1 January 2017 in Physics of Metals and Metallography
The effect of the composition and cooling rate of the melt on the microhardness, phase composition, and fine-structure parameters of as-cast and splat-quenched (SQ) high-entropy (HE) Al–Cu–Fe–Ni–Si alloys was studied. The quenching was performed by conventional splat-cooling technique. The cooling rate was estimated to be ~106 K/s. Components of the studied HE alloys were selected taking into account both criteria for designing and estimating their phase composition, which are available in the literature and based on the calculations of the entropy and enthalpy of mixing, and the difference between atomic radii of components as well. According to X-ray diffraction data, the majority of studied Al–Cu–Fe–Ni–Si compositions are two-phase HE alloys, the structure of which consists of disordered solid solutions with bcc and fcc structures. At the same time, the Al0.5CuFeNi alloy is single-phase in terms of X-ray diffraction and has an fcc structure. The studied alloys in the as-cast state have a dendritic structure, whereas, after splat quenching, the uniform small-grained structure is formed. It was found that, as the volume fraction of bcc solid solution in the studied HE alloys increases, the microhardness increases; the as-cast HE Al–Cu–Fe–Ni–Si alloys are characterized by higher microhardness compared to that of splat-quenched alloys. This is likely due to the more equilibrium multiphase state of as-cast alloys.
25 July 2014 in Physics of Metals and Metallography
Structure and mechanical properties of multicomponent high-entropy CoCrCuFeNiSn x alloys ( x = 0.5; 1.0) have been studied for the first time in the as-cast and splat-quenched (at a rate of ∼106K/s)...
9 May 2022 in Molecular Crystals and Liquid Crystals
In this study, Co19Cr18Fe22Mn21Ni20 HEA thin films have been obtained by the modernized method of three-electrode ion-plasma sputtering of mosaic targets consisting of pure metals. The structure, electrical resistance and magnetic properties of films were investigated. Single diffuse halo is observed on the XRD patterns of the as-deposited films, which confirms their amorphous structure. Some of the thin films, which were annealed at 900 K in a vacuum were identified to be oxidized by the small amount of oxygen in the work chamber. After the heat treatment, the Co19Cr18Fe22Mn21Ni20 films are transformed from an amorphous state into a crystallized FCC solid solution with the lattice parameter a = 0.3613 nm. Also, the cubic B2 phase of FeCo with a lattice parameter of 0.2857 nm is formed in the annealed films. As a result of oxidation processes, a dispersed phase of manganese oxide is also arising after annealing. Calculation of the activation energy of the beginning of phase transition was carried out by the generalized Kissinger method. The temperature dependencies of electrical resistivity of films were measured by the four-point technique upon continuously heating in the high vacuum. Both as-deposited and annealed films clearly reveal a typical ferromagnetic behavior. The as-deposited HEA film exhibits the soft magnetic properties while the annealed films can be attributed to hard magnetic materials.
1 September 2006 in Physics of Metals and Metallography
A modified ion-plasma sputtering technique was used to produce metastable states, in particular, amorphous (from the standpoint of X-ray diffraction) and nanocrystaline phases in nickel-carbon film al
28 September 2021 in East European Journal of Physics
The article investigates the structure and physical properties of the multicomponent high-entropy alloy CoCr0.8Cu0.64FeNi in the cast and quenched state. The composition of the alloy under study is analyzed using the criteria available in the literature for predicting the phase composition of high-entropy alloys. These parameters are based on calculations of the entropy and enthalpy of mixing and also include the concentration of valence electrons, the thermodynamic parameter Ω, which takes into account the melting point, entropy of mixing, and enthalpy of mixing. Another important parameter is the difference in atomic radii between the alloy components δ. Cast samples of the CoCr0.8Cu0.64FeNi alloy of nominal composition were prepared on a Tamman high-temperature electric furnace in an argon flow using a copper mold. The weight loss during the manufacture of ingots did not exceed 1%, and the average cooling rate was ~ 102K/s. Thereafter, the cast ingot was remelted, and films were obtained from the melt. The splat quenching technique used in this work consisted of the rapid cooling of melt droplets when they collide with the inner surface of a rapidly rotating (~ 8000 rpm) hollow copper cylinder. The cooling rate, estimated from the film thickness, was ~ 106 K / s. X-ray structural analysis was performed on a DRON-2.0 diffractometer with monochromatic Cu Kα radiation. Diffraction patterns were processed using the QualX2 program. The magnetic properties of the samples were measured using a vibrating sample magnetometer at room temperature. The microhardness was measured on a PMT-3 device at a load of 50 g. In accordance with theoretical predictions confirmed by the results of X-ray diffraction studies, the structure of the alloy, both in the cast and in the quenched state, is a simple solid solution of the FCC type. The lattice parameters in the cast and liquid-quenched states are 0.3593 nm and 0.3589 nm, respectively. Measurements of the magnetic properties showed that the CoCr0.8Cu0.64FeNi alloy can be classified as soft magnetic materials. In this case, quenching from a liquid state increases the coercivity. On quenched samples, increased microhardness values were also obtained. This can be explained by internal stresses arising during hardening.
3 February 2016 in Physica Status Solidi (a)