Background: The durability of computer-aided design/computer-aided manufacturing (CAD/CAM) resin nanoceramics in the oral environment is influenced by aging factors such as thermocycling and ultraviolet (UV) exposure. This study investigates the impact of these aging processes on surface characteristics and repair bond strength. Methods: CAD/CAM resin nanoceramic samples were divided into the following five groups: control (non-aged), 1-year and 5-year thermocycling, and 1-year and 5-year UV aging (n = 12). For the thermocycling procedure, the parameters employed were a temperature range of 5–55 °C with dwell times of 20 s per bath and 10,000 and 50,000 cycles; for the ultraviolet aging process, the parameters were established at a wavelength of 340 nm, an intensity of 0.55 W/m², and durations of 300 h and 1500 h. Surface roughness, microhardness, and repair bond strength were analyzed through profilometry, Vickers microhardness testing, and shear bond strength assessment, respectively. SEM, AFM, and XRD analyses were performed for structural evaluation. Results: Both thermocycling and UV aging significantly increased surface roughness (p < 0.001) while reducing microhardness and repair bond strength (p < 0.001). UV aging had a more pronounced effect, particularly after five years, leading to the highest surface roughness (Ra: 61.77 μm; Rz: 271.57 μm) and lowest microhardness properties (63.13). EDAX analysis indicated matrix degradation and an increase in inorganic filler exposure. Conclusions: Aging significantly affects the surface characteristics of CAD/CAM resin nanoceramics, with UV aging exhibiting the most detrimental impact. These findings highlight the necessity of considering long-term material stability in dentistry.
The success of adhesive restorations largely depends on the optimal bond strength between the tooth structure and the restorative material. The aim of this study was to evaluate the shear bond strength (SBS) of four different adhesives applied to mandibular molars on deep and superficial dentin. The total of 56 teeth used in the study were randomly divided into 2 subgroups of superficial dentin and deep dentin participants (n = 28). Superficial and deep dentin groups were randomly divided into 4 subgroups (n = 7) for application with different adhesive agents. We formed the following groups: Group 1 (G1)—deep dentin and GC bonding agent (G-Premio BOND); Group 2 (G2)—superficial dentin and GC bonding agent; Group 3 (G3)—deep dentin and Clearfil S3 bond bonding agent (Clearfil TM S3 BOND); Group 4 (G4)—superficial dentin and Clearfil S3 bond bonding agent; Group 5 (G5)—deep dentin and KerrOptibond bonding agent (KerrOptibondTM Universal); Group 6 (G6)—superficial dentin and Kerr Optibond bonding agent; Group 7 (G7)—deep dentin and 3M-ESPE universal bonding agent (3M ESPE); Group 8 (G8)—superficial dentin and 3M-ESPE universal bonding agent. The silicone block with a diameter of 3 mm and a thickness of 1 mm was placed in the middle of the occlusal surface and the test composite was loaded. All prepared specimens were aged in thermal cycles at 5–55 °C for 5000 cycles. The teeth were subjected to SBS (shear bond strength) tests at a crosshead speed of 1 mm/min in a universal testing machine. In all adhesive systems, deep dentin showed a higher bond strength than superficial dentin and the bond strength value was statistically significant (p = 0.05). The bond strength in all tested adhesive systems was observed to be significantly higher in deep dentin than in superficial dentin.
By means of a pull-out test, this study compared the retentive force of three fiber-reinforced resin composite posts and a zirconia post. These posts were cemented using two different dual-polymerizing adhesive resin luting agents. Forty freshly extracted canines were selected for the study. All tooth root were endodontically treated and the post spaces prepared. The posts were luted using luting agents according to the manufacturers' guidelines. A tensile force was applied, and all data were collected and analyzed statistically. Glass fiber posts that were luted with Panavia F (Group 3) had the highest median load (3.610 N), while zirconia posts that were luted with RelyX ARC (Group 8) had the lowest median load (0.926 N). Among the different post systems that were luted with Rely X ARC, significant differences were observed in their median tensile loads (p<0.047). When comparing between Panavia F and RelyX ARC of each post system, a significantly higher tensile load was seen with zirconia posts luted with Panavia F (Group 7) (p<0.032).