Photochemical cathodic protection (PEC) efficiency was enhanced by doping TiO2 with Cu (Cu/TiO2) through impregnation and reduction under hydrogen. The Cu loading was vaired from 0.1 to 1.0 mol% (0.1 Cu/TiO2, 0.5 Cu/TiO2, 1 Cu/TiO2). Then, up to 50 wt% Cu/TiO2 was mixed with TiO2 to form nanocomposite films. The film photocurrent and photopotential were measured under 1 mW/cm2 UV irradiation. The Cu/TiO2 film with 10 wt% of 0.5 Cu/TiO2 exhibited the highest photocurrent of 29.0 mA/g, which was three times higher than the TiO2 film. The underlying reason for the high photocurrent was the lower photopotential of film than the corrosion potential of copper for PEC. This film was also applied on copper terminal lug for anti-corrosion measurement by Tafel polarization in 3.5 wt% NaCl solution. The results showed that the photopotential of terminal lug coated with the film was −0.252 V vs. Ag/AgCl, which was lower than the corrosion potential of copper (−0.222 V vs. Ag/AgCl). Furthermore, the film can protect the corrosion of copper in the dark with 86.7% lower corrosion current (icorr) than that of bare copper.
Titanium dioxide is used extensively in ultraviolet-visible irradiation to induce oxidation. However, this method relies on daylight harvesting. Alternatively, our experiment utilized titanium dioxide directly under thermal excitation. Three different titanium oxide-based catalysts, i.e., commercial titanium dioxide Degussa P25, black titanium dioxide, and black titanium dioxide modified with copper oxide, were investigated at moderate temperatures (70 and 120 °C). The utilization of titanium-based catalysts with tert-butyl hydroperoxide (TBHP) in alkaline water is practical for oxidizing carbonyl derivatives of furan to one or two carbon-less carboxylic acids, such as succinic acid (selective to 38-87%), furoic acid (selective to 0-70%), and maleic acid (selective to 3-39%), under moderate conditions. These titanium-based catalysts differ in their physicochemical properties, resulting in variations in their catalytic activity and selectivity, and are active at different temperatures. Electron paramagnetic resonance (EPR) revealed no traces of oxygen vacancy sites on the titanium oxide. In contrast, black titanium dioxide consisted of an oxygen vacancy with one electron, whereas copper-modified black titanium dioxide consisted of a doubly ionized oxygen vacancy.
Nickel supported on a zeolite Linde Type A 5A (zeolite LTA 5A) catalyst (Ni/zeolite LTA 5A) was fabricated into cylindrical pellets using two types of binders: methylcellulose (MC) with poly(vinyl alcohol) (PVA) and glutinous flour (GF). Carbon dioxide methanation was conducted under atmospheric pressure at 200–500 °C. The gas hourly space velocity (GHSV) was varied from 1,125 to 15,000 h–1, corresponding to volumetric flow rates of 60–500 mL/min. The conversion of carbon dioxide to methane decreased as GHSVs increased. Fabricated catalysts produced higher methane yields than the catalyst powder, with CO2-to-CH4 conversion rates of 70–90% and 10–90%, respectively. The CO2 conversion of the catalyst with MC+PVA approached 90% at 400 °C, superior to that of the catalyst with GF, which reached 84% at the same temperature and a volumetric flow rate of 60 mL min–1. The most active temperature for CO2 methanation was 400 °C, and nearly all catalysts were selective to methane, with selective rates exceeding 80%. The stabilities of the fabricated catalysts were tested over 96 h. The stability of the catalyst with MC+PVA was noncomparable to that of the catalyst with GF, since the catalyst with MC+PVA exhibited a 1–6% reduction in activity after 36 h, owing to nickel metal sintering, whereas the catalyst with GF binder exhibited minor fluctuations and remained stable within 96 h. The employed catalysts lost their configurated shapes, existing only as small particles due to binder decomposition.