Oxide dispersion-strengthened (ODS) materials contain homogeneous dispersions of temperature-stable nano-oxides serving as obstacles for dislocations and further pinning of grain boundaries. The strategy for dispersion strengthening based on complex oxides (Y-Hf, -Zr, -Ce, -La) was developed in order to refine oxide dispersion to enhance the dispersion strengthening effect. In this work, the strengthening of EUROFER steel by complex oxides based on Y and elements of the IIIB group (lanthanum, scandium) and IVB group (cerium, hafnium, zirconium) was explored. Interparticle spacing as a dispersoid characteristic appeared to be an important factor in controlling the dispersion strengthening contribution to the yield strength of ODS EUROFER steels. The dispersoid size and average grain size of ODS EUROFER steel were altered in the ranges of 5–13 nm and 0.6–1.7 µm, respectively. Using this strategy, the yield strength of the prepared alloys varied between 550 MPa and 950 MPa depending on the doping element.
This work describes the behavior of T91 (9Cr ferritic-martensitic steel), MA957 ODS (14%Cr, 0.3Mo, 0.9Ti, 0.25%Y2O3) and PM2000 ODS (19%Cr, 5%Al, 0.25%Y2O3) steels produced by mechanical alloying process, after long-term exposure to liquid lead-bismuth eutectic. Small bend specimens were pre-strained, then exposed to flowing lead-bismuth at 350°C for 100, 500 and 1000 hours. After exposure, the specimens were examined by using SEM equipped with EDX. The resulting changes of surface and built-up oxide layers are discussed. Liquid Metal Embrittlement, LME, crack initiation was not observed in the specimens. The absence of LME in these conditions is discussed.
This paper studies the impact fracture behavior of the 14%Cr Oxide Dispersion Strengthened (ODS) steel (ODM401) after high temperature exposures in helium and air in comparison to the as-received state. A steel bar was produced by mechanical alloying and hot-extrusion at 1150 °C. Further, it was cut into small specimens, which were consequently exposed to air or 99.9% helium in a furnace at 720 °C for 500 h. Impact energy transition curves are shifted towards higher temperatures after the gas exposures. The transition temperatures of the exposed states significantly increase in comparison to the as-received steel by about 40 °C in He and 60 °C in the air. Differences are discussed in terms of microstructure, surface and subsurface Scanning Electron Microscope (SEM) and Transmission Electron Microscope (TEM) observations. The embrittlement was explained as temperature and environmental effects resulting in a decrease of dislocation level, slight change of the particle composition and interface/grain boundary segregations, which consequently affected the nucleation of voids leading to the ductile fracture.