Eli Harma

Mr. Eli Harma

orcid

Research Focus & Metrics

Academic Career Length

4Years (2023-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
Eli HarmaEli Harma
Eli Harma
PSPaul Sanders
Paul Sanders
TWThomas Wood
Thomas Wood
TLTimothy J Langan
Timothy J Langan
There is a demand for a 6005A series extrusion alloy with improved strength that maintains good extrudability. Replacing Mn and Cr dispersoid formers with Sc and Zr is expected to increase the room temperature mechanical properties while not affecting extrudability. Al3X dispersoids with a Sc core surrounded by a Zr shell are stable at higher temperatures and enhance recrystallization resistance and precipitation strengthening. However, there is little information on how the Sc and Zr additions affect the properties of an extrudate as a function of extrusion geometry and ratio. A 6005A series alloy with Cr and Mn additions is compared to an alloy with Sc and Zr additions with rod and flat cross-sections at extrusion ratios of 25 and 92. The results show that Sc and Zr additions increased yield strength and ultimate tensile strength while maintaining ductility compared to Cr and Mn additions. Rod shapes performed significantly better than flat shapes, but there was no significant effect of extrusion ratio.

Verified
Journal Article
Open access
PDF file
Eli HarmaEli Harma
Eli Harma
TLTimothy J Langan
Timothy J Langan
PSPaul Sanders
Paul Sanders
Adding Sc to 6xxx series alloys has led to inconsistent results due to the formation of the high-temperature, thermodynamically stable V-phase (AlSc2Si2). Thermo-Calc single-axis equilibrium and phase diagram calculations were employed to identify V-phase formation with varying Si and Zr concentrations, indicating that increasing Zr and decreasing Si lowered the V-phase equilibrium volume fraction. Increasing Zr also shifted the V-phase equilibrium to higher Si concentrations. To access real-world influences of Zr and Si, four compositions were cast with different Si and Zr concentrations: a high-Si, low-Zr alloy; a medium-Si, medium-Zr alloy; a low-Si, high-Zr alloy; and a baseline alloy without Zr and Sc. The compositions were DC-cast followed by multi-step isochronal and isothermal heat treatments, which revealed that increasing Zr concentration did not influence the formation of V-phase but did result in higher hardness at high temperatures, likely due to Al3Zr precipitation. In contrast, higher Si and lower Zr concentrations produced higher hardness in the peak-aged condition but lower hardness at homogenization temperatures in the 400 °C to 520 °C range. Given these conclusions, a new alloy and a multi-step homogenization process are proposed to further develop Sc- and Zr-containing 6xxx extrusion alloys.


7 September 2023
Verified
Thesis
Open access
PDF file
Eli HarmaEli Harma
Eli Harma
Alloy 6082 aluminum is used for high-volume manufacturing in the automotive industry due to its high strength, impact performance, and corrosion resistance. However, given these improved properties, the alloy has decreased formability compared to other 6xxx series alloys, especially in the extrusion process. Controlling the dynamic recovery and recrystallization properties by changing the additions of Mg and Si can improve the hot deformation properties. Five alloys of varying Mg and Si concentrations between 0.6 to 1.2wt% Mg and 0.7 to 1.3wt% Si were made with constant concentrations of Cr, Fe, and Mn and the same homogenization heat treatment. The proposed alloys are tested using hot compression to identify the activation energy for hot deformation at temperatures of 400℃, 450℃, and 500℃ with strain rates of 0.1s-1, 0.01s-1, and 0.001s-1. The resulting compression samples are analyzed using EBSD to identify the fraction recrystallized. The results show that increasing Mg from 0.6 to 1.2wt% decreases the activation energy from 262 to 220 kJ/mol. In contrast, increases in Si from 0.7 to 1.3wt% decreased the recrystallization fraction and increased activation energy from 262 to 292 kJ/mol. An optimal composition range was identified to be a ratio of Mg to Si between 0.8 and 1, as all alloys close to this ratio had low recrystallized fractions and activation energies compared to other alloys tested for the select temperature and strain rate conditions.

23 February 2026
Verified
Book Chapter
Closed access
PDF file
Eli HarmaEli Harma
Eli Harma
PSPaul Sanders
Paul Sanders