This article focuses on wear tests of spur gears made with the use of additive manufacturing techniques from thermoplastic materials. The following additive manufacturing techniques were employed in this study: Melted and Extruded Modelling (FDM) and Fused Filament Fabrication (FFF). The study analysed gears made from ABS M-30 (Acrylonitrile Butadiene Styrene), ULTEM 9085 (PEI Polyetherimide) and PEEK (Polyetheretherketone), and the selection of these materials reflects their hierarchy in terms of economical application and strength parameters. A test rig designed by the authors was used to determine the fatigue life of polymer gears. Gear trains were tested under load in order to measure wear in polymer gears manufactured using FDM and FFF techniques. In order to understand the mechanism behind gear wear, further tests were performed on a P40 coordinate measuring machine (CMM) and a TalyScan 150 scanning instrument. The results of the gear tests made under load allow us to conclude that PEEK is resistant to wear and gear train operating temperature. Its initial topography undergoes slight changes in comparison to ABS M-30 and Ultem 9085. The biggest wear was reported for gears made from Ultem 9085. The hardness of the material decreased due to the loaded gear train’s operating temperature.
Tissue engineering is an interdisciplinary field of science that has developed very intensively in recent years. The first part of this review describes materials with medical and dental applications from the following groups: metals, polymers, ceramics, and composites. Both positive and negative sides of their application are presented from the point of view of medical application and mechanical properties. A variety of techniques for the manufacture of biomedical components are presented in this review. The main focus of this work is on additive manufacturing and 3D printing, as these modern techniques have been evaluated to be the best methods for the manufacture of medical and dental devices. The second part presents devices for skull bone reconstruction. The materials from which they are made and the possibilities offered by 3D printing in this field are also described. The last part concerns dental transitional implants (scaffolds) for guided bone regeneration, focusing on polylactide–hydroxyapatite nanocomposite due to its unique properties. This section summarises the current knowledge of scaffolds, focusing on the material, mechanical and biological requirements, the effects of these devices on the human body, and their great potential for applications.
Additive manufacturing (AM) is a rapidly growing branch of manufacturing techniques used, among others, in the medical industry. New machines and materials and additional processing methods are improved or developed. Due to the dynamic development of post-processing and its relative novelty, it has not yet been widely described in the literature. This study focuses on the surface topography (parameters Sa, Sz, Sdq, Sds, Str, Sdr) of biocompatible polyamide 12 (PA12) samples made by selective laser sintering (SLS) and multi jet fusion (MJF). The surfaces of the samples were modified by commercial methods: four types of smoothing treatments (two mechanical and two chemical), and two antibacterial coatings. The smoothing treatment decreased the values of all analyzed topography parameters. On average, the Sa of the SLS samples was 33% higher than that of the MJF samples. After mechanical treatment, Sa decreased by 42% and after chemical treatment by 80%. The reduction in Sdq and Sdr is reflected in a higher surface gloss. One antibacterial coating did not significantly modify the surface topography. The other coating had a smoothing effect on the surface. The results of the study can help in the development of manufacturing methodologies for parts made of PA12, e.g., in the medical industry.
An important factor having an impact on the condition of machine parts is their surface topography. For instance, in the production of a molded element in casting or injection molding processes, the surface topography of the molding cavity has a significant impact on the surface condition of the product. An analysis of the wear of a mold made with the PolyJet technique was performed in this work, and we examined the surface topography using the stylus method after casting a wax model of the turbine blade. The surface topographies showed a gradual degradation of the mold cavity surface. After the manufacture of 40 castings, there was a significant deformation of the microstructure of the mold cavity. The maximum height value (Sz) parameter had the most dynamic change from 18.980 to 27.920 μm. Its growth dynamics are mainly influenced by maximum peak height (Sp) rather than the maximum pit height (Sv) parameter. In the case of the root mean square height (Sq) and arithmetic mean height (Sa), their gradual increases can be seen from 2.578 to 3.599 μm and from 2.038 to 2.746 μm. In the case of the value of the skewness (Ssk) parameter, a small positive skew was observed. As for the kurtosis (Sku) values, the distributions are clearly leptokurtic.
This research paper aims to explore the mechanical characteristics of polyamide PA12 (PA12) as a 3D material printed utilizing Selective Laser Sintering (SLS) and HP MultiJet Fusion (HP MJF) technologies in order to design and manufacture forearm orthoses. The study assessed the flowability of the materials used and compared the mechanical performance of PA12 with each other using tensile, flexure, and impact tests in five different fabrication orientations: X, Y, Z, tilted 45° XZ, and tilted 45° YZ. The results of the study provide, firstly—the data for testing the quality of the applied polyamide powder blend and, secondly—the data for the design of the orthosis geometry from the aspect of its strength parameters and the safety of construction. The mechanical parameters of SLS specimens had less variation than MJF specimens in a given orientation. The difference in tensile strength between the 3D printing technologies tested was 1.8%, and flexural strength was 4.7%. A process analysis of the forearm orthoses revealed that the HP MJF 5200 system had a higher weekly production capacity than the EOS P396 in a production variance based on obtaining maximum strength parameters and a variance based on maximizing economic efficiency. The results suggest that medical device manufacturers can use additive manufacturing technologies to produce prototypes and small-batch parts for medical applications. This paper pioneers using 3D printing technology with Powder Bed Fusion (PBF) methods in designing and manufacturing forearm orthoses as a low- to medium-volume product. The applied solution addresses the problem of medical device manufacturers with regard to the analysis of production costs and mechanical properties when using 3D printing for certified medical devices.
The development of new solutions in craniofacial surgery brings the need to increase the accuracy of 3D printing models. The accuracy of the manufactured models is most often verified using optical coordinate measuring systems. However, so far, no decision has been taken regarding which type of system would allow for a reliable estimation of the geometrical accuracy of the anatomical models. Three types of optical measurement systems (Atos III Triple Scan, articulated arm (MCA-II) with a laser head (MMD × 100), and Benchtop CT160Xi) were used to verify the accuracy of 12 polymer anatomical models of the left side of the mandible. The models were manufactured using fused deposition modeling (FDM), melted and extruded modeling (MEM), and fused filament fabrication (FFF) techniques. The obtained results indicate that the Atos III Triple Scan allows for the most accurate estimation of errors in model manufacturing. Using the FDM technique obtained the best accuracy in models manufactured (0.008 ± 0.118 mm for ABS0-M30 and 0.016 ± 0.178 mm for PC-10 material). A very similar value of the standard deviation of PLA and PET material was observed (about 0.180 mm). The worst results were observed in the MEM technique (0.012 mm ± 0.308 mm). The knowledge regarding the precisely evaluated errors in manufactured models within the mandibular area will help in the controlled preparation of templates regarding the expected accuracy of surgical operations.