Yandong Jia

Yandong Jia


Research Focus & Metrics

Academic Career Length

8Years (2019-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
25 June 2020 in Frontiers in Materials
Verified
Journal Article
Open access
PDF file
YJYuefei Jia
Yuefei Jia
LZLiangbo Zhang
Liangbo Zhang
PLPeiyou Li
Peiyou Li
XMXindi Ma
Xindi Ma
LXLong Xu
Long Xu
GWGang Wang
Gang Wang
Low-density refractory medium entropy alloys (NbTiVZr, Nb0.5TiVZr, and NbTiV) were produced by vacuum arc melting, then heat-treated at 1,200°C for 1 h, water quenched, and finally annealed at 500°C for 0.5 h. Their respective microstructures, elevated-temperature (600–1,000°C) mechanical properties, and thermal expansion behavior were then investigated. All the alloys are characterized by a BCC structure with a grain size of c. 85–135 μm. The results demonstrated that NbTiVZr alloy exhibits relatively high yield strength and specific strength at 600, 800, and 1,000°C. Moreover, a low coefficient of thermal expansion was also obtained for this alloy when the temperature was below 750°C. This study provides guidance for the engineering application of low-density refractory medium entropy alloys at elevated temperatures.

2 July 2019 in Materials
Verified
Journal Article
Open access
PDF file
SZShikai Zhang
Shikai Zhang
PMPan Ma
Pan Ma
YJYandong Jia
Yandong Jia
ZYZhishui Yu
Zhishui Yu
SRSokkalingam Rathinavelu
Sokkalingam Rathinavelu
Prashanth Konda GokuldossPrashanth Konda Gokuldoss
Prashanth Konda Gokuldoss
In this study, a combination of Al–12Si and Al–20Si (Al–(12-20)Si) alloys was fabricated by selective laser melting (SLM) as a result of increased component requirements such as geometrical complexity and high dimensional accuracy. The microstructure and mechanical properties of the SLM Al–(12-20)Si in as-produced as well as in heat-treated conditions were investigated. The Al–(12-20)Si interface was in the as-built condition and it gradually became blurry until it disappeared after heat treatment at 673 K for 6 h. This Al–(12-20)Si bi-material displayed excellent mechanical properties. The hardness of the Al–20Si alloy side was significantly higher than that of the Al–12Si alloy side and the disparity between both sides gradually decreased and tended to be consistent after heat treatment at 673 K for 6 h. The tensile strength and elongation of the Al–(12-20Si) bi-material lies in between the Al–12Si and Al–20Si alloys and fracture occurs in the Al–20Si side. The present results provide new insights into the fabrication of bi-materials using SLM.

6 July 2022 in Materials
Verified
Journal Article
Open access
PDF file
TYTixin Yang
Tixin Yang
YCYouyang Chen
Youyang Chen
KYKangdong You
Kangdong You
ZDZiqiang Dong
Ziqiang Dong
YJYandong Jia
Yandong Jia
WJWang Jiajun
Wang Jiajun
The Sn-Ag-Cu (SAC) solder alloys with a low Ag (Ag < 3 wt.%) content have attracted great attention owing to their low cost, increased ability in bulk compliance, and plastic energy dissipation. However, some of their mechanical properties are generally lower than the SAC alloys with a higher Ag content. Adding alloying elements is an effective approach for improving the mechanical properties of the SAC alloys. In this study, the effect of Bi, Sb, and Ti on Sn-1 wt.%Ag-0.5 wt.%Cu (SAC105) solder alloys was investigated. The SAC solders with four compositions: SAC105-1 wt.%Bi, SAC105-1 wt.%Sb, SAC105-1 wt.%Bi-1 wt.%Sb, SAC105-1 wt.%Bi-1 wt.%Sb-0.4 wt.%Ti were prepared. The microstructure and phase compositions were characterized using electron scanning microscopy, and X-ray diffraction. The thermal properties and wettability were also examined. Uniaxial tensile tests and nano-indentation tests were conducted to evaluate the mechanical properties. The results show that adding Bi or Sb could increase the strength of SAC105 alloys mainly due to the solid solution strengthening effect. The creep resistance of SAC105 alloys was also improved with the additions of Bi and Sb. The co-additions of Bi and Sb into SAC105 alloys exhibit an enhanced creep resistance than that calculated by the theoretical calculation. The further addition of Ti into SAC105-1Bi-1Sb alloys demonstrated a much-improved creep resistance, which could be attributed to the synergistic effects of both solid solution strengthening and the precipitation hardening effects.

25 November 2022 in Metals
Verified
Journal Article
Open access
PDF file
YJYandong Jia
Yandong Jia
XYXingyu Yin
Xingyu Yin
YXYulai Xu
Yulai Xu
GWGang Wang
Gang Wang
In order to obtain steel with high tensile strength and elongation and good pitting resistance, the economical duplex stainless steel with and without the addition of tungsten (W) was prepared in this paper. The comparison and distribution of the two phases were controlled by optimizing the heat treatment process. The highest product of tensile strength and elongation of Cr19 series duplex stainless steel (DSS) DSS were obtained after solution treatment at 1050 °C for 5 min, up to 58692 Mpa%(876 Mpa * 67%), when the area f.raction of α was about 50.7%. The addition of tungsten reduces tensile strength due to the increased area fraction of α at 1050–1150 °C. Finer grain size leads to higher tensile strength after solution treatment at 1050 °C. The microstructure is characterized by transmission electron microscopy (TEM) and electron backscatter diffraction (EBSD). The steels exhibit an excellent transformation-induced plasticity (TRIP) effect after the solution treated is at 1050 °C, which may primarily be due to the existence of a more unstable austenite phase. The TRIP effect acts through the phase transformation of γ to α′-M during high deformation, and the orientation relationship of {111}γ || {110}α′-M & γ || α′-M belongs to the standard variants of Nishiyama–Wassermann relationship.