To evaluate evolution of physical and mechanical properties due to drying and heat modification, a load of radiata pine wood was selected and properties were measured after each drying process. The results revealed interesting correlations between intrinsic factors and properties; the values of density were highly dispersed after drying or thermal treatment and uncorrelated with other parameters, but the minimum density values were kept constant after heat treatment. Moreover, weight loss (WL) and moisture content (MC) were decreasing proportionally to the treatment intensity, due to wood–water interactions, cell wall changes, and thermal degradation of wood fractions. WL and MC were reasonably correlated with the dimensional stability, improving the dimensional stability after drying treatments, but keeping the same order of anisotropy. Regarding the wood stiffness (modulus of elasticity, MOE), it was unaffected by the drying temperature, and the correlations between MOE and MC or WL appear to be acceptable, and the values of MC or WL did not adversely affect the MOE. However, the modulus of rupture was dropped during the drying process, obtaining three differentiated groups with a decrease in around 59% after thermal modification.
This study deals with the effect of heat treatment on Pinus oocarpa specimens from forest plantations in Colombia. The effects of two heat treatments at 170 and 190 °C for 2.5 h in saturated vapor were evaluated based on the color, dimensional stability, air-dry and basic densities, modulus of elasticity (MOE), and modulus of rupture (MOR) in static bending of samples. The evaluations were carried out following the Colombian Technical Standards NTC 290 and 663, and the color changes resulting from heat treatments were monitored using the CIE-Lab, as well as other standards from the literature. The results show that there was 2.4% and 3.3% mass loss of wood modified at 170 and 190 °C, respectively. The air-dry and basic densities were higher in 170 °C treatment than after 190 °C treatment, and the thermal modifications applied increased the dimensional stability of the treated wood. After treatment at 170 and 190 °C, the lightness to darkness (L*) was reduced by 10% and 22%; the a* coordinate increased by 11% and 26%, causing redness in the treated wood; the b* coordinate increased by 14% and 17%; and the values of the wood color saturation (c*) increased by 14% and 18%, respectively. The general color change (ΔE*) increased gradually with the increase in the treatment temperature, resulting in a high color change to a very different color. The bending strength of thermally modified wood was improved and significantly increased to values higher than those of unmodified Pinus oocarpa wood. The high air-dry and basic densities, improved dimensional stability and resistance to bending, and attractive appearance of the treated wood indicate that thermal modification is a promising alternative for the transformation of Pinus oocarpa wood into a raw material with a high added value.
Collapse is almost certain to occur in the industrial drying of Eucalyptus nitens and, as such this prevents the lumber manufacturing industry in Chile from producing commercial solid wood products from this species. This problem is still unsolved, and different studies to reduce collapse are currently underway. In this exploratory study, shrinkage and collapse after drying of Eucalyptus nitens was measured for boards cut from different radial locations within the stem (core, transition, and outer wood from pith to bark) and having different annual ring orientations (flat-sawn and quarter-sawn). Though exploratory, the results appear to confirm that pieces that were cut from the center of the trees were less susceptible to collapse than pieces cut from the transition zone between the center and the periphery. On average, collapse in transition wood was approximately 50% higher than the collapse observed in wood cut from the central zone of the trees.
This article reports the results of an exploratory study designed to reduce heat and electricity consumption in industrial drying of radiata pine. The experiments were performed with slight modifications of the standard drying schedules used by the sawmill to dry radiata pine in 100-m3 industrial kilns. The heat and electricity consumption were determined with data collected during the drying runs and calculations based on mathematical models. The results showed that depending on the case, heat and power consumption were respectively reduced by up to 14 and 35%.
24 May 2019 in European Journal of Wood and Wood Products
Wood drying is an important process for adding value and manufacturing innovative products. Eucalyptus nitens wood is inherently difficult to dry because of its natural propensity for checking as well as collapse and shrinkage. Lumber recovery after industrial drying of eucalypts is also very low. This study measured the wood quality of E. nitens juvenile wood (13 mm thickness) after radio-frequency vacuum (RFV) drying and wood dried in a conventional kiln dryer (KD). Drying cycles were performed using a radio frequency vacuum dryer with a 3 m3 of capacity and convective kiln-dryer equipment with a 3.5 m3 of capacity. The results showed that the drying time using the radio frequency vacuum method was reduced by 47% when compared to conventional kiln drying. The shrinkage was significantly lower in the RFV than in the conventional KD. The volumetric collapse decreased by approximately 60% in the RFV drying. RFV drying of E. nitens juvenile wood improves the wood quality for solid wood products because the intensity of surface checking and collapse are reduced.