Hossam Hemdan El-Fahhar

Dr. Hossam Hemdan El-Fahhar

Suez University, Suez, As Suways, Egypt
orcid

Research Focus & Metrics

Academic Career Length

5Years (2022-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
10 December 2022 in Materials
Verified
Journal Article
Open access
PDF file
MEMohamed Ibrahim Abd Elaal
Mohamed Ibrahim Abd Elaal
Hossam Hemdan El-FahharHossam Hemdan El-Fahhar
Hossam Hemdan El-Fahhar
Abdelkarim yousif MohamedAbdelkarim yousif Mohamed
Abdelkarim yousif Mohamed
Elshafey Ahmed GadallahElshafey Ahmed Gadallah
Elshafey Ahmed Gadallah
Al-Al2O3 and SiC metal matrix composites (MMCs) samples with different volume fractions up to 20% were produced by high-pressure torsion (HPT) using 10 GPa for 30 revolutions of Al-Al2O3, and SiC and powder metallurgy (PM). The effect of the processing method of micro-size Al MMCs on the density, microstructure evolution, mechanical properties, and tensile fracture mode was thoroughly investigated. HPT processing produces fully dense samples relative to those produced using powder metallurgy (PM). The HPT of the Al MMCs reduces the Al matrix grain size and fragmentation of the reinforcement particles. The Al matrix average grain size decreased to 0.39, 0.23, and 0.2 µm after the HPT processing of Al, Al-20% Al2O3, and SiC samples. Moreover, Al2O3 and SiC particle sizes decreased from 31.7 and 25.5 µm to 0.15 and 0.13 µm with a 99.5% decrease. The production of ultrafine grain (UFG) composite samples effectively improves the microhardness and tensile strength of the Al and Al MMCs by 31–88% and 10–110% over those of the PM-processed samples. The good bonding between the Al matrix and reinforcement particles noted in the HPTed Al MMCs increases the strength relative to the PM samples. The tensile fracture surface morphology results confirm the tensile properties results.
2

1 August 2024 in Science and Technology of Welding and Joining
Verified
Journal Article
Closed access
RFRamy A. Fouad
Ramy A. Fouad
Mohamed. I. A. HabbaMohamed. I. A. Habba
Mohamed. I. A. Habba
YEYousef G.Y. Elshaghoul
Yousef G.Y. Elshaghoul
MSMohamed M. El-Sayed Seleman
Mohamed M. El-Sayed Seleman
Khalid Mohamed HafezKhalid Mohamed Hafez
Khalid Mohamed Hafez
WBWaheed S. Barakat
Waheed S. Barakat
In this study, 4-mm thick AISI 201 austenitic stainless steel butt joints were fabricated using the tungsten inert gas (TIG) process with ER309L, ER316L and ER2209 filler rods. TIG welding was performed using a current of 100 A, voltage of 14 V, with pure argon as the shielding gas at a flow rate of 10 L/min, and filler rod diameters of 2.4 mm. The microstructural and mechanical properties were analysed. ER2209 and ER316L promote an austenitic structure in the fusion zone. ER316L filler produced the finest grain structure (9.39 μm) and the lowest δ-ferrite content (25.85%) in the weld zone. Welds made of ER316L exhibited the highest hardness (314 HV), ultimate tensile strength (857 MPa) and yield strength (448 MPa). ER316L welds also demonstrated superior strain-hardening capacity (0.91) and impact toughness (19.8 GPa). Fracture analysis revealed finer dimples in the ER316L welds, indicating improved ductility and strength compared to other welded joints.

20 April 2022 in Materials
Verified
Journal Article
Open access
PDF file
MEMohamed Ibrahim Abd Elaal
Mohamed Ibrahim Abd Elaal
Hossam Hemdan El-FahharHossam Hemdan El-Fahhar
Hossam Hemdan El-Fahhar
Abdelkarim yousif MohamedAbdelkarim yousif Mohamed
Abdelkarim yousif Mohamed
Elshafey Ahmed GadallahElshafey Ahmed Gadallah
Elshafey Ahmed Gadallah
The influence of the number of passes and the tube materials on the microstructural evolution, mechanical properties, and wear behavior of Cu and brass tubes after parallel tubular channel angular pressing (PTCAP) was investigated. The grain size decreased to final grain sizes of 138.6 nm and 142.7 nm, after PTCAP of the Cu and brass tubes was conducted in up to 4 and 2 passes, respectively. PTCAP contributes to obtaining an ultra-fine grain (UFG) microstructure, with a mixture of different grain sizes that conferred high hardness. The present results indicate the superior wear resistance of Cu and brass PTCAP tubes, relative to Cu and brass samples that were previously deformed by different severe plastic deformation (SPD) processes. The wear mechanism of the Cu tubes changed from delamination and cracks with a high degree of adhesive wear before PTCAP into a combination of adhesive and abrasive wear, with a decrease in the presence of oxygen content after the PTCAP procedure. The wear mechanism also changed from a combination of adhesive and abrasive mechanisms into abrasive ones with the absence of oxygen after the PTCAP of brass tubes.
2

26 December 2022 in Materials
Verified
Journal Article
Open access
PDF file
MEMohamed Ibrahim Abd Elaal
Mohamed Ibrahim Abd Elaal
Hossam Hemdan El-FahharHossam Hemdan El-Fahhar
Hossam Hemdan El-Fahhar
Abdelkarim yousif MohamedAbdelkarim yousif Mohamed
Abdelkarim yousif Mohamed
Elshafey Ahmed GadallahElshafey Ahmed Gadallah
Elshafey Ahmed Gadallah
The motivation for the current study was to improve the wear and frictional properties of Al, Al–Al2O3, and SiC MMCs through HPT processing. The wear test using a tungsten carbide (WC) ball was carried out for different PM and HPT-processed Al and MMC samples. The effect of the sample processing methods on the wear rate, friction, and wear surface morphology was thoroughly investigated. The high hardness after Al grain refinement and reinforcement fragmentation through the HPT processing of the samples increased the wear resistance by 16–81% over that of the PM samples. The average coefficient values and variation ranges were reduced after HPT processing. The Al and Al MMC processing methods affected the wear mechanism and surface morphologies, as proven by the microscopic observations and analyses of the worn surfaces of the samples and WC balls.

11 August 2026 in Proceedings of the Institution of Mechanical Engineers, Part E: Journal of Process Mechanical Engineering
Verified
Journal Article
Closed access
Elshafey Ahmed GadallahElshafey Ahmed Gadallah
Elshafey Ahmed Gadallah
Hossam Hemdan El-FahharHossam Hemdan El-Fahhar
Hossam Hemdan El-Fahhar
MEMohamed Ibrahim Abd Elaal
Mohamed Ibrahim Abd Elaal
Mohamed BassyouniMohamed Bassyouni
Mohamed Bassyouni
SASabry Moussa Abdel Aziz
Sabry Moussa Abdel Aziz
EMElsayed Maroof Metwaly
Elsayed Maroof Metwaly
The lack in previous works concerned with a full study of the deformation homogeneity, and how to reach a high level of deformation homogeneity in the different directions of equal-channel angular pressing (ECAP) processed Cu samples was the motivation of the current study. Therefore, reaching a high level of deformation homogeneity of the copper through optimizing the imposed strain according to the used ECAP die angles was investigated. ECAP was performed using three die angles 90 o , 110 o , and 130° up to 4 passes at room temperature. Microstructural characterization using optical and scanning electron microscopy revealed grain refinement across all die angles, with the 90° die producing the finest and most homogeneous fine-grained structure due to the highest-imposed shear strain. Grain size decreased from 31.3 µm in the annealed condition to 2.7, 4.8, and 7.2 µm after 4 passes using the angles 90°, 110°, and 130° respectively (pressing direction). Similarly, grain size decreased to 3.3, 5.8, and 7.4 µm after 4 passes using the 90, 110, and 130° dies, respectively (transverse direction). At the same time, refinement was comparatively less pronounced at higher die angles. Hardness mapping across ZY, YX, and ZX planes demonstrated significant strengthening and improved deformation homogeneity with increasing passes, with the 90° die consistently achieving the highest hardness values and lowest homogeneity index (H index ). After 4 passes, hardness increased by 144.7, 115.1 and 95.6% (ZY plane), 129.3, 107.8 and 92.7% (YX plane), and 125, 104.3 and 91% (ZX plane) for 90°, 110°, and 130° dies, respectively. The mechanical properties of the 90° die deliver the highest strengthening (up to 403.7% in proof-strength and 70.3% in ultimate tensile strength), but with significant ductility loss. While the 110°and 130° dies show lower strengthening with relatively better ductility. Overall, the 90° angle provides the most effective processing route for producing fine-grained, high-strength Cu samples with excellent deformation homogeneity.

31 October 2025 in JES. Journal of Engineering Sciences
Verified
Journal Article
Closed access
Hossam Hemdan El-FahharHossam Hemdan El-Fahhar
Hossam Hemdan El-Fahhar
EGElshafey Ahmed Gadallah
Elshafey Ahmed Gadallah
AGAdel Ibrahim Gelany
Adel Ibrahim Gelany
ANAhmed E El Nikhaily
Ahmed E El Nikhaily
AMAbdelkarim Yousif Moahmed
Abdelkarim Yousif Moahmed
In this work, AA7075-T6 aluminum alloy 6 mm thick were welded using both metal inert gas (MIG) and tungsten inert gas (TIG) processes with ER5356 filler metal. The welded joints were characterized through optical and scanning electron microscopy (SEM), Vickers microhardness testing, tensile testing, and immersion corrosion testing in aggressive chloride solution. MIG welded joints exhibited superior microstructural integrity with defect-free solidification and formation of a distinct "bleed band structure" at the weld metal (WM)/heat-affected zone (HAZ) interface, indicating optimal metallurgical bonding. In contrast, TIG welded joints showed solidification discontinuities including elongated shrinkage cavities and subgrain structures in the partially melted zone (PMZ). Hardness measurements revealed significant reduction in both processes, with MIG joints showing 25-40% decrease compared to 13-31% for TIG joints in the HAZ. Tensile testing demonstrated that MIG joints retained 58% of base material (BM) ultimate tensile strength (UTS) versus 51% for TIG joints, while TIG joints exhibited higher elongation and strain hardening capacity. Corrosion testing revealed formation of conical-shaped corrosion products on weld zones (WZ), with MIG joints showing increased precipitation sites. MIG welding proves superior for joining 6 mm thick AA7075-T6 plates, offering better microstructural integrity and mechanical performance due to higher heat input and effective cathodic cleaning action. The absence of solidification defects and formation of homogeneous bleed band structure make MIG the preferred process compared to the TIG process for welding of AA7075-T6