Platinum (Pt) is a widely used electrocatalyst material in fuel cells and electrolysers. Proton exchange membrane (PEM) fuel cells and electrolysis operate under highly acidic conditions whereas the more recently developed anion exchange membrane (AEM) processes take place under alkaline conditions. Pt dissolution and Pt oxidation during operation and varying potentials has been studied mainly for the acidic PEM and less for the alkaline AEM. This study presents a comparison of Pt dissolution and Pt oxidation in 0.5 M H2SO4 and 1 M KOH using electrochemical quartz crystal microbalance (EQCM) on Pt thin films. Physical characterisation using electron microscopy and atomic force microscopy (AFM) revealed small, yet significant differences in the Pt film surface structure, which is related to differences in measured electrochemical surface area (ECSA). The mass increase from adsorption of oxygenated species and Pt oxidation is higher in alkaline conditions compared to in acid while dissolution of Pt is similar.
While the market for fuel cell vehicles is increasing, these vehicles will still coexist with combustion engine vehicles on the roads and will be exposed to an environment with significant amounts of contaminants that will decrease the durability of the fuel cell. To investigate different recovery methods, in this study, a PEM fuel cell was contaminated with 100 ppm of NO2 at the cathode side. The possibility to recover the cell performance was studied by using different airflow rates, different current densities, and by subjecting the cell to successive polarization curves. The results show that the successive polarization curves are the best choice for recovery; it took 35 min to reach full recovery of cell performance, compared to 4.5 h of recovery with pure air at 0.5 A cm−2 and 110 mL min−1. However, the performance recovery at a current density of 0.2 A cm−2 and air flow 275 mL min−1 was done in 66 min, which is also a possible alternative. Additionally, two operation techniques were suggested and compared during 7 h of operation: air recovery and air depletion. The air recovery technique was shown to be a better choice than the air depletion technique.
1 January 2026 in International Journal of Energy Research
In recent years, anion exchange membrane fuel cells (AEMFCs) have drawn more attention by showing high performance and potentially allowing catalysts based on more abundant materials. One frequently overlooked parameter in these systems is membranes permeability, often referred to as gas crossover. This undesirable phenomenon creates mixed potentials and also hotspots with temperatures high enough to cause membrane defects and pinholes. Therefore, it is important to investigate it quantitatively at conditions where a fuel cell often operates. In this study, hydrogen and oxygen crossover of several Aemion anion exchange membranes (AEMs) are measured with mass spectrometer (MS) at various relative humidities (RHs) and temperatures. The proton exchange membrane (PEM) Nafion is also investigated for a comparison. AEMs are generally less permeable to oxygen and hydrogen than PEM. The first‐generation AEMs show a decreasing trend in permeability with RH, opposite to PEM. The second‐generationAEMs are much less affected by RH levels. The measured oxygen crossover was two to six times lower compared to hydrogen crossover, depending on the membrane type and RH. The influence of membrane interface on crossover is evaluated to be higher for reinforced membranes, but overall smaller compared to the bulk contribution. Overall, AEMs show lower crossover than PEM, and from that perspective making them more suitable and a safer choice for fuel cell and electrolysis applications.
20 August 2025 in Journal of the Electrochemical Society
The integration of reversible molten carbonate fuel cells (RMCFC) into biomass gasification is a novel concept. However, the knowledge of the electrochemical performance of molten carbonate fuel and molten carbonate electrolysis cells working with raw product gas is currently limited. Electrochemical measurements were performed under varied conditions on a lab-scale RMCFC operating with raw product gas from direct air-steam, direct oxygen-steam, and indirect steam gasification to evaluate this concept while filling the knowledge gap. Our results show that raw product gases generally lead to favourable electrochemical performance similar to hydrogen-rich fuel. However, raw product gas from direct oxygen-steam gasification at 600°C underperforms due to steam reforming and water-gas shift equilibria. These reactions change the gas compositions, generally improving performance while causing a decline under certain conditions. Direct oxygen-steam and indirect steam gasification at 40% inlet humidity and 650°C provide the most promising conditions for RMCFC, with a preference for steam-rich processes. Our study validates this novel concept experimentally, providing direction and realistic cell parameters for future research.