The fluid flow and slag entrainment in a slab continuous casting mold were investigated by establishing a full-scale water model. Meanwhile, the heat transfer and solidification process of liquid steel in the mold were studied through numerical simulation. The effect of two different submerged entry nozzles (SENs) was compared and analyzed, named as original SEN and L1 SEN, respectively. The results indicate that the structure of the SEN has a significant influence on the fluid flow pattern and solidification process in the slab mold. For the original SEN, the liquid level in the mold fluctuated obviously and the slag phase was easily entrained into the mold. The percentage of ±3mm level fluctuation was 57.2-74.3%. By enlarging the exit size, the L1 SEN considerably reduced the jet velocity at the nozzle exit and subsequently decreased the surface velocity at the top surface. The level fluctuation and slag entrainment in the mold have been effectively controlled. The percentage of ±3mm level fluctuation was increased to 91.7-98.6%. Furthermore, under the condition of L1 SEN, the thickness of the solidifying shell at the mold outlet was increased from 13.5 mm to 16.4 mm, which was beneficial to decrease the risk of breakouts and quality problems.
Non-metallic inclusions in steel have great influence on the continuity of the steel matrix and the mechanical properties of steel. The precipitation sequence of Ce inclusions in molten steel is predicted by thermodynamic calculations. The results show that Ce content will affect the precipitation sequence of rare earth inclusions in molten steel, and the formation of CeO2, Ce2O3 and CeAlO3 will be inhibited with the increase in Ce content. Our laboratory smelted the test steel without rare earth additive and the test steel with rare earth Ce additive (0.0008%, 0.0013%, 0.0032%, 0.0042%). It was found that the MnS inclusions and inclusions containing Al, Ca, Mg and Si oxides or sulfides in the steel after rare earth addition were modified into complex inclusions containing CeAlO3 and Ce2O2S. The size of inclusion in steel was reduced and the aspect ratio of inclusion was improved. The addition of Ce also improved the grain size of U75V steel and significantly refined the pearlite lamellar spacing. After mechanical property testing of the test steel, it was found that when Ce is increased within 0.0042%, the tensile and impact properties of U75V steel are also improved.
24 January 2025 in Metallurgical and Materials Transactions B
The multiphase flow in the mold has a significant impact on the surface quality of the slab. In this paper, the multiphase flow in the mold is studied by establishing a one-quarter scale water mold, with the aid of a high-speed camera and particle image velocimetry (PIV). The oil phase will make the liquid surface velocity around the nozzle smaller. The greater the viscosity of the oil, the greater the critical water model casting speed and the shallower the critical immersion depth of submerged entry nozzle (SEN). Blowing will enhance the turbulence of the flow field in the mold and have a suppressing effect on the surface velocity. However, the vertical velocity of the narrow surface does not change significantly. The randomness of the bubble entering the mold from the nozzle can easily cause asymmetry of the instantaneous flow. The number of bubbles with a diameter less than 1 mm increase with the increase in gas flow rate. The larger the bubble size, the more buoyant around the nozzle when it escapes. The larger the diameter of bubble, the closer the vortex center of the upper circulation is to the nozzle and the closer the center of the lower circulation is to the narrow surface.
U75V heavy rail steel production uses an aluminum-free deoxidation process; however, large particles of MgO–Al2O3 inclusions form in the steel, which has a great impact on product quality. In this paper, we try to explain how spinel inclusions, which affect the metallurgical quality of heavy rail steel, are produced by thermodynamic and experimental methods, and then determined measures for avoiding such inclusions. The formation mechanism of spinel inclusions in U75V heavy rail steel was determined through the analysis of nozzle clogging in the pouring process and typical inclusions in steel. The results show that there are two types of spinel inclusions in heavy rail steel: one is pure Mg–Al spinel inclusions and the other is Mg–Al spinel inclusions coated with calcium aluminate. The small, pure Mg–Al spinel inclusions were precipitated during the solidification of the molten steel, and the precipitation temperature was related to the composition of the molten steel. The large spinel inclusions were derived from clogging of the submersed nozzle. Mg–Al spinel inclusions coated with calcium aluminate were transformed from CaO–SiO2–Al2O3–MgO complex inclusions in the steel during cooling, and the formation temperature was related to the content of Al2O3 and MgO in the inclusions. The content of Al2O3 and MgO in the inclusions was the key to the formation of the Mg–Al spinel inclusions. Therefore, in order to control the production of spinel inclusions in steel, it is necessary to strictly control the content of impurity elements such as magnesium and aluminum in the alloy auxiliary materials, to reduce the secondary oxidation of liquid steel and to reduce the erosion of refractory materials.