Despite the consensus on the constructive effect of LPSO (long-period stacking-ordered) phases, the true effect of bulk LPSO phases on strengthening and toughening in deformed magnesium alloys is still controversial. This article, which introduces the alloys Mg-8Gd-4Y-0.6Zn-0.5Zr, without bulk LPSO phases, and Mg-8Gd-4Y-1.6Zn-0.5Zr, containing bulk LPSO phases, details a systematically comparative analysis conducted to clarify the true contribution of bulk LPSO phases to the properties of as-extruded alloys. The results indicate that bulk LPSO phases significantly improve strength by refining grain sizes remarkably. But contrary to expectations, bulk LPSO phases themselves only provide a small strengthening effect and deteriorate plasticity, ascribed to the poor compatible plastic deformation of bulk LPSO phases. More importantly, this work may offer new insights into the strengthening and toughening of LPSO phases for further research and engineering applications of this series of alloys. Additionally, an example of a design strategy for Mg-Gd-Y-Zn alloys with superior strength and excellent plasticity is proposed at the end of this article.
Mg–Sn–Al alloy is a new type of heat-resistant magnesium alloy with great potential and the hot deformation process of this alloy is of great significance for its application. The microstructure, hot deformation behavior, textural evolution, and processing map of a Mg–8 wt.% Sn–1.5 wt.% Al alloy were studied. A Gleeble 1500 D thermo-mechanical simulator was used. The temperature of deformation was 653 to 773 K, the strain rate was 0.001–1 s−1, and the maximum deformation degree was 60%. The obtained results show that the rheological stress of the alloy decreases with an increase in deformation temperature and increases with an increase in the strain rate. The alloy is completely dynamically recrystallized at 653 K, and the entire structure is formed of homogeneous crystals/grains, with small secondary phase particles distributed at the crystal boundary. The mean apparent activation energy of hot compression deformation is 153.5 kJ/mol. The Mg–8 wt.% Sn–1.5 wt.% Al alloy exhibits excellent plastic deformation properties, an expansive thermal processing interval, and a narrow instability zone under the test temperature and deformation rate. The optimal process parameters of the alloy comprise deformation temperatures between 603 and 633 K and strain rates of 0.03 to 0.005 s−1.