Aluminum-doped ZnO (AZO) has huge prospects in the field of conductive electrodes, due to its low price, high transparency, and pro-environment. However, enhancing the conductivity of AZO and realizing ohmic contact between the semiconductor and AZO source/drain (S/D) electrodes without thermal annealing remains a challenge. Here, an approach called pulsed laser deposition (PLD) is reported to improve the comprehensive quality of AZO films due to the high energy of the laser and non-existence of the ion damage. The 80-nm-thick AZO S/D electrodes show remarkable optical properties (transparency: 90.43%, optical band gap: 3.42 eV), good electrical properties (resistivity: 16 × 10−4 Ω·cm, hall mobility: 3.47 cm2/V·s, carrier concentration: 9.77 × 1020 cm−3), and superior surface roughness (Rq = 1.15 nm with scanning area of 5 × 5 μm2). More significantly, their corresponding thin film transistor (TFT) with low contact resistance (RSD = 0.3 MΩ) exhibits excellent performance with a saturation mobility (µsat) of 8.59 cm2/V·s, an Ion/Ioff ratio of 4.13 × 106, a subthreshold swing (SS) of 0.435 V/decade, as well as good stability under PBS/NBS. Furthermore, the average transparency of the unpatterned multi-films composing this transparent TFT can reach 78.5%. The fabrication of this TFT can be suitably transferred to transparent arrays or flexible substrates, which is in line with the trend of display development.
In this research, a passivated methodology was proposed for achieving good electrical characteristics for back-channel-etch (BCE) typed amorphous Si-Sn-O thin film transistors (a-STO TFTs). This methodology implied that the thermal annealing (i.e., pre-annealing) should be carried out before deposition of a SiOx passivation layer. The pre-annealing played an important role in affecting device performance, which did get rid of the contamination of the lithography process. Simultaneously, the acceptor-like sub-gap density of states (DOS) of devices was extracted for further understanding the reason for improving device performance. It found that the SiOx layer could reduce DOS of the device and successfully protect the device from surroundings. Finally, a-STO TFT applied with this passivated methodology could possess good electrical properties including a saturation mobility of 4.2 ± 0.2 cm2/V s, a low threshold voltage of 0.00 V, a large on/off current ratio of 6.94 × 108, and a steep subthreshold swing of 0.23 V/decade. The threshold voltage slightly shifted under bias stresses and recovered itself to its initial state without any annealing procedure, which was attributed to the charge trapping in the bulk dielectric layers or interface. The results of this study indicate that a-STO TFT could be a robust candidate for realizing a large-size and high-resolution display.
In this work, a high-performance thin film transistor with an neodymium-doped indium zinc oxide (Nd:IZO) semiconductor via a room temperature approach and adopting the Nd:IZO/Al2O3 nanolaminate structure was investigated. The effects of the ultrathin Al2O3 layer and the thickness of Nd:IZO layer in the nanolaminate structure on the improvement of electrical performance and stability of thin film transistors (TFTs) were systematically studied. Besides the carrier movement confined along the near-channel region, driven by the Al2O3 layer under an electrical field, the high performance of the TFT is also attributed to the high quality of the 8-nm-thick Nd:IZO layer and the corresponding optimal Nd:IZO/Al2O3 interface, which reduce the scattering effect and charge trapping with strong M–O bonds in bulk and the back-channel surface of Nd:IZO, according to the X-ray reflectivity (XRR), X-ray photoelectron spectroscopy (XPS), and micro-wave photo conductivity decay (μ-PCD) results. As a result, the Nd:IZO/Al2O3 TFT exhibits an outstanding performance, with a high μsat of 32.7 cm2·V−1·s−1, an Ion/Ioff of 1.9 × 108, and a low subthreshold swing (SS) value of 0.33 V·dec−1, which shows great potential for the room temperature fabrication of TFTs in high-resolution or high-frame-rate displays by a scalable, simple, and feasible approach.
In this work, a thin film transistor (TFT) with Zr-doped aluminum-zinc-tin oxide (Zr-AZTO) semiconductor as active layer was investigated. The Zr-AZTO thin films were co-sputtered by ZrO2 and AZTO targets (RF-Sputter) in Ar, and annealed at 350 °C in air atmosphere. With the discharge power of AZTO increasing from 100 W to 120 W, the content of Zr element decreases from 0.63 ± 0.01 at.% to 0.34 ± 0.01 at.%, and the oxygen vacancy decreases from (19.0 ± 0.1)% to (17.3 ± 0.8)%. The results of Zr-AZTO thin film show that the main factor is the co-sputter power of ZrO2 target. With the co-sputter power of ZrO2 increasing from 15 W to 45 W, the content of Zr element increases from 0.63 ± 0.01 at.% to 2.79 ± 0.01 at.%, the content of oxygen vacancy decreases from (19.0 ± 0.1)% to (14.1 ± 0.1)%, Eg increases from 2.76 eV to 2.86 eV, and the root mean square (RMS) roughness firstly decreases from 0.402 nm to 0.387 nm and then increases to 0.490 nm. The Micro Wave Photo Conductivity Decay (μ-PCD, LTA-1620SP) was used to measure the quality of Zr-AZTO thin film and the mean peak and D value decreases from 139.3 mV to 80.9 mV and from 1.54 to 0.77 as the co-sputter power of ZrO2 increases from 15 W to 45 W, which means it has highest localized states and defects in high ZrO2 co-sputter power. The devices prepared at 15 W (ZrO2)/100 W (AZTO) co-sputter show a best performance, with a μsat of 8.0 ± 0.6 cm2/(V∙S), an Ion/Ioff of (2.01 ± 0.34) × 106, and a SS of 0.18 ± 0.03 V/dec. The device of Sample B has a 0.5 V negative shift under −20 V NBS and 9.6 V positive shift under 20 V PBS.
The indium-free amorphous oxide semiconductor thin film transistor (AOS-TFT) with aluminum (Al) electrodes shows broad application prospects in new-generation display technologies, such as ultra-high definition large-screen display, OLED display and 3D display. In this work, the thin film transistor (TFT) with a zinc-aluminum-tin-oxide (ZATO) semiconductor as the active layer and an Al electrodes as the source and drain (S/D) was investigated. The optical, electrical and semiconductive properties of the ZATO films were evaluated by atomic force microscopy (AFM), ultraviolet–visible spectrophotometry and microwave photoconductivity decay (μ-PCD), respectively. The result shows that the film is smooth and transparent and has low localized states and defects at a moderate oxygen concentration (~5%) and a low sputtering gas pressure (~3 mTorr). After the analysis of the transfer and output characteristics, it can be concluded that the device exhibits an optimal performance at the 623 K annealing temperature with an Ion/Ioff ratio of 5.5 × 107, an SS value of 0.15 V/decade and a saturation mobility (μsat) of 3.73 cm2·V−1·s−1. The ZATO TFT at the 623 K annealing has a −8.01 V negative shift under the −20 V NBS and a 2.66 V positive shift under the 20 V PBS.