The formation and characteristics of non-metallic inclusions in 316L stainless steel produced by the AOD (argon oxygen decarburization)–ladle furnace–continuous casting process were investigated. The morphology and composition of inclusions changed significantly during the refining and casting processes. After de-oxidation with Si/Mn additions, spherical complex inclusions mainly consisting of calcium silicates were observed. The contents of MgO and Al2O3 in these inclusions continuously increased as the steel moved from the AOD through ladle processing to the tundish. As the temperature decreased from the tundish through to solidification, harmful crystals of MgO/Al2O3 spinel were precipitated within the steel melt as well as within the calcium silicate matrix of existing inclusions. The results obtained from thermodynamic calculations carried out using FactSage™ commercial software agreed well with the information derived from evaluation of the industrial samples enabling recommendations to be made for the avoidance of detrimental spinel inclusions.
5 June 2021 in International Journal of Minerals, Metallurgy and Materials
The number, morphology, size and composition of inclusions after deoxidation and alloying in Ti-stabilised stainless steel were investigated. This was carried out by electrolytic extraction of inclusions from steel matrix, followed by microscopic examination. It was found that after the addition of ferrosilicon and manganese, and later aluminium, the composition of inclusions changed from manganese silicate-rich inclusions to alumina-rich inclusions. After tapping and titanium wire feeding, three types of TiN inclusion morphologies were observed, single, twinned and clusters. Both the turbulence and Stokes' collision mechanisms play a considerable role in the formation of TiN clusters.
31 March 2016 in Ironmaking & Steelmaking: Processes, Products and Applications
The characteristics of non-metallic inclusions in 347 stainless steel samples taken during a net-shape casting process after different holding times and melting temperatures were investigated using electrolytic extraction and polished cross-sections. The inclusions can be classified into three groups: oxides, composite inclusions and sulphides. Within the first two groups the inclusions were subdivided based on their morphology into the following categories: spherical, irregular and clusters. As the temperature decreased, sulphide and NbC precipitated within the steel melt as well as on the surface of existing oxides. The number density and area fraction of inclusions as well as the total oxygen contents increased with higher melt temperatures and longer holding times. The results obtained from thermodynamic calculations carried out using the FactSage™ commercial software agreed well with the experimental observations. In addition, it has been concluded that turbulent collisions are the dominant mode for the growth of inclusion clusters.