Growing environmental concerns have increased the scientific interest in the utilization of natural fibers for the development of epoxy biocomposite materials. The incorporation of one or more fibers in the production of hybrid epoxy polymer composites has been a subject of discussion. It is interesting to acknowledge that natural/synthetic fiber hybridized epoxy composites have superior properties over natural/natural fiber hybridized epoxy composites. Significant efforts have been devoted to the improvement of natural fiber surface modifications to promote bonding with the epoxy matrix. However, to achieve sufficient surface modification without destroying the natural fibers, optimization of treatment parameters such as the concentration of the treatment solution and treatment time is highly necessary. Synthetic and treated natural fiber hybridization in an epoxy matrix is expected to produce biocomposites with appreciable biodegradability and superior mechanical properties by manipulating the fiber/matrix interfacial bonding. This paper presents a review of studies on the processing of epoxy natural fiber composites, mechanical properties, physical properties such as density and water absorption, thermal properties, biodegradability study, nondestructive examination, morphological characterizations, and applications of epoxy-based natural fiber biocomposites. Other aspects, including a review of variables that enhance the mechanical and functional performance of epoxy/natural fibers composites while also increasing the biodegradability of the composite material for environmental sustainability, were presented. The future research focus was elucidated. It is hoped that this review will stimulate and refocus research efforts toward advancing the manufacture of epoxy/natural fiber composites to meet the growing demand for biocomposite materials in the global world.
In this study, groundnut shell powder (GSP) was used for the reinforcement of recycled polypropylene (recycled PP). The GSP consisting of two-particle sizes viz (0–250 μm and 250–420 μm) was partly treated with sodium hydroxide at room temperature and the GSP both treated and untreated were compressed and compounded with recycled PP to produce GSP-recycled PP composites. For comparison, recycled PP was equally produced as a control sample. The effects of GSP addition and sodium hydroxide treatment on recycled PP were investigated through the mechanical testing of the developed composites. The mechanical properties (tensile strength, hardness, and toughness) of the composites were evaluated and the tensile strength of both treated and untreated GSP-recycled PP composites is higher than the recycled PP and the treated GSP of particle size 0–250 μm having the highest tensile strength at 25 wt% GSP in recycled PP matrix. The hardness of the recycled PP increases with increasing content of GSP while the toughness decreases with increasing concentration of GSP in the recycled PP matrix. The water uptake of the GSP-recycled PP composites was equally studied, and the results revealed that the treated GSP-recycled PP composites has lower rate of water absorption as compared to untreated GSP-recycled PP composites Thermal stability and crystallinity of the composites and monolithic recycled PP were investigated, and it was discovered that the thermal stability and crystallinity of the polymer were enhanced with GSP addition. Morphological characterization of the selected samples through a scanning electron microscope (SEM) and x-ray diffraction (XRD) were equally done to validate the mechanical performance of the composites. Finally, biodegradability study on the composites and the control sample was conducted and it was found out that, the addition of GSP in both forms promotes the biodegradation of the recycled PP polymer. Such biodegradable GSP-recycled PP polymer composite materials are highly valuable for manufacturing food takeaway packages and some of the interior parts of the automobiles.
The quest to enhance public health and the need for a reduction in the environmental solid wastes have prompted this study. Despite abundant studies on silica fume (SF or S) and waste glass powder (WGP or G), there is a need to understand the interaction of WGP with SF in the production of ordinary Portland cement (OPC or C)-based concrete using the water/binder ratio of 0.42. The investigated concrete comprised 90 wt.% of OPC and 10 wt.% of WGP+SF. The samples were denoted as C90GxS10−x such that x varied from 0–10 wt.% at the interval of 2.5. The findings revealed that an increase in the WGP/SF ratio enhanced the absorption of silica/glass blended concrete due to size incompatibility and proliferations of interfacial transition zones between the glass particle, silica fume and cement matrix. The density of fresh OPC concrete was higher than that of glass/silica blended concrete due to the difference in their relative densities. Incorporating WGP and SF in synergy enhanced silicate reorganization and led to a more amorphous binder and a reduction in hydroxyl-based compounds such as portlandite but caused microstructural heterogeneity in the morphology of the binder as obtained from XRD, FTIR and SEM/EDS results. The 28-day compressive strength of 46 MPa is achievable if the WGP and SF are kept within 2.5–5 wt.% and 5–7.5 wt.%, respectively. The study will foster the production of economic, environmental, and cost-efficient concrete.
24 August 2021 in Polymers from Renewable Resources
Natural fibers are becoming the right candidate material as a substitute for glass fibers in the reinforcement of plastic polymers for various applications. The ease of their processing with minimal energy consumption and the quest to produce biodegradable plastics with lightweight has given natural fibers comparative advantages over synthetic fibers. In this study, groundnut shell powder (GSP) in different forms (untreated, sodium hydroxide treated and ash) were characterized using X-ray diffraction (XRD), Fourier transform infrared (FTIR), X-ray fluorescence (XRF), Nuclear magnetic resonance (NMR), Differential scanning calorimetry (DSC) and Scanning electron microscopy (SEM) to evaluate their possible utilization as reinforcement in polymers. GSP was treated with sodium hydroxide for 5 hrs and dried in vacuum for 24 hrs to obtain treated GSP while ash GSP was formed by heating GSP in the furnace at 600 °C for about 3 hrs. The results reveal that sodium hydroxide treatment was very effective in the breaking down of the hydrogen bond with a consequent reduction in the hydrophilicity of the GSP. This would promote GSP bonding with the hydrophobic polymer matrix in the development of natural fiber reinforced plastic polymer composite materials. Ash GSP was found to have the highest crystallinity among the three forms of GSP based on XRD results. Therefore, the result achieved in this work confirmed that treated and ash GSP fibers are good reinforcement material in the production of polymer composites, with the actual choice depending on end-use property requirements of the composite.