1 August 2020 in Applied Surface Science
Verified
Journal Article
Closed access
TKTatyana Kuznetsova
Tatyana Kuznetsova
VLVasilina Lapitskaya
Vasilina Lapitskaya
Anastasiya KhabaravaAnastasiya Khabarava
Anastasiya Khabarava
SCSergei Chizhik
Sergei Chizhik
BWBogdan Warcholinski
Bogdan Warcholinski
AGAdam Gilewicz
Adam Gilewicz

1 June 2017 in Surface and Coatings Technology
Verified
Journal Article
Closed access
BWBogdan Warcholinski
Bogdan Warcholinski
AGAdam Gilewicz
Adam Gilewicz
TKTatyana Kuznetsova
Tatyana Kuznetsova
Tatsiana ZubarTatsiana Zubar
Tatsiana Zubar
SCS.A. Chizhik
S.A. Chizhik
VLVasilina Lapitskaya
Vasilina Lapitskaya

3 July 2018 in Journal of Materials Engineering and Performance
Verified
Journal Article
Open access
PDF file
BWBogdan Warcholinski
Bogdan Warcholinski
TKTatyana Kuznetsova
Tatyana Kuznetsova
AGAdam Gilewicz
Adam Gilewicz
Tatsiana ZubarTatsiana Zubar
Tatsiana Zubar
VLVasilina Lapitskaya
Vasilina Lapitskaya
VGV. S. Goltvyanytsya
V. S. Goltvyanytsya
ZrN and Zr-Si-N coatings were formed using vacuum-arc plasma fluxes deposition system at the substrate bias voltage (UB) ranged from − 50 to − 220 V on HS6-5-2 steel substrates. The structural, mechanical and tribological properties were characterized using x-ray diffraction, atomic force microscopy, scanning electron microscopy, optical microscopy, nanoindentation and ball-on-disk test. The surface roughness parameter Ra of ZrN coatings is lower than Zr-Si-N coatings. Both roughness Ra of Zr-Si-N coatings and the number of surface defects with mainly small dimensions to 1 µm decrease with increasing negative substrate bias voltage. The addition of silicon to ZrN significantly reduces the crystallite size, from about 18.3 nm for ZrN coating to 6.4 nm for Zr-Si-N coating both deposited at the same UB = − 100 V and 7.8 nm for UB = − 150 V. The hardness of Zr-Si-N coatings increases to about 30 GPa with the increase in negative substrate bias voltage (UB = − 220 V). Adhesion of the coatings tested is high, and critical load is above 80 N and reduces with UB increase. Coefficient of friction determined using AFM shows similar trend as surface roughness in microscale.

13 April 2020 in Inorganic Chemistry
Verified
Journal Article
Closed access
AKAlexander Khort
Alexander Khort
Valentin RomanovskiValentin Romanovski
Valentin Romanovski
VLVasilina Lapitskaya
Vasilina Lapitskaya
TKTatyana Kuznetsova
Tatyana Kuznetsova
KYKhabib Yusupov
Khabib Yusupov
KPKirill Podbolotov
Kirill Podbolotov

15 September 2021 in Nanomaterials
Verified
Journal Article
Open access
PDF file
GMGalina Melnikova
Galina Melnikova
TKTatyana Kuznetsova
Tatyana Kuznetsova
VLVasilina Lapitskaya
Vasilina Lapitskaya
APAgata Petrovskaya
Agata Petrovskaya
SCSergei Chizhik
Sergei Chizhik
SYStanislav Yakovin
Stanislav Yakovin
The present paper addresses the problem of identification of microstructural, nanomechanical, and tribological properties of thin films of tantalum (Ta) and its compounds deposited on stainless steel substrates by direct current magnetron sputtering. The compositions of the obtained nanostructured films were determined by energy dispersive spectroscopy. Surface morphology was investigated using atomic force microscopy (AFM). The coatings were found to be homogeneous and have low roughness values (<10 nm). The values of microhardness and elastic modulus were obtained by means of nanoindentation. Elastic modulus values for all the coatings remained unchanged with different atomic percentage of tantalum in the films. The values of microhardness of the tantalum films were increased after incorporation of the oxygen and nitrogen atoms into the crystal lattice of the coatings. The coefficient of friction, CoF, was determined by the AFM method in the “sliding” and “plowing” modes. Deposition of the coatings on the substrates led to a decrease of CoF for the coating-substrate system compared to the substrates; thus, the final product utilizing such a coating will presumably have a longer service life. The tantalum nitride films were characterized by the smallest values of CoF and specific volumetric wear.

18 March 2021 in Materials
Verified
Journal Article
Open access
PDF file
AKAleksander Kuprin
Aleksander Kuprin
AGAdam Gilewicz
Adam Gilewicz
TKTatyana Kuznetsova
Tatyana Kuznetsova
VLVasilina Lapitskaya
Vasilina Lapitskaya
GTGalina N. Tolmachova
Galina N. Tolmachova
ESEvgeniy Sadyrin
Evgeniy Sadyrin
The transition metal oxynitrides are a coating material with decorative features due to their adjustable color and good mechanical properties. The purpose of the research was to study the effect of the relative oxygen concentration O2(x) = O2/(N2 + O2) in particular on adhesion, but also on the color, structural and mechanical properties of ZrON coatings synthesized by cathodic arc evaporation on HS6-5-2 steel substrates. The surface morphology, phase and chemical composition and mechanical properties were determined using scanning electron microscopy, X-ray diffraction, wavelength dispersive X-ray spectroscopy, nanoindentation and scratch test. It was found that color of the coatings changed from light yellow for ZrN first to gold and then to graphite for Zr-O phase with increase of oxygen concentration. X-ray diffraction patterns showed that the phase separation of ZrN and ZrO2 occurred for about 35 at.% of oxygen in the coating. Increase in oxygen concentration in the coatings led to decrease in crystallite size from about 20 nm for ZrN to about 5 nm for coatings with about 35 at.% of oxygen and about 25 at.% of nitrogen. An increase in hardness from about 26 GPa for ZrN to about 30 GPa for coating with small concentration of oxygen (about 9 at.%) and then decrease to about 15 GPa was observed. Adhesion of Zr-O-N coatings demonstrated strong dependence on oxygen concentration. Critical load for ZrN is about 80 N and decreases with oxygen concentration increase to about 30 N for ZrO2.