For the first time, next to the flammability tests (LOI, UL-94 HB, VBB, TGA), experimental tests and computer simulation have been conducted on the flame spread and combustion of glass fiber-reinforced epoxy resins (GFRER) with 6% graphene and 6% DDM-DOPO flame-retardant additives. The downward rates of flame spread (ROS) in opposed flow with oxidizer and the upward ROS along GFRER composites have been first measured as well as the distribution of temperature over the combustion surface of the composites with flame-retardant additives and without them. The LOI and UL-94 HB tests showed a reduction in the flammability of GFRER when flame retardants were added and predicted a higher effectiveness of DDM-DOPO compared to graphene. Adding DDM-DOPO resulted in increasing the rate of formation of the volatile pyrolysis products and their yield, indicating, together with the other data obtained, the gas phase mechanism of the flame retardant’s action. Adding graphene resulted in an increase in the soot release on the burning surface and an increase in the amount of non-volatile pyrolysis products on the burning surface, reducing the amount of fuel that participated in the oxidation reactions in the gas phase. The developed numerical combustion model for GFRER with a DDM-DOPO additive, based on the action of DDM-DOPO as a flame retardant acting in the gas phase, satisfactorily predicts the effect of this flame retardant on the reduction in downward ROS over GFRER for 45–50% oxygen concentrations. The developed model for GFRER with graphene additive, based on a reduction in the amount of fuel and increase in the amount of incombustible volatile pyrolysis products when graphene is added, predicts with good accuracy downward ROS over GFRER depending on oxygen concentration.
In the present review, using an integrated approach based on the experimental and theoretical study of the processes of thermal decomposition and combustion of practically important polymers, such as polymethyl methacrylate, polyethylene, and glass-fiber-reinforced epoxy resin, the features of the mechanism for reducing the combustibility of these materials with phosphorus-containing flame-retardants (FR), as well as graphene, are identified. A set of original experimental methods was developed and applied that make it possible to study the kinetics of thermal decomposition and the thermal and chemical structure of the flames of the studied materials, including those with FR additives, as well as to measure the flame propagation velocity, the mass burning rate, and the heat fluxes from the flame on the surface of a material. Numerical models were developed and tested to describe the key parameters of the flames of the studied polymeric materials. An analysis of the experimental and numerical simulation data presented showed that the main effect of phosphorus-containing fire-retardants on reducing the combustibility of these materials is associated with the inhibition of combustion processes in the gas phase, and the effect of adding graphene manifests itself in both gas and condensed phases.
The flammability of various materials used in industry is an important issue in the modern world. This work is devoted to the study of the effect of flame retardants, graphene and DDM-DOPO (9,10-dihydro-9-oxa-10-phosphaphenanthrene-10-oxide-4,4′-diamino-diphenyl methane), on the flammability of glass-fiber-reinforced epoxy resin (GFRER). Samples were made without additives and with additives of fire retardants: graphene and DDM-DOPO in various proportions. To study the flammability of the samples, standard flammability tests were carried out, such as thermogravimetric analysis, the limiting oxygen index (LOI) test, and cone calorimetry. In addition, in order to test the effectiveness of fire retardants under real fire conditions, for the first time, the thermal structure of downward flame propagation over GFRER composites was measured using thin thermocouples. For the first time, the measured thermal structure of the flame was compared with the results of numerical simulations of flame propagation over GFRER.
This paper presents a study of the flammability and thermal decomposition products of glass fiber-reinforced epoxy resin (GFRER) with the addition of cardanol-based phosphorus-containing benzoxazine monomer (CBz) and graphene and their combinations in different proportions (up to 20 wt.%). The addition of CBz alone or in combination with graphene resulted in an increase in the limiting oxygen index (LOI) and self-extinguishing in the UL-94 HB test. The flame-retardant samples had better tensile mechanical properties than the sample without additives. The differential mass-spectrometric thermal analysis (DMSTA) of the thermal decomposition products of GFRER without additives and with the addition of CBz and graphene was carried out. CBz addition promoted the thermal decomposition of high-molecular-weight products of epoxy resin decomposition in the condensed phase and at the same time decreased the time of release of low-molecular-weight thermal decomposition products into the gas phase. Graphene addition resulted in an increase in the relative intensities of high-molecular-mass peaks compared to GFRER without additives.