Carbon nanotubes (CNTs) are synthesized by the flame fragment deposition (FFD) technique using Iraqi liquefied petroleum gas (LPG) as a source of carbon in a hand-made reactor at a low temperature (160 °C) without using a catalyst. Purification of the multi-walled carbon nanotubes (MWCNTs) is carried out using a two-step process consisting of sonication in 30 wt.% hydrogen peroxide (H2O2) solution at room temperature to remove amorphous impurities adhering to the walls of the CNTs and carbon nanoparticles (CNPs), followed by sonication in an acetone bath to remove the polyaromatic hydrocarbons (PAH) formed during the LPG gas burning. Comprehensive characterizations such as X-ray diffraction (XRD), atomic force microscopy (AFM), thermo-gravimetric analysis (TGA), and transmission electron microscopy (TEM) were conducted to verify the efficiency of the purification process. The results clearly demonstrated that this process is promising for the purification of the synthesized CNTs.
Nanocoatings on solids can be achieved by various processes, including sol-gel and atomic layer deposition. However, challenges remain for achieving uniform nanocoatings on nanoscale substrates at a large scale. Here, we report a versatile and fundamentally different technique, termed condensed layer deposition, for depositing conformal metal oxide nanocoatings on nanoparticles and nanofibers. This approach involves water in liquid hydrocarbons condensing as a nanoscale water film on the substrate surface, enabled by interfacial tension between polar water and nonpolar liquid hydrocarbons. Chemical precursors are then added, which react with the condensed water film to form a metal oxide nanocoating. We demonstrate this for titania, alumina, and niobia on substrates including carbon nanotubes, iron oxide particles and carbon black. Condensed layer deposition can achieve oxide nanocoatings on a variety of substrates with tunable thickness, in one pass, at room temperature.
This study evaluated the effect of carbon nanofibers (CNFs) coated by aluminum oxide Al2O3 as a reinforcement on compressive strength, frost resistance, and drying shrinkage of cement mortars. Three weight ratios of 0.125%, 0.25%, and 0.5% of Al2O3/CNFs and bare CNF cement mortars were compared with reference cement mortar samples. The reactive porous and high surface area layer of alumina induced the hydration reaction and promoted the production of well-distributed hydration gel. Derivative thermal analysis–differential thermogravimetric (TGA-DTG) and X-ray powder diffraction (XRD) characterization showed that Al2O3/CNFs reinforcement led to greater hydration gel production than bare CNFs. Transmission electron microscopy (TEM) and scanning electron microscopy (SEM) were performed to study the coating and microstructure of the cement mortars evaluated in this paper. The results show that the optimum enhancement of the cement mortar properties was obtained at ratios of 0.125% for Al2O3/CNFs and 0.25% for CNFs. This enhancement was greater with Al2O3/CNFs-reinforced specimens in terms of high compressive strength, less compressive strength degradation after 150 cycles, and less drying shrinkage. The low use of the CNFs in Al2O3/CNFs samples indicates the coating is an economical and promising approach for improving the performance of cement mortars.