Influence of manufacturing parameters (beam current from 13 to 17 mA, speed function 98 and 85) on microstructure and hydrogen sorption behavior of electron beam melted (EBM) Ti-6Al-4V parts was investigated. Optical and scanning electron microscopies as well as X-ray diffraction were used to investigate the microstructure and phase composition of EBM Ti-6Al-4V parts. The average α lath width decreases with the increase of the speed function at the fixed beam current (17 mA). Finer microstructure was formed at the beam current 17 mA and speed function 98. The hydrogenation of EBM Ti-6Al-4V parts was performed at the temperatures 500 and 650 °С at the constant pressure of 1 atm up to 0.3 wt %. The correlation between the microstructure and hydrogen sorption kinetics by EBM Ti-6Al-4V parts was demonstrated. Lower average hydrogen sorption rate at 500 °C was in the sample with coarser microstructure manufactured at the beam current 17 mA and speed function 85. The difference of hydrogen sorption kinetics between the manufactured samples at 650 °C was insignificant. The shape of the kinetics curves of hydrogen sorption indicates the phase transition αH + βH→βH.
In this work, a laboratory X-ray diffraction complex for in situ investigations of structural phase evolution of materials under gaseous atmosphere and elevated temperatures was developed. The approbation of the complex was carried out using a commercially pure titanium (CP-Ti) powder, zirconium (Zr-1Nb) alloy and electron beam melted Ti-6Al-4V alloy. It was established that hydrogenation of the CP-Ti powder occurred at a temperature of 500 °C and a hydrogen pressure of 0.5 atm, accompanied by the formation of metastable γ titanium hydride (γ-TiH) phase. The lifetime of the γ-TiH phase was 35–40 min. Decomposition of the γ-TiH occurred after reaching a temperature of 650 °C as a result of the thermally stimulated desorption of hydrogen. The α-Zr → δ-ZrH phase transformation was observed under hydrogenation of the zirconium Zr-1Nb alloy at a temperature of 350 °C and a hydrogen pressure of 0.5 atm. It was revealed that the increase in hydrogenation temperature to 450 °C accelerated this transformation by two times. Hydrogenation of the electron beam melted titanium Ti-6Al-4V alloy at a temperature of 650 °C and hydrogen pressure of 0.5 atm was accompanied by the α → α + β → β + α2 phase transformations.
1 March 2019 in International Journal of Hydrogen Energy
This paper describes the influence of silicon carbide (SiC) coating on hydrogen sorption kinetics of zirconium alloy E110 (Zr-1Nb). Amorphous SiC coating of 1.5-μm thickness was deposited on Zr-1Nb alloy substrate by direct current magnetron sputtering of composite cathode. Hydrogen absorption by SiC-coated Zr-1Nb alloy significantly decreased due to low hydrogen permeability of the coating. Hydrogenation tests show that SiC coating provides protective properties against hydrogen permeation in the investigated temperature range of 350–450 °C. It was shown that hydrogenation of uncoated Zr-1Nb leads to formation of δ hydrides at 350 °C and δ and γ hydrides at higher temperatures whereas in the SiC-coated Zr-1Nb alloy only δ hydrides formed. Gradient hydrogen distribution through the SiC coating and H trapping in the carbon-rich interface was observed. The adhesion strength of the coating was ~5 N. Hydrogenation up to 450 °C for 5 h does not degrade the adhesion properties during scratch testing.
1 April 2019 in International Journal of Hydrogen Energy