The micromechanisms “slip transfer, slip irreversibility, microplasticity, and fatigue cracking” in titanium alloys are reviewed, with a special emphasis on near-α and α + β alloys. As the interplay between slip activity, microplasticity, and fatigue cracking governs both the microscale and macroscale mechanical response, we reveal how the slip irreversibility and localized dislocation activity at the grain boundaries (GBs) and α/β interfaces generate dislocation pile-ups and strain localization, subsequently driving fatigue crack initiation and propagation. The review highlights the favorable crack initiation along basal planes and the roles of α grain orientations, slip transfer barriers, and the β phase in governing fatigue cracking, while addressing unresolved questions about localized interactions and texture effects. It also explores the complex interactions that govern the effects of microstructures, textures, and defects on fatigue cracking. Ultimately, the review provides a unified framework for linking slip events to microplasticity and to fatigue failure, offering actionable insights for alloy design and fatigue prediction.
Understanding the mechanisms of microstructure evolution and defect formation, and their influence on mechanical properties and fracture mechanisms (from crack initiation to failure stage), is essential for manufacturing high-strength, fatigue-resistant A7075 alloy by selective laser melting (SLM). In this investigation, the A7075 alloy was fabricated using a laser power of 350 W with various hatch spacings of 1.0, 1.5, and 2.0 μm, and scanning speeds of 800, 1100, and 1300 mm/s. The results show that the alloy exhibits an equiaxed grain structure, which varies from coarse grains at small hatch spacing and low scanning speed to fine grains with increasing hatch spacing and scanning speed. The alloys exhibit low tensile strength due to solidification cracking and pores. However, this tensile strength increases with hatch spacing, while it decreases with scanning speed. At small hatch spacing and low scanning speed, fracture occurs through the coalescence of pores and solidification cracking along the weakly bonded grain boundaries (GBs) due to eutectic growth along these boundaries. In contrast, with increasing hatch spacing and scanning speed, fracture occurs through solidification cracking and coalescence of pores. This research provides valuable insights into the microstructure evolution, defect formation, and fracture mechanisms of the A7075 alloy under common processing conditions.
11 June 2026 in Journal of Materials Research and Technology