The stability of graphene oxide (GO) in water is extremely relevant because of its application as an adsorbent material, as well as for its fate and behavior in the environment. Zeta potential was used to study the effect of secondary salts (carbonate, sulfate, and phosphate), temperature (20 to 60 °C), and pH (5 to 9) on the stability of six different GOs produced from natural, synthetic, and amorphous graphite—with and without the use of attrition milling. Generally, GOs produced with attrition-milled graphites had lower ζ-potentials than their unmilled counterparts because of their smaller particle sizes and higher concentration of oxygen-containing functional groups. It was observed that GO produced from graphite and synthetic graphite had ζ-potential values lower than −30 mV, even at 30 °C. However, it was observed that all the GOs studied were unstable in the presence of carbonate and sulfate salts at concentrations between 170 and 1695 mg L−1, as they reached a ζ-potential of −4.1 mV. Density-functional theory electronic structure calculations suggested that the instability of GO in the presence of carbonate and sulfate was caused by the abstraction of a proton resulting in interaction energies Eint of 28.3 and 168.9 kJ mol−1, respectively. Our results suggest that temperatures above 30 °C, as well as carbonate and sulfate salts at concentrations relevant to arid and semi-arid regions, could promote the formation of agglomerates of GO, thus limiting its use and mobility in water.
Metal oxide nanoparticles (NPs) are known to have biological activity against various microorganisms; thus, they have been widely used as microbicidal agents, and their use poses potential solutions to problems such as biofouling. This study focuses on the surface modification of TiO2 and ZrO2 nanoparticles with lactic acid (LA) and stearic acid (SA) to enhance their antibacterial activity (AA). The surface modification of TiO2 and ZrO2 nanoparticles was performed using continuous frequency ultrasound. Sonication was performed at different reaction times. Characterization of the modified nanoparticles by TGA, DSC, XRD, FTIR, and XPS techniques demonstrated the presence of the organic ligand on the surface of the nanoparticles. The surface modification results in a reduction in the crystal size of the nanoparticles. Regarding the antibacterial properties of modified TiO2 and ZrO2 nanoparticles, their minimum bactericidal concentration (MBC) against Gram-negative and Gram-positive bacteria of the bacterial strains Escherichia coli and Staphylococcus aureus was evaluated. The results obtained from the AA of the modified and unmodified nanoparticles demonstrated greater efficacy of the modified nanoparticles, in the particular case of TiO2 and TiO2-LA, evaluated at concentrations of 200, 500, 800, 1100, and 1400 ppm, TiO2-LA nanoparticles showed better results at most of the concentrations studied and a bacterial inhibition percentage of 99.0% was achieved at a concentration of 500 ppm against the Escherichia coli bacteria, while TiO2 NPs only reached 55.0%, this shows that ligands with more than one functional group play an important role in improving AA.