In order to quantitatively study the difference in occurrence content of functional groups in coals with different metamorphic degrees, the samples of long flame coal, coking coal, and anthracite of three different coal ranks were characterized by FTIR and the relative content of various functional groups in different coal ranks was obtained. The semi-quantitative structural parameters were calculated, and the evolution law of the chemical structure of the coal body was given. The results show that with the increase in the metamorphic degree, the substitution degree of hydrogen atoms on the benzene ring in the aromatic group increases with the increase in the vitrinite reflectance. With the increase in coal rank, the content of phenolic hydroxyl, carboxyl, carbonyl, and other active oxygen-containing groups gradually decreased, and the content of ether bonds gradually increased. Methyl content increased rapidly first and then increased slowly, methylene content increased slowly first and then decreased rapidly, and methylene content decreased first and then increased. With the increase in vitrinite reflectance, the OH-π hydrogen bond gradually increases, the content of hydroxyl self-association hydrogen bond first increases and then decreases, the oxygen-hydrogen bond of hydroxyl ether gradually increases, and the ring hydrogen bond first significantly decreases and then slowly increases. The content of the OH-N hydrogen bond is in direct proportion to the content of nitrogen in coal molecules. It can be seen from the semi-quantitative structural parameters that with the increase in coal rank, the aromatic carbon ratio fa, aromatic degree AR and condensation degree DOC increase gradually. With the increase in coal rank, A(CH2)/A(CH3) first decreases and then increases, hydrocarbon generation potential ‘A’ first increases and then decreases, maturity ‘C’ first decreases rapidly and then decreases slowly, and factor D gradually decreases. This paper is valuable for analyzing the occurrence form of functional groups in different coal ranks and clarifying the evolution process of structure in China.
25 June 2019 in Energy Sources, Part A: Recovery, Utilization, and Environmental Effects
To explore the propagation of gas explosions in roadways, test pipes with circular, square, rectangular, and trapezoidal cross-sections were used to monitor the temperature and pressure changes. The results showed the longest time was required for the flame to fill the roadway with a trapezoidal cross-section. The highest temperature was observed for the square cross-section. The maximum explosion pressures in the roadways was about 0.6 MPa, but the longest time was required in the roadway with a trapezoidal cross-section, while the gas explosion temperature was the lowest, and the time to reach the maximum explosion pressure was the longest.
An in-depth investigation of the adsorption and diffusion mechanism of hydrogen in low-rank coals is of great significance for optimizing the technical path of geological hydrogen storage and improving the efficiency of hydrogen storage. Two kinds of coal samples with a low metamorphic degree from Foran Coal Mine and Sihe Coal Mine were used as adsorbents, and the metamorphic degree and molecular structure of the coal samples were determined experimentally, and the adsorption and diffusion mechanism of H2 molecules in the structure of low metamorphic coal was analyzed from the atomic level based on numerical simulation. It was found that the aliphatic carbon in the low-rank coal mainly links the aromatic ring in the form of a branched chain and exists as an aliphatic ring, side chain, or bridging carbon, and the lower the deterioration degree of the coal, the longer the length of the alkane side chain in the molecular structure. The branched structure present in the aliphatic carbon and the polybenzene ring structure present in the aromatic carbon can provide more effective adsorption sites and enhance the adsorption of H2 by the low-rank coal structure. High specific surface area and porosity will enhance the adsorption of H2 from coal samples, while the presence of oxygen-containing functional groups in low-rank coals will strengthen the interaction between the microporous structure and H2. These findings provide theoretical support for the application of low-rank coals in geological hydrogen storage.
To clarify the complex relationship between the factors causing safety accidents in metallurgical enterprises and predict the risk of accidents in enterprises, a correlation analysis model of the factors causing safety accidents in metallurgical enterprises based on grey Decision-Making Trial and Evaluation Laboratory/Interpretative Structural Modeling (DEMATEL/ISM) was established, and a Bayesian network early warning model was constructed on this basis. The relationship and action path of accident-causing factors in metallurgical enterprises were clarified. The factors were hierarchically divided and a multi-layer hierarchical structure model was established to obtain the neighboring cause, transitional cause, and essential cause of the accident. The results showed that the employee violation rate, the hazardous substances reserves, the toxic gas and dust pollution control compliance rate, the pass rate for equipment maintenance, and the qualification rate of special equipment were the neighboring causes of the accident. The perfection of the safety production management system was the essential cause. The Bayesian network early warning model was applied to the Fuxin Jiuxing Titanium work site. The expected risk probability of an accident was 17.9%, which was in a comparatively safe state (State2). The results obtained by the Bayesian model are consistent with those obtained by AHP and fuzzy comprehensive evaluation method, which proved the accuracy of the early warning model. The Bayesian model can give the risk probability value of the accident and the risk probability value of the accident cause factors at the same time, and include the causal relationship and conditional correlation relationship among the indicator variables in the reasoning process, which can provide targeted technical support for the construction of the emergency system of risk classification management and control.
In fluid networks, flow fluctuation is an important indicator for fluid network stability. However, changes of flow are affected by a variety of factors, and flow resistance change is one of the common influencing factors. Changes in branch flow resistance can cause changes in the flow in that branch and others, which will affect the stability of the entire fluid network. In order to quantitatively analyze the effect of branch flow resistance changes on flow fluctuation, this study introduced the concept of building a sensitivity-based mathematical model and calculated the sensitivity of each branch to construct a sensitivity matrix, and then, based on the uniqueness of the correspondence between the system state and the sensitivity matrix, sensitivity was used to quantitatively describe the system state. In the sensitivity matrix, the column element indicates the sensitivity of the flow resistance change in one branch to the flow change in other branches; the row element indicates the sensitivity of the branch flow change to the flow resistance change in other branches. This study proposed an algorithm which can quickly and accurately calculate the sensitivity value, and it gave a detailed solution to the problem of over-iteration and ill-conditioned solution in the sensitivity solution process. It was verified by an example that the method can accurately describe the influence of the flow resistance change from a branch in a fluid network on the flow in itself and other branches. The fluid network stability theory based on sensitivity has certain guiding significance for the design and optimization of fluid networks.
Based on comprehensive experimental datasets—proximate/ultimate analyses, XPS, solid-state 13C NMR, and Raman spectroscopy—we constructed and optimized a compositionally faithful macromolecular model of SG coking coal. Using density-functional theory (DFT) calculations, we simulated electrostatic-potential (ESP) fields and frontier molecular orbitals (FMO) to probe elementary oxidation steps relevant to combustion, and focused on how heteroatom speciation and carbon ordering govern site-selective reactivity. Employing multi-peak deconvolution and parameter synthesis, we obtained an aromatic fraction fa = 76.56%, a bridgehead-to-periphery ratio XBP = 0.215, and Raman indices ID1/IG ≈ 1.45 (area) with FWHM(G) ≈ 86.7 cm−1; the model composition C190H144N2O21S and its predicted 13C NMR envelope validated the structural assignment against experiment. ESP–FMO synergy revealed electron-rich hotspots at phenolic/ether/carboxyl and thiophenic domains and electron-poor belts at H-terminated edges/aliphatic bridges, rationalizing carbon-end oxidation of CO, weak electrostatic steering by O2/CO2, and a benzylic H-abstraction → edge addition → O-insertion/charge-transfer sequence toward CO2/H2O, with thiophenic sulfur comparatively robust. We quantified surface functionalities (C–O 65.46%, O–C=O 24.51%, C=O 10.03%; pyrrolic/pyridinic N dominant; thiophenic-S with minor oxidized S) and determined a naphthalene-dominant, stacked-polyaromatic architecture with sparse alkyl side chains after Materials Studio optimization. The findings are significant for mechanistic understanding and control of coking-coal oxidation, providing actionable hotspots and a reproducible workflow (multi-probe constraints → model building/optimization → DFT reactivity mapping → spectral back-validation) for blend design and targeted oxidation-inhibition strategies.