Willemite is an inorganic semiconductor material used for optoelectronic applications. The present study purposes a new polymer thermal treatment method involving calcination temperature to fabricate the willemite nanoparticles. The effects of polyvinylpyrrolidone (PVP) on the structural and optical properties of the material were thoroughly investigated. Thermogravimetric and its derivative confirmed the decomposition behavior of PVP. The minimum calcination temperature to decompose PVP was appraised at 740 °C. The FTIR and the Raman analyses confirmed the presence of organic source before the calcination process and the formation of the crystalline structure of the willemite nanoparticles after the heat treatment. The optimum PVP concentration in this study based on the FTIR results was found to be 40 g L−1. This is the minimum concentration at which the willemite nanoparticles remained pure with homogenous distribution. X-ray diffraction analysis of the PVP samples before calcination was confirmed to be amorphous, and upon calcination between 800 and 1000 °C, an α-willemite phase was obtained. The morphology and the average particle size were determined with FESEM and HR-TEM analysis. The average particle size is between 23.8 and 36.7 nm. The optical energy band was found to be increasing from 5.24 to 5.32 eV with the corresponding increase in PVP concentration from 20 to 50 g L−1. The findings in this study provides a new pathway to understand the effects of PVP concentrations on the structural and optical properties of willemite semiconductor nanoparticles as it may have key potential applications for future optoelectronic devices. Graphical abstract The primary task of polyvinylpyrrolidone (PVP) is to serve as a capping agent and to stabilize the metallic salts. The interaction between the PVP and the metallic salts (zinc acetate dihydrate and silicon tetraacetate) is through the strong ionic bonds between the metallic ions and the amide group via oxygen in the PVP chain. The PVP stabilizes the dissolved metallic precursor by amide group steric and electrostatic stabilization. In the drying process at the temperature about 80 °C, the PVP decompose to the shorter polymer chains which they cap the metallic ions. In the step of calcination at the range of 900 °C for 1–4 h, the polymer content and unwanted anions are entirely removed and the nucleation of willemite nanoparticles achieved.
Willemite is a wide band gap semiconductor used in modern day technology for optoelectronics application. In this study, a new simple technique with less energy consumption is proposed. Willemite nanoparticles (NPs) were produced via a water–based solution consisting of a metallic precursor, polyvinylpyrrolidone (PVP), and underwent a calcination process at 900 °C for several holding times between 1–4 h. The FT–IR and Raman spectra indicated the presence of metal oxide bands as well as the effective removal of PVP. The degree of the crystallization and formation of the NPs were determined by XRD. The mean crystallite size of the NPs was between 18.23–27.40 nm. The morphology, particle shape and size distribution were viewed with HR-TEM and FESEM analysis. The willemite NPs aggregate from the smaller to larger particles with an increase in calcination holding time from 1–4 h with the sizes ranging between 19.74–29.71 nm. The energy values obtained from the experimental band gap decreased with increasing the holding time over the range of 5.39 eV at 1 h to at 5.27 at 4 h. These values match well with band gap obtained from the Mott and Davis model for direct transition. The findings in this study are very promising and can justify the use of these novel materials as a potential candidate for green luminescent optoelectronic applications.
24 June 2016 in Journal of Materials Science: Materials in Electronics
The contemporary market needs for enhanced solid–state lighting devices has led to an increased demand for the production of willemite based phosphors using low-cost techniques. In this study, Ce3+ doped willemite nanoparticles were fabricated using polymer thermal treatment method. The special effects of the calcination temperatures and the dopant concentration on the structural and optical properties of the material were thoroughly studied. The XRD analysis of the samples treated at 900 °C revealed the development and or materialization of the willemite phase. The increase in the dopant concentration causes an expansion of the lattice owing to the replacement of larger Ce3+ ions for smaller Zn2+ ions. Based on the FESEM and TEM micrographs, the nanoparticles size increases with the increase in the cerium ions. The mean particles sizes were estimated to be 23.61 nm at 1 mol% to 34.02 nm at 5 mol% of the cerium dopant. The optical band gap energy of the doped samples formed at 900 °C decreased precisely by 0.21 eV (i.e., 5.21 to 5.00 eV). The PL analysis of the doped samples exhibits a strong emission at 400 nm which is ascribed to the transition of an electron from localized Ce2f state to the valence band of O2p. The energy level of the Ce3+ ions affects the willemite crystal lattice, thus causing a decrease in the intensity of the green emission at 530 nm and the blue emission at 485 nm. The wide optical band gap energy of the willemite produced is expected to pave the way for exciting innovations in solid–state lighting applications.