This study investigated how the water–cement ratio and silica fume concentration affect the compressive strength of cement mortars. This comprehensive study delved into the intricate interplay between water–cement ratio and silica fume concentration, examining their influence on cement-based mortars’ compressive strength and water absorption characteristics. The silica fume concentration was investigated, ranging from 5% to 15% of the cement weight. The investigation employed two distinct mixing techniques, mixing cement and silica fume, before extracting appropriate samples; alternatively, a magnetic stirrer was used to prepare samples by dissolving silica fume in water. The cement mortars were also prepared with three different water–cement ratios: 0.44, 0.47, and 0.5. The interesting findings of compressive tests illuminated a consistent trend across all curing days and mixing methods—a reduction in the water–cement ratio corresponded with a notable increase in compressive strength. However, it is essential to note that the influence of the mixing method on the compressive strength of cement-based mortars is based on the water–cement ratio. The results show that by using the suggested technological method, it was observed that samples prepared with water–cement ratios (W/C) of 0.47 and 0.44 exhibited higher compressive strengths compared to those prepared using the well-known standard mixing method. The compressive test results underscored that the water–cement ratio reduction consistently enhanced the compressive strength in every combination of curing days and mixing techniques. Furthermore, this reduction in the water–cement ratio was correlated with a decrease in water absorption of the mortar. Conversely, the water–cement ratio itself played a pivotal role in defining how the mixing technique affected the compressive strength and water absorption of cement-based mortars. This multifaceted exploration underscores the nuanced relationships between key variables, emphasizing the need for a comprehensive understanding of the intricate factors influencing the mechanical and absorptive properties of cement-based materials.
In this work, multi-walled carbon nanotubes (MWCNTs) have been synthesized using a modified method of solid-phase pyrolysis. The MWCNTs are effectively dispersed using a simple and facile method such as ultrasonic energy without and with surfactant for two different sonication times (15 min and 40 min). In the present study, the effect of MWCNT concentration (0.001, 0.01, 0.05, 0.1 wt.%) on the compressive strengths of cement mortars has been investigated. Compressive tests were carried out on an automatic pressure machine (C089) with a loading rate of 0.5 kN/s at the age of 7 days and 28 days. It is shown that the optimal value of the nanotubes’ concentration does not exist in the case of 15 min of sonication time, whereas the optimal value for 40 min of sonication time without and with surfactant is 0.01%. Moreover, in the absence of surfactants, the strength of the specimen over 7 days of hardening increased by 13%, and by 19.5% in the presence of surfactants. The compressive strength for a curing period of 28 days increased by 6.3% and 13.8%, respectively.
In this work, the effect of biosilica concentration and two different mixing methods with Portland cement on the compressive strength of cement-based mortars were investigated. The following values of the biosilica concentration of cement weight were investigated։ 2.5, 5, 7.5, and 10 wt.%. The mortar was prepared using the following two biosilica mixing methods: First, biosilica was mixed with cement and appropriate samples were prepared. For the other mixing method, samples were prepared by dissolving biosilica in water using a magnetic stirrer. Compressive tests were carried out on an automatic compression machine with a loading rate of 2.4 kN/s at the age of 7 and 28 days. It is shown that, for all cases, the compressive strength has the maximum value of 10% biosilica concentration. In particular, in the case of the first mixing method, the compressive strength of the specimen over 7 days of curing increased by 30.5%, and by 36.5% for a curing period of 28 days. In the case of the second mixing method, the compressive strength of the specimen over 7 days of curing increased by 23.4%, and by 47.3% for a curing period of 28 days. Additionally, using the first and second mixing methods, the water absorption parameters were reduced by 22% and 34%, respectively. Finally, it is worth noting that the obtained results were intend to provide valuable insights into optimizing biosilica incorporation in cement mortar. With the aim of contributing to the advancement of construction materials, this research delves into the intriguing application of biosilica in cement mortar, emphasizing the significant impact of mixing techniques on the resultant compressive strength.
This article touches upon the development of dispersed-reinforced concrete components and the improvement of their physical and mechanical properties. They can be used in road and defense structures, bridges, and takeoff and landing zones. Multifunctional micro-reinforced fine-grained concrete compositions have been developed based on basalt fiber, where the limit of compression strength varies from 65.6 to 78.35 MPa, flexural strength from 6.4 to 9.1 MPa, and water permeability from 3.7 to 1.8%. Among the compositions of micro-reinforced concrete with basalt fiber, the best strength result was recorded in the case of 2% basalt fiber and 10% microsilica, with compression and flexural strengths of 78.35 and 9.1 MPa, respectively. The best water absorption result of 1.8% was obtained only with basalt fiber concrete when the fiber content was increased to 3.2%. As a result, the water absorption was reduced by 62% compared to the initial concrete. The increases in flexural and compression strengths were 42.19% and 13.8%, respectively.
Petrographic characterization of stone and the forms of destruction in the " St. Astvatsatsin" Church of "Tatev" Monastic Complex have been mapped and studied. Mineralogical studies included a microscopic investigation of stone sections, united by external similarity into four groups. Each group’s structural and textural characteristics, as well as its mineralogical composition, were investigated. The generalization of chemical-mineralogical and technological results made it possible to identify the rock materials used in the construction of the "St. Astvatsatsin." church. The work has been carried out using the visual inspection technique developed in the laboratory of the construction company “Horizon-95” LLC and the system for describing and assessing damage to stones by the International Scientific Committee for Stone (ICOMOS). The survey results were used in the "St. Astvatsatsin" church restoration. The work permits quantifying the forthcoming material costs associated with the rock material renewal. Individual stones were identified and marked for renewal or replacement, depending on the degree of damage.