We report on the output performances of a fiber-coupled diode pumped Nd:LGSB laser passively Q-switched by a Cr4+:YAG saturable absorber (SA), with emissions at 1.06-μm near-infrared wavelength, as well as at 0.53-μm visible green spectrum through the self-frequency doubling process. The 2.3-at.% Nd:LGSB crystal delivered 1.43 W continuous-wave power at 1.06 μm with an overall optical-to-optical efficiency (with respect to the absorbed pump power) of 0.50. Green light with 3.3-mW power was emitted in a free-generation regime at 1.95-W absorbed pump power. By employing a Cr4+:YAG SA crystal with initial transmission Ti = 0.89, laser pulses at 1.06 μm with 13.4-μJ energy at 17.1-kHz repetition rate were obtained for ∼1.8 W absorbed pump power. The green laser pulse energy was 0.21 μJ at a 37.7-kHz repetition rate. The pulse duration amounted to 4.8 ns for both wavelengths of emission, indicating pulse peak power of 2.8 kW and 43.7 W for operation at 1.06 μm and 0.53 μm, respectively.
A 5.0-at.% Nd-doped La0.64Gd0.41Sc2.95(BO3)4 (Nd:LGSB) borate laser crystal was successfully grown by the Czochralski method, for the first time to our knowledge. The spectroscopic properties of the grown crystal are discussed and 1 µm laser emission, under end-pumping with a fiber-coupled diode laser at 807 nm, is reported. A c-cut Nd:LGSB medium yielded 1.35 W continuous-wave output power at 0.63 overall optical-to-optical efficiency, with respect to the absorbed pump power, together with the high 0.68 slope efficiency. With an a-cut Nd:LGSB sample, 0.81 W output power at 0.52 optical-to-optical efficiency was obtained. The laser emission performances under quasi-continuous wave pumping are presented as well, for both c-cut and a-cut crystals. Passive Q-switching was investigated with a semiconductor saturable absorber mirror (SESAM). Laser pulses with 2.2 µJ energy and 32.8 ns durations were recorded from a-cut Nd:LGSB. The average output power reached 0.36 W at 1.55 W absorbed pump power. Passive mode-locking with SESAM was achieved in a long Z-type resonator. Ultrashort pulses with 0.19 W average power, 1.63 nJ energy, and 1.43 ps pulse duration, at 118 MHz repetition rate, are demonstrated for the a-cut Nd:LGSB medium.
We report the first results on 1.06-μm mode-locking performances of a Czhochralski-grown a-cut Nd:LGSB, uncoated medium. Ultrashort pulses of 1.43 ps, at 118-MHz repetition rate are achieved with a Z resonator and SESAM approach.