This study investigates the use of finely ground coal bottom ash (FGCBA) as a substitute for Portland cement in concrete, comparing it with coal fly ash from the same power plant. The incorporation of this ash necessitates the addition of a superplasticizer to achieve the desired slump at the same replacement rate. The results demonstrate that at an optimal 20% replacement rate, as determined by 91-day compressive strength tests, the maximum strength achieved by FGCBA is 97.7% of the control group with pure cement, whereas coal fly ash reaches 114.0%. Drying shrinkage tests indicate for both materials have similar volume stability, while rapid chloride permeability tests show their effectiveness in reducing chloride ion permeability, with superior performance from FGCBA. Under optimal conditions, the result of the RCPT test was only 559 coulombs, which is significantly better compared to the 4108 coulombs when using fly ash from coal combustion. Our results demonstrate that utilizing low-cost bottom ash by finely grinding it to replace Portland cement in concrete is feasible, achieving both carbon reduction and economic viability.
The compressive strengths of fly ash-based alkali-activated materials (AAM), produced using various activators of only sodium hydroxide, were measured. Fly ash-based AAM specimens, produced by mixing different kinds of fly ash and ground granulated blast-furnace slag (GGBFs) with an activator containing only sodium hydroxide, were cured at ambient temperature, and then placed in air for different numbers of days. The short- and long-term compressive strengths and shrinkage of fly ash-based AAM were measured and compared to one another. The effects of type of fly ash, alkali-equivalent content, GGBFs replace percentage, and ages on the compressive strengths and shrinkage of fly ash-based AAM were investigated. Even when different fly ash was used as the raw material for AAM, a similar compressive strength can be achieved by alkali-equivalent content, GGBFs replaces percentage. However, the performance of shrinkage due to different types of fly ash differed significantly.
Inorganic polymeric materials react slowly at room temperature and therefore, usually require high-temperature curing. This study determined the correlation between temperature and duration in high-temperature curing. The results revealed optimal values for each alkali equivalent of an activator (weight ratio of Na2O/glass powder), curing temperature, and curing duration. Increasing the curing duration and curing temperature had positive effects when the alkali equivalent was lower than the optimal percentage. However, over-curing resulted in the visible cracking of the specimens. Furthermore, despite being initially high, the compressive strength of specimens gradually diminished after standing in air. To ensure the durability of glass-based geopolymers, the curing temperature and duration should not exceed 70 °C, and 1 day, respectively.
This study used experimental and numerical simulation methods to discuss the attenuation mechanism of a blast inside a tunnel for different forms of a tunnel pressure reduction module under the condition of a tunnel near-field explosion. In terms of the experiment, a small-scale model was used for the explosion experiments of a tunnel pressure reduction module (expansion chamber, one-pressure relief orifice plate, double-pressure relief orifice plate). In the numerical simulation, the pressure transfer effect was evaluated using the ALE fluid–solid coupling and mapping technique. The findings showed that the pressure attenuation model changed the tunnel section to diffuse, reduce, or detour the pressure transfer, indicating the blast attenuation effect. In terms of the effect of blast attenuation, the double-pressure relief orifice plate was better than the one-pressure relief orifice plate, and the single-pressure relief orifice plate was better than the expansion chamber. The expansion chamber attenuated the blast by 30%, the one-pressure relief orifice plate attenuated the blast by 51%, and the double-pressure relief orifice plate attenuated the blast by 82%. The blast attenuation trend of the numerical simulation result generally matched that of the experimental result. The results of this study can provide a reference for future protective designs and reinforce the U.S. Force regulations.