Polypyrrole one-dimensional nanostructures (nanotubes, nanobelts and nanofibers) were prepared using three various dyes (Methyl Orange, Methylene Blue and Eriochrome Black T). Their high electrical conductivity (from 17.1 to 60.9 S cm−1), good thermal stability (in the range from 25 to 150 °C) and resistivity against ageing (half-time of electrical conductivity around 80 days and better) were used in preparation of lightweight and flexible composites with silicone for electromagnetic interference shielding in the C-band region (5.85–8.2 GHz). The nanostructures’ morphology and chemical structure were characterized by scanning electron microscopy, Brunauer–Emmett–Teller specific surface measurement and attenuated total reflection Fourier-transform infrared spectroscopy. DC electrical conductivity was measured using the Van der Pauw method. Complex permittivity and AC electrical conductivity of respective silicone composites were calculated from the measured scattering parameters. The relationships between structure, electrical properties and shielding efficiency were studied. It was found that 2 mm-thick silicone composites of polypyrrole nanotubes and nanobelts shield almost 80% of incident radiation in the C-band at very low loading of conductive filler in the silicone (5% w/w). Resulting lightweight and flexible polypyrrole composites exhibit promising properties for shielding of electromagnetic interference in sensitive biological and electronic systems.
A sedimentation-stable magnetorheological (MR) polishing slurry on the basis of ferrofluid, iron particles, Al2O3, and clay nanofiller in the form of sepiolite intended for MR polishing has been designed, prepared, and its polishing efficiency verified. Added clay substantially improved sedimentation stability of the slurry, decreasing its sedimentation rate to a quarter of its original value (1.8 to 0.45 mg s−1) while otherwise maintaining its good abrasive properties. The magnetisation curve measurement proved that designed slurry is soft magnetic material with no hysteresis, and its further suitability for MR polishing was confirmed by its magnetorheology namely in the quadratically increased yield stress due to the effect of applied magnetic field (0 to 600 kA m−1). The efficiency of the MR polishing process was tested on the flat samples of injection-moulded polyamide and verified by surface roughness/3D texture measurement. The resulting new composition of the MR polishing slurry exhibits a long-term stable system with a wide application window in the MR polishing process.
This paper presents a methodology for accurately gauging the true plane wave shielding effectiveness of composite polymer materials via rectangular waveguides. Since the wave propagation of the waveguides is not in the form of plane wave patterns, it is necessary to post-process the S-parameters for the measured data of the waveguide lines to obtain such patterns and ascertain the effectiveness of true plane wave shielding. The authors propose two different methods to achieve this. The first applies simple renormalization of S-parameters, where reference impedance is changed from the value for the waveguide to that for free space, which ensures good accuracy of shielding effectiveness with a small degree of discontinuity across the range of frequencies. The other relies on rigorous extraction of the composite materials’ effective permittivity and permeability ascertained from rectangular waveguides; afterward, plane wave shielding effectiveness is calculated analytically and gives very high accuracy. Both procedures assume the given samples are isotropic in character. We validated the accuracy of the methodologies by conducting tests on a set of synthetic samples of 2 mm thickness with unit permittivity and variable conductivity and on a dielectric material of known permittivity (FR4 laminate). The applicability of both methods was further proven by analyzing the isotropic composite materials, a process involving the use of iron particles embedded in a dielectric matrix. The synthetic samples and an FR4 material were tested to check the accuracy of the methods. Based on numerical studies and measurements, we concluded that materials with a shielding effectiveness of up to 25 dB could be measured at a maximum amplitude error of 1 dB to 3dB to a frequency of 18 GHz, depending on the relative permittivity of the material; hence, the first method was suitable for approximation purposes. For maximal accuracy, the second method typically demonstrated an amplitude error of below 0.5 dB to the same frequency across the entire range.
The design of a unipole and a dual band F-shaped antenna was conducted to find the best parameters of prepared antenna. Antenna radiator part is fully made of polymer and nonmetal base composite. Thermoplastic polyurethane (PU) was chosen as a matrix and multi-wall carbon nanotubes (MWCNT) as an electrical conductive filler, which creates conductive network. The use of the composite for the antenna has the advantage in simple preparation through dip coating technique. Minor disadvantage is the usage of solvent for composite preparation. Composite structure was used for radiator part of antenna. The antenna operates in 2.45 and 5.18 GHz frequency bands. DC conductivity of our PU/MWCNT composite is about 160 S/m. With this material, a unipole and a dual band F antenna were realized on 2 mm thick polypropylene substrate. Both antenna designs were also simulated using finite integration technique in the frequency domain (FI-FD). Measurements and full wave simulations of S11 of the antenna showed good agreement between measurements and simulations. Except for S11, the gain and radiation pattern of the antennas were measured and simulated. Maximum gain of the designed unipole antenna is around −10.0 and −5.5 dBi for 2.45 and 5.18 GHz frequency bands, respectively. The manufactured antennas are intended for application in wearable electronics, which can be used to monitor various activities such as walking, sleeping, heart rate or food consumption.