Poly (vinyl pyrrolidone) (PVP)/cellulose nanocrystal (CNC)/silver nanoparticle composite fibers were prepared via electrospinning using N,N′-dimethylformamide (DMF) as a solvent. Rheology, morphology, thermal properties, mechanical properties, and antimicrobial activity of nanocomposites were characterized as a function of material composition. The PVP/CNC/Ag electrospun suspensions exhibited higher conductivity and better rheological properties compared with those of the pure PVP solution. The average diameter of the PVP electrospun fibers decreased with the increase in the amount of CNCs and Ag nanoparticles. Thermal stability of electrospun composite fibers was decreased with the addition of CNCs. The CNCs help increase the composite tensile strength, while the elongation at break decreased. The composite fibers included Ag nanoparticles showed improved antimicrobial activity against both the Gram-negative bacterium Escherichia coli (E. coli) and the Gram-positive bacterium Staphylococcus aureus (S. aureus). The enhanced strength and antimicrobial performances of PVP/CNC/Ag electrospun composite fibers make the mat material an attractive candidate for application in the biomedical field.
The objective of this study was to investigate the mechanical properties of wood/plastic composites (WPCs) produced using wood flour (WF) prepared by wet ball-milling under various milling times (0–120 min) and drying methods (freeze- or heat drying). The drying method did not affect the particle size distribution, shape, or specific surface area of WF at milling times shorter than 40 min. At milling ≥ 40 min, freeze-dried ball-milled WF (FDWF) had smaller particle sizes and higher specific surface area than heat-dried ball-milled WF (HDWF). The highest tensile strength and modulus of rupture (MOR) were observed in WPCs made from freeze- and heat-dried WF at a milling time of 30 min. At milling time of 30 min, the amount of 100–300 µm FDWF and HDWF was 37% and 36%, respectively. The impact strength of WPCs increased, as the milling time increased. The amount of small freeze- and heat-dried WF particles increased due to an increase in the amount of 17 µm particles and specific surface area with increased milling time. Thus, impact strength of WPCs increased as particle size decreased. At milling times ≤ 60 min, there were no significant differences in mechanical properties between WPCs containing freeze- and heat-dried WF under the condition of this study.
Commercial wood flour of pine (Pinus densiflora) was used as an experimental material. It was milled with different milling times 0, 10, 20, 30, 40, 60, and 120 min to investigate the effect of their particle size distribution on the mechanical properties of the wood–plastic composite. Two kinds of drying conditions, 7 days of freeze-drying at a temperature of −45 °C and heat drying (80 °C) for 24 h were applied. Polypropylene and maleic anhydride-grafted polypropylene were used as a matrix and the compatibilizer of the wood–plastic composite compound, respectively. Particle size analysis showed that an increase in the time of ball milling decreased the wood flour size. However, an excessive milling period of time longer than 40 min corresponded to an increase in the amount of aggregation. Scanning electron microscope images showed the existence of aggregation for the wood flour with 120 min of wet milling time. As the particle size decreased, mechanical properties of wood–plastic composite increased for up to 30 min of wet milling time and then slightly decreased. This behavior might be due to aggregation. The optimum mechanical property was obtained at 30 min of wet milling time under freeze-drying conditions.
Wood-based materials are used extensively in residual construction worldwide. Most of the adhesives used in wood-based materials are derived from fossil resources, and some are not environmentally friendly. This study explores nanofiber technology as an alternative to such adhesives. Previous studies have shown that the three-dimensional binding effects of cellulose nanofiber (CNF), when mixed with wood flour, can significantly improve the physical and mechanical properties of wood flour board. In this study, ligno-cellulose nanofibers (LCNF) were fabricated by wet disk milling of wood flour. Composite boards of wood flour and LCNF were produced to investigate the binding effect(s) of LCNF. The fabrication of LCNF by disk milling was simple and effective, and its incorporation into wood flour board significantly enhanced the physical and mechanical properties of the board.
12 March 2018 in Journal of Wood Chemistry and Technology
Maleic anhydride-modified polypropylene (MAPP) is a compatibilizer used to improve the physical and mechanical properties of many wood/plastic composites (WPCs). The properties of WPCs containing MAPP differ according to the characteristics of the specific MAPP that it is used. In this study, the physical and mechanical properties, including shear viscosity, of polypropylene-based WPCs containing different types of MAPP were investigated before and after water absorption. The shear viscosity of MAPP increased with increasing molecular weight, but remained nearly constant for WPCs containing different types of MAPP. In dry conditions, the strongest WPC contained the MAPP with the highest acid value. The highest flexural modulus was observed with the WPC containing the MAPP with the highest molecular weight. In wet conditions, the WPC exhibiting the best mechanical properties contained a MAPP with a molecular weight of 58,000.
Wood-based materials are fabricated with adhesives composed of various materials derived from fossil fuels. It is difficult to identify replacements for these chemical adhesives. This study explored nanofiber technologies as an alternative to these adhesives. In this study, we focused on reinforcement effects of lingo-cellulose nanofiber (LCNF) on fiberboards made from softwood and hardwood fiber. We discuss the density effects of reinforcement with LCNF because the density of medium-density fiberboard (MDF), which is widely used for construction, is standardized at about 0.60–0.80 g/cm3. Fiberboards were manufactured with three densities (0.60, 0.75, and 1.00 g/cm3). For softwood fiberboards, the bending properties for LCNF-mixed boards were higher than those for the control fiberboards at all densities. In this paper, control fiberboard means fiberboard with fiber only. For hardwood fiberboards, the bending properties for LCNF-mixed fiberboard for 1.00 g/cm3-density board were higher than those for the control fiberboard. For internal bond strength (IB), the IB for LCNF-mixed fiberboard was higher than that for the control fiberboard. The thickness swelling (TS) and weight change (WC) with water absorption for fiberboards containing LCNF were lower than those for control fiberboards. As a conclusion, physical and mechanical properties of the resulting fiberboards were significantly improved with the addition of LCNF, especially for softwood fiberboards, due to close binding between LCNF and wood fibers.