Epoxy resin plays a key role in composite matrices and DGEBA is the major precursor used. With the aim of favouring the use of bio resources, epoxy resins can be prepared from lignin. In particular, diglycidyl ether of isoeugenol derivatives are good candidates for the replacement of DGEBA. This article presents an effective and eco-friendly way to prepare epoxy resin derived from isoeugenol (BioIgenox), making its upscale possible. BioIgenox has been totally characterized by NMR, FTIR, MS and elemental analyses. Curing of BioIgenox and camphoric anhydride with varying epoxide function/anhydride molar ratios has allowed determining an optimum ratio near 1/0.9 based on DMA and DSC analyses and swelling behaviours. This thermoset exhibits a Tg measured by DMA of 165 °C, a tensile storage modulus at 40 °C of 2.2 GPa and mean 3-point bending stiffness, strength and strain at failure of 3.2 GPa, 120 MPa and 6.6%, respectively. Transposed to BioIgenox/hexahydrophtalic anhydride, this optimized formulation gives a thermoset with a Tg determined by DMA of 140 °C and a storage modulus at 40 °C of 2.6 GPa. The thermal and mechanical properties of these two thermosets are consistent with their use as matrices for structural or semi-structural composites.
Extension of hydroxytelechelic polybutadiene oligomers ( 3200 g/mol) is performed in mild conditions, in order to avoid backbone modifications, using succinic anhydride or methylenedicyclohexyl diisocyanate. The two routes present significative extension of the initial oligomers. Extension through the anhydride route, in the presence of DCC and DMAP, leads to new hydroxytelechelic oligomers ( 8000 g/mol). Extension through the diisocyanate route, catalyzed by DBTL at 65°C leads to hydroxytelechelic oligomers of higher average molecular weight ( 20000 g/mol). New materials are characterized by FTIR/1H-NMR and changes in their Tg according to , are discussed. The influence of reaction time on the length of the macromolecular chains is also studied.
This study describes the production of a new biobased epoxy thermoset and its use with long hemp fibres to produce high-performance composites that are totally biobased. The synthesis of BioIgenox, an epoxy resin derived from a lignin biorefinery, and its curing process have been optimised to decrease their environmental impact. The main objective of this study is to characterise the rheology and kinetics of the epoxy system with a view to optimising the composite manufacturing process. Thus, the epoxy resin/hardener system was chosen considering the constraints imposed by the implementation of composites reinforced with plant fibres. The viscosity of the chosen mixture shows the compatibility of the formulation with the traditional implementation processes of the composites. In addition, unlike BPA—a precursor of diglycidyl ether of bisphenol A (DGEBA) epoxy resin—BioIgenox and its precursor do not have endocrine disrupting activities. The neat polymer and its unidirectional hemp fibre composite are characterised using three-point bending tests. Results measured for the fully biobased epoxy polymer show a bending modulus, a bending strength, a maximum strain at failure and a Tg of, respectively, 3.1 GPa, 55 MPa, 1.82% and 120 °C. These values are slightly weaker than those of the DGEBA-based epoxy material. It was also observed that the incorporation of fibres into the fully biobased epoxy system induces a decrease in the damping peak and a shift towards higher temperatures. These results point out the effective stress transfers between the hemp fibres and the fully biobased epoxy system. The high mechanical properties and softening temperature measured in this work with a fully biobased epoxy system make this type of composite a very promising sustainable material for transport and lightweight engineering applications.
27 September 2022 in Acta Crystallographica Section E Crystallographic Communications
The title compound, C13H16O3 [GE-isoEu; systematic name: 2-({2-methoxy-4-[(E)-1-propen-1-yl]phenoxy}methyl)oxirane], which crystallizes in the triclinic P\overline{1} space group, was synthesized in one step from iso-eugenol, a bio-based phenylpropanoid, with an excess of epichlorohydrin. Colourless prismatic crystals suitable for X-ray diffraction were obtained from a mixture of ethyl acetate and cyclohexane, during purification by column chromatography on silica gel. GE-isoEu, which corresponds to the trans isomer of the monoglycidyl ether of iso-eugenol, is based on a 1,2,4-trisubstituted benzene ring by diglycidyl ether, methoxy and 1-(E)-propenyl groups, respectively. In the crystal, molecules are organized through offset π-stacking interactions. Chemically, GE-isoEu constitutes an intermediate in the synthesis protocol of 2-[3-methoxy-4-(2-oxiranylmethoxy)phenyl]-3-methyloxirane (GEEp-isoEu), a diepoxydized monomer used in the manufacturing of thermosetting resins and intended for the elaboration of bio-composites.