Ni‐rich layered lithium metal oxides are the cathode active materials of choice for high‐energy‐density Li‐ion batteries. While the high content of Ni is responsible for the excellent capacity, it is also the source of interfacial instability, limiting the material's lifetime due to a variety of correlated in‐ and extrinsic factors. Hence, reconciling the opposing trends of high Ni content and long‐term cycling stability by modifying the material's surface is one of the challenges in the field. Here, we review various studies on surface modification of Ni‐rich (≥ 80 %) layered cathode active materials in order to categorize current research efforts. Broadly, the three strategies of coating, surface doping and washing are discussed, each with their advantages and shortcomings. In conclusion, we highlight new directions of research that could bring Ni‐rich layered lithium metal oxide cathodes from the laboratory to the real world.
Multicomponent materials may exhibit favorable Li‐storage properties because of entropy stabilization. While the first examples of high‐entropy oxides and oxyfluorides show good cycling performance, they suffer from various problems. Here, we report on side reactions leading to gas evolution in Li‐ion cells using rock‐salt (Co0.2Cu0.2Mg0.2Ni0.2Zn0.2)O (HEO) or Li(Co0.2Cu0.2Mg0.2Ni0.2Zn0.2)OF (Li(HEO)F). Differential electrochemical mass spectrometry indicates that a robust solid‐electrolyte interphase layer is formed on the HEO anode, even when using an additive‐free electrolyte. For the Li(HEO)F cathode, the cumulative amount of gases is found by pressure measurements to depend strongly on the upper cutoff potential used during cycling. Cells charged to 5.0 V versus Li+/Li show the evolution of O2, H2, CO2, CO and POF3, with the latter species being indirectly due to lattice O2 release as confirmed by electron energy loss spectroscopy. This result attests to the negative effect that lattice instability at high potentials has on the gassing.
A remarkable enhancement of electro-catalytic activity of a cobalt-free (La 0.6 Sr 0.4 ) 0.98 FeO 3−δ electrode by applying a nanoengineered hybrid catalyst coating via co-infiltration.
The state-of-the-art oxygen electrode materials used in solid oxide cells at 600–800 °C can deteriorate by gradual passivation of their surfaces related to changes in the surface chemistry. We have recently observed the unexpected recovery of the oxygen-exchange activity on La0.6Sr0.4FeO3 after short-term exposure to high temperatures; a 10 h-long thermal treatment at above 800 °C resulted in a 40-fold increase in the oxygen-exchange coefficient, kchem, from 1 × 10–5 to 4 × 10–4 cm/s. The present work addresses the underlying mechanism of this improvement by investigating the chemical and morphological changes at the surface with respect to thermal history. Using repeated sequences of 10 h-long thermal treatments at 1000 °C over weeks-long aging at around 650 °C, we have probed the oxygen-exchange kinetics and surface chemistry concurrently by electrical conductivity relaxation and X-ray photoelectron spectroscopy (XPS). The oxygen-exchange coefficient decreases with aging at 650 °C following Avrami-type kinetics but sharply increases after each high-temperature treatment. An increased amount of strontium [40% cation fraction; XSr/(XLa + XSr + XFe)] is found on the surface of all thermally treated samples (compared to the bulk nominal 20%). Hence, the passivation/reactivation is not due to the total Sr enrichment as such. By XPS, two different states of Sr are observed on the surface (labeled “lattice-bound” and “secondary phase”). The relative amounts in these two phases vary with time, differently at 650 °C versus 1000 °C. The amount of “lattice-bound Sr” decreases and the amount of “secondary phase Sr” increases with aging at 650 °C and the opposite at 1000 °C. We show that it is the Sr in the secondary phases, rather than the total amount, which is the main culprit for performance degradation. The findings are further supported by the observations of morphological changes on the surface in the form of SrO, SrCO3, and SrSO4 precipitates and layers. Decomposition of secondary Sr phases at 1000 °C and simultaneous dissolution of Sr back in a perovskite lattice rejuvenate the surface and lead to a significant increase in exchange kinetics.
The rate of oxygen surface exchange on (La0.6Sr0.4)0.99CoO3−δ (LSC) and (La0.6Sr0.4)0.98FeO3−δ (LSF) was investigated by means of Electrical Conductivity Relaxation (ECR) in oxidizing atmospheres (0.2–0.1 bar pO2) from 650 °C to 900 °C. We observed reversible and reproducible changes in materials' performance as a consequence of thermal treatment, manifested through drastic changes in surface exchange coefficient (kchem) and the related activation energy with thermal history. The effect is found to be more pronounced in case of LSF, where kchem at 650 °C and 0.1 bar pO2 can vary from 3 × 10−4 to 1.1 × 10−5 cm s−1, while bulk properties such as electrical conductivity and the chemical diffusion coefficient of oxygen remain constant. The changes are related to a surface-confined phenomenon and the transition from one state to another is found to follow classical models of nucleation and growth processes. The findings demonstrate the importance of thermal history for studies of oxygen exchange kinetics in perovskite materials and offer an explanation for some of the discrepancies found in the literature.