also found to increase with the addition of chitosan in starch-based films and was confirmed by thermogravimetric analysis (TGA) and differential thermal analysis (DTA). Fourier transform infrared (FT-IR) spectroscopy supported the molecular interactions due to the reinforcement of chitosan in starch-based films. Surface and interface morphologies of chitosan film and starch/chitosan composite film were examined by scanning electron microscope (SEM) and suggested sufficient homogenization of starch and chitosan in the biodegradable composite films.

23 February 2009 in Journal of Reinforced Plastics and Composites
Verified
Journal Article
Closed access
RKRuhul Khan
Ruhul Khan
MKMubarak A. Khan
Mubarak A. Khan
SSSabrina Sultana
Sabrina Sultana
MKM. Nuruzzaman Khan
M. Nuruzzaman Khan
Quazi T. H. ShubhraQuazi T. H. Shubhra
Quazi T. H. Shubhra
FNFarhana G. Noor
Farhana G. Noor
Polypropylene (PP) matrix synthetic phosphate based degradable fiber reinforced unidirectional composites (10% fiber by weight) were fabricated by compression molding. Tensile strength (TS), tensile modulus (TM), elongation at break (%), bending strength (BS), bending modulus (BM), and impact strength (IS) were found to be 38 MPa, 1.5 GPa, 12%, 44 MPa, 4.9 GPa, and 7.58 kJ/m 2 respectively. Degradation tests of the fibers and composites were performed for six months in aqueous medium at room temperature (25°C). After six months, the mechanical properties of the composites retained almost 80% of their original properties. The interfacial shear strength (IFSS) of the composites were also measured by single fiber fragmentation test (SFFT). The IFSS of the composite system was found 5.9 MPa that indicated good fiber matrix adhesion.

29 November 2011 in International Journal of Polymeric Materials and Polymeric Biomaterials
Verified
Journal Article
Closed access
MRMushfiqur Rahman
Mushfiqur Rahman
KDKamol Dey
Kamol Dey
FPFahmida Parvin
Fahmida Parvin
NSNusrat Sharmin
Nusrat Sharmin
RKRuhul Khan
Ruhul Khan
ACA. M. S. Chowdhury
A. M. S. Chowdhury
Gelatin-based polyvinyl alcohol (PVA) films were prepared (using a casting process) by mixing aqueous solutions of gelatin and PVA in different ratios. Monomer 1, 4-butanediol diacrylate (BDDA) was dissolved in methanol. Films containing 95% gelatin + 5% PVA were soaked in 3% BDDA monomer (w/w). These films were then irradiated under gamma radiation (60Co) at different doses (50–500 krad) at a dose rate of 350 krad/h. The physico-mechanical and thermal properties of these films were evaluated. It was evident that 5% PVA-containing gelatin blend film exhibited the highest tensile strength (TS) value at 50 krad (51 MPa), which was 46% higher than that of non-irradiated blend films. It was also found that incorporation of PVA significantly reduced the TS value of the blend films compared to the raw film, whereas elongation at break (Eb) value was increased. A significant improvement of the blend films was also confirmed by thermogravimetric analysis (TGA) and thermo-mechanical analysis (TMA) when the acrylate group (from BDDA) was introduced into the film.