Converting omnipresent environmental energy through the assistance of spontaneous water evaporation is an emerging technology for sustainable energy systems. Developing bio‐based hydrovoltaic materials further pushes the sustainability, where wood is a prospect due to its native hydrophilic and anisotropic structure. However, current wood‐based water evaporation‐assisted power generators are facing the challenge of low power density. Here, an efficient hydrovoltaic wood power generator is reported based on wood cell wall nanoengineering. A highly porous wood with cellulosic network filling the lumen is fabricated through a green, one‐step treatment using sodium hydroxide to maximize the wood surface area, introduce chemical functionality, and enhance the cell wall permeability of water. An open‐circuit potential of ≈140 mV in deionized water is realized, over ten times higher than native wood. Further tuning the pH difference between wood and water, due to an ion concentration gradient, a potential up to 1 V and a remarkable power output of 1.35 µW cm−2 is achieved. The findings in this study provide a new strategy for efficient wood power generators.
Polymer shape-memory aerogels (PSMAs) are prospects in various fields of application ranging from aerospace to biomedicine, as advanced thermal insulators, actuators, or sensors. However, the fabrication of PSMAs with good mechanical performance is challenging and is currently dominated by fossil-based polymers. In this work, strong, shape-memory bio-aerogels with high specific surface areas (up to 220 m2/g) and low radial thermal conductivity (0.042 W/mK) were prepared through a one-step treatment of native wood using an ionic liquid mixture of [MTBD]+[MMP]-/DMSO. The aerogel showed similar chemical composition similar to native wood. Nanoscale spatial rearrangement of wood biopolymers in the cell wall and lumen was achieved, resulting in flexible hydrogels, offering design freedom for subsequent aerogels with intricate geometries. Shape-memory function under stimuli of water was reported. The chemical composition and distribution, morphology, and mechanical performance of the aerogel were carefully studied using confocal Raman spectroscopy, AFM, SAXS/WAXS, NMR, digital image correlation, etc. With its simplicity, sustainability, and the broad range of applicability, the methodology developed for nanoscale reassembly of wood is an advancement for the design of biobased shape-memory aerogels.
Eco-friendly materials with superior thermal insulation and mechanical properties are desirable for improved energy- and space-efficiency in buildings. Cellulose aerogels with structural anisotropy could fulfill these requirements, but complex processing and high energy demand are challenges for scaling up. Here we propose a scalable, nonadditive, top-down fabrication of strong anisotropic aerogels directly from wood with excellent, near isotropic thermal insulation functions. The aerogel was obtained through cell wall dissolution and controlled precipitation in lumen, using an ionic liquid (IL) mixture comprising DMSO and a guanidinium phosphorus-based IL [MTBD][MMP]. The wood aerogel shows a unique structure with lumen filled with nanofibrils network. In situ formation of a cellulosic nanofibril network in the lumen results in specific surface areas up to 280 m2/g and high yield strengths >1.2 MPa. The highly mesoporous structure (average pore diameter ∼20 nm) of freeze-dried wood aerogels leads to low thermal conductivities in both the radial (0.037 W/mK) and axial (0.057 W/mK) directions, showing great potential as scalable thermal insulators. This synthesis route is energy efficient with high nanostructural controllability. The unique nanostructure and rare combination of strength and thermal properties set the material apart from comparable bottom-up aerogels. This nonadditive synthesis approach is believed to contribute significantly toward large-scale design and structure control of biobased aerogels.
Functional wood materials often rely on active additives due to the weak piezoelectric response of wood itself. Here, we chemically modify wood to form functionalized, eco-friendly wood veneer for self-powered vibration sensors. Only the piezoelectricity of the cellulose microfibrils is used, where the drastic improvement comes only from molecular and nanoscale wood structure tuning. Sequential wood modifications (delignification, oxidation, and model fluorination) are performed, and effects on vibration sensing abilities are investigated. Wood veneer piezoelectricity is characterized by the piezoresponse force microscopy mode in atomic force microscopy. Delignification, oxidation, and model fluorination of wood-based sensors provide output voltages of 11.4, 23.2, and 60 mV by facilitating cellulose microfibril deformation. The vibration sensing ability correlates with improved piezoelectricity and increased cellulose deformation, most likely by large, local cell wall bending. This shows that nanostructural wood materials design can tailor the functional properties of wood devices with potential in sustainable nanotechnology.
13 July 2023 in ACS Sustainable Chemistry & Engineering
Hydrovoltaic energy harvesting offers the potential to utilize enormous water energy for sustainable energy systems. Here, we report the utilization and tailoring of an intrinsic anisotropic 3D continuous microchannel structure from native wood for efficient hydrovoltaic energy harvesting by Fe3O4 nanoparticle insertion. Acetone-assisted precursor infiltration ensures the homogenous distribution of Fe ions for gradience-free Fe3O4 nanoparticle formation in wood. The Fe3O4/wood nanocomposites result in an open-circuit voltage of 63 mV and a power density of ∼52 μW/m2 (∼165 times higher than the original wood) under ambient conditions. The output voltage and power density are further increased to 1 V and ∼743 μW/m2 under 3 suns solar irradiation. The enhancement could be attributed to the increase of surface charge, nanoporosity, and photothermal effect from Fe3O4. The device exhibits a stable voltage of ∼1 V for 30 h (3 cycles of 10 h) showing good long-term stability. The methodology offers the potential for hierarchical organic-inorganic nanocomposite design for scalable and efficient ambient energy harvesting.
The transition to sustainable materials and eco‐efficient processes in commercial electronics is a driving force in developing green electronics. Iron‐catalyzed laser‐induced graphitization (IC‐LIG) has been demonstrated as a promising approach for rendering biomaterials electrically conductive. To optimize the IC‐LIG process and fully exploit its potential for future green electronics, it is crucial to gain deeper insights into its catalyzation mechanism and structural evolution. However, this is challenging due to the rapid nature of the laser‐induced graphitization process. Therefore, multiscale preparation techniques, including ultramicrotomy of the cross‐sectional transition zone from precursor to fully graphitized IC‐LIG electrode, are employed to virtually freeze the IC‐LIG process in time. Complementary characterization is performed to generate a 3D model that integrates nanoscale findings within a mesoscopic framework. This enabled tracing the growth and migration behavior of catalytic iron nanoparticles and their role during the catalytic laser‐graphitization process. A three‐layered arrangement of the IC‐LIG electrode is identified including a highly graphitized top layer with an interplanar spacing of 0.343 nm. The middle layer contained γ‐iron nanoparticles encapsulated in graphitic shells. A comparison with catalyst‐free laser graphitization approaches highlights the unique opportunities that IC‐LIG offers and discuss potential applications in energy storage devices, catalysts, sensors, and beyond.