Tobias Tauböck

Prof. Dr. Tobias Tauböck

Department of Conservative and Preventive Dentistry, Center for Dental Medicine, University of Zurich, Plattenstrasse 11, Zurich, Switzerland

Research Focus & Metrics

Academic Career Length

16Years (2011-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
1 November 2015 in Journal of Dentistry
Verified
Journal Article
Open access
Tobias TauböckTobias Tauböck
Tobias Tauböck
ZTZrinka Tarle
Zrinka Tarle
Danijela MarovićDanijela Marović
Danijela Marović
TAThomas Attin
Thomas Attin
To investigate the influence of pre-heating of high-viscosity bulk-fill composite materials on their degree of conversion and shrinkage force formation. Four bulk-fill composite materials (Tetric EvoCeram Bulk Fill-TECBF, x-tra fil-XF, QuixFil-QF, SonicFill-SF) and one conventional nano-hybrid resin composite (Tetric EvoCeram-TEC) were used. The test materials were either kept at room temperature or pre-heated to 68°C by means of a commercial heating device, before being photoactivated with a LED curing unit for 20s at 1170mW/cm(2). Shrinkage forces (n=5) of 1.5-mm-thick specimens were recorded in real-time for 15min inside a temperature-controlled chamber at 25°C (simulating intraoral temperature after rubber dam application) with a custom-made stress analyzer. Degree of conversion (n=5) was determined at the bottom of equally thick (1.5mm) specimens using Fourier transform infrared spectroscopy. Data were analyzed with Student's t-test, ANOVA and Tukey's HSD post-hoc test (α=0.05). Composite pre-heating significantly increased the degree of conversion of TECBF, but had no effect on monomer conversion of the other materials investigated. For each of the test materials, pre-heated composite generated significantly lower shrinkage forces than room-temperature composite. At both temperature levels, TECBF created the significantly highest shrinkage forces, and QF caused significantly higher shrinkage forces than both XF and TEC. Both the composite material and the pre-cure temperature affect shrinkage force formation. Pre-heating of bulk-fill and conventional restorative composites prior to photoactivation decreases polymerization-induced shrinkage forces without compromising the degree of conversion. Composite pre-heating significantly reduces shrinkage force formation of high-viscosity bulk-fill and conventional resin composites, while maintaining or increasing the degree of monomer conversion, dependent upon the specific composite material used.


11 July 2014 in European Journal of Oral Sciences
Verified
Journal Article
Closed access
PDF file
Tobias TauböckTobias Tauböck
Tobias Tauböck
AFAlbert J. Feilzer
Albert J. Feilzer
WBWolfgang Buchalla
Wolfgang Buchalla
CKCornelis J. Kleverlaan
Cornelis J. Kleverlaan
IKIvo Krejci
Ivo Krejci
TAThomas Attin
Thomas Attin

1 October 2020 in Journal of Dentistry
Verified
Journal Article
Open access
Matej ParMatej Par
Matej Par
Danijela MarovićDanijela Marović
Danijela Marović
TAThomas Attin
Thomas Attin
ZTZrinka Tarle
Zrinka Tarle
Tobias TauböckTobias Tauböck
Tobias Tauböck
To compare the effect of high-intensity (3 s with 3440 mW/cm2) and conventional (10 s with 1340 mW/cm2) light-curing on shrinkage properties and degree of conversion of conventional and bulk-fill resin composites, including two composites specifically designed for high-intensity curing. Real-time linear shrinkage and shrinkage force of 1.5 mm thick composite specimens were measured for 15 min after the start of light-curing using custom-made devices. From the shrinkage force data, maximum shrinkage force rate and time to achieve maximum shrinkage force rate were determined. Degree of conversion was measured using Fourier transform infrared spectrometry. Flowable composites showed significantly higher linear shrinkage compared to sculptable composites (1.93-2.91 % vs. 1.15-1.54 %), as well as significantly higher shrinkage forces (18.7-24.4 N vs. 13.5-17.0 N). Degree of conversion amounted to 45.8-60.1 %. For high-intensity curing, degree of conversion was significantly lower in three out of seven composites, whereas shrinkage forces were either increased, decreased, or unchanged compared to conventional curing. For high-intensity curing, maximum shrinkage rates were 6-61 % higher, whereas times to achieve maximum shrinkage force rate were 15-53 % shorter compared to conventional curing. Composites specifically designed for high-intensity curing showed shrinkage parameters comparable to other investigated composites. Shrinkage behavior under conditions of high-intensity light-curing was material-dependent. Shrinkage force kinetics were more strongly affected by high-intensity curing than absolute values of linear shrinkage and shrinkage force. Despite being attractive for its convenience, high-intensity curing can lead to considerably faster development of shrinkage forces in the early stage of polymerization.

12 March 2020 in Journal of Clinical Medicine
Verified
Journal Article
Open access
PDF file
ROReto Odermatt
Reto Odermatt
Matej ParMatej Par
Matej Par
DMDirk Mohn
Dirk Mohn
DWDaniel B Wiedemeier
Daniel B Wiedemeier
TAThomas Attin
Thomas Attin
Tobias TauböckTobias Tauböck
Tobias Tauböck
Bioactive resin composites can contribute to the prevention of secondary caries, which is one of the main reasons for failure of contemporary dental restorations. This study investigated the effect of particle size of bioactive glass 45S5 on chemical and physical composite properties. Four experimental composites were prepared by admixing the following fillers into a commercial flowable composite: (1) 15 wt% of micro-sized bioactive glass, (2) 15 wt% of nano-sized bioactive glass, (3) a combination of micro- (7.5 wt%) and nano-sized (7.5 wt%) bioactive glass, and (4) 15 wt% of micro-sized inert barium glass. Hydroxyapatite precipitation and pH rise in phosphate-buffered saline were evaluated during 28 days. Degree of conversion and Knoop microhardness were measured 24 h after specimen preparation and after 28 days of phosphate-buffered saline immersion. Data were analyzed using non-parametric statistics (Kruskal–Wallis and Wilcoxon tests) at an overall level of significance of 5%. Downsizing the bioactive glass particles from micro- to nano-size considerably improved their capability to increase pH. The effect of nano-sized bioactive glass on degree of conversion and Knoop microhardness was similar to that of micro-sized bioactive glass. Composites containing nano-sized bioactive glass formed a more uniform hydroxyapatite layer after phosphate-buffered saline immersion than composites containing exclusively micro-sized particles. Partial replacement of nano- by micro-sized bioactive glass in the hybrid composite did not impair its reactivity, degree of conversion (p > 0.05), and Knoop microhardness (p > 0.05). It is concluded that downsizing bioactive glass particles to nano-size improves the alkalizing potential of experimental composites with no negative effects on their fundamental properties.

7 June 2022 in Materials
Verified
Journal Article
Open access
PDF file
Danijela MarovićDanijela Marović
Danijela Marović
Matej ParMatej Par
Matej Par
KPKarlo Posavec
Karlo Posavec
IMIvana Marić
Ivana Marić
DŠDominik Štajdohar
Dominik Štajdohar
ZTZrinka Tarle
Zrinka Tarle
The objective was to evaluate new commercially available ion-releasing restorative materials and compare them to established anti-cariogenic materials. Four materials were tested: alkasite Cention (Ivoclar Vivadent) in self-cure or light-cure mode, giomer Beautifil II (Shofu), conventional glass-ionomer Fuji IX (GC), and resin composite Tetric EvoCeram (Ivoclar Vivadent) as a control. Flexural strength, flexural modulus, and Weibull modulus were measured one day, three months, and after three months with accelerated aging in ethanol. Water sorption and solubility were evaluated for up to one year. Degree of conversion was measured during 120 min for self-cured and light-cured Cention. In this study, Beautifil II was the ion-releasing material with the highest flexural strength and modulus and with the best resistance to aging. Alkasite Cention showed superior mechanical properties to Fuji IX. Weibull analysis showed that the glass-ionomer had the least reliable distribution of mechanical properties with the highest water sorption. The solubility of self-cured alkasite exceeded the permissible values according to ISO 4049. Degree of conversion of light-cured Cention was higher than in self-cure mode. The use of alkasite Cention is recommended only in the light-cure mode.