This study presents the key mechanical and residual properties after high-temperature of different Nano SiO2 carbon fiber-reinforced concrete (NSCFRC) mixtures. A total of seven NSCFRC mixtures incorporating 0%–0.35% of carbon fiber by volume of concrete and 0%–2% Nano SiO2 by weight of the binder were studied. The key mechanical properties such as compressive strength, tensile strength, and flexural strength of NSCFRC with 0.25% carbon fiber and 1% NS were 6.8%, 20.3%, and 11.7% higher than PC (0% CFs, 0% NS), respectively. Scanning Electron Microscopy (SEM) shows that Nano SiO2 reduced the internal porosity and increased the compactness of the concrete matrix. Furthermore, the experimental result demonstrates that NSCFRC can improve the mechanical properties of concrete after high-temperature and equations were obtained to describe the evolution of residual properties at elevated temperatures. Results suggested that the effect of carbon fibers on the residual properties of concrete after high-temperature is less than steel fiber and polypropylene fiber. It was also indicated that adding appropriate Nano SiO2 to concrete is an effective means to improve the residual performance after high-temperature.
In this paper, Ag-TiO2 photocatalysts with different Ag contents (1 mol%–5 mol%) were prepared and applied to cement mortar. The photocatalytic performance of Ag-TiO2 and photocatalytic cement mortar under UV light and simulated solar light was evaluated. The results showed that Ag loading on the surface of TiO2 could reduce its band gap width and increase its absorbance in the visible region, and 2% Ag-TiO2 had the highest photocatalytic activity under UV light, the degradation rate of methyl orange (MO) was 95.5% at 30 min, and the first-order reaction constant k was 0.0980 min−1, which was 61.7% higher than that of TiO2, and 5% Ag-TiO2 had the highest photocatalytic activity under solar light, the degradation rate of methylene blue (MB) was 69.8% at 40 min, and the first-order reaction constant k was 0.0294 min−1, which was 90.9% higher than that of TiO2. The photocatalytic mortar prepared by the spraying method has high photocatalytic performance, The MO degradation rate of sample S2 under UV light was 87.5% after 120 min, MB degradation rate of sample S5 under solar light was 75.4% after 120 min. The photocatalytic reaction conforms to the zero-order reaction kinetics, which was 1.5 times–3.3 times higher than that of the mixed samples and has no effect on the mechanical properties of mortar.
1 July 2013 in Rare Metal Materials and Engineering