23 June 2020 in The Journal of Physical Chemistry C
19 November 2018 in ACS Applied Materials & Interfaces
21 July 2024 in Acta Materialia
12 April 2021 in npj Materials Degradation
To understand the atomistic phenomenon behind initial oxidation processes, we have studied the nanoscale evolution of oxide growth prior to the formation of a complete layer on a Ni–15 wt%Cr(100) alloy surface using scanning tunneling microscopy/spectroscopy (STM/STS). At the onset of oxidation, a NiO superlattice forms oxide wedges across the step edges, eventually growing across the terraces. The completion of the NiO layer is followed by nucleation of the next layer, which always commences at the groove site of the superlattice. The Cr-oxide formation initiates as disk-shaped oxide particles early in the oxidation process, which Monte Carlo simulations reveal are likely caused by Cr clustering across the alloy surface. Upon further oxidation, a Cr(100)-p(2 × 2)O reconstructed surface is observed, indicating phase separation of Cr predicates the formation of the passive Cr-oxide film. The STS results vary across the oxide–alloy interface and between each oxide, providing greater insight into the origins of electronic heterogeneity and their effect on oxide growth. Using these data, we propose an oxidation model that highlights the growth of partial oxide layers on Ni–Cr(100) alloys within the pre-Cabrera–Mott regime.
8 April 2020 in The Journal of Physical Chemistry C
1 June 2022 in Journal of the Electrochemical Society
The high temperature oxidation of alloys is most often considered within the continuum framework developed by C. Wagner. We argue that in order to make progress in understanding exclusive scale formation, one needs to examine the atomic-scale kinetic processes that today are amenable to a variety of experimental, computational and theoretical approaches. In our discussion, we suggest that there is an analogy between the kinetic processes required for exclusive scale formation and thin film layer-by-layer growth. In both cases, the magnitude of the Ehrlich-Schwoebel barrier sets an effective length scale for growth, that if too large, results in three-dimensional rather than lateral island or oxide growth. In this event, exclusive scale formation can only occur if there is a sufficiently large density of oxide nucleation events at the surface of the alloy. We suggest that a suitably identified, dilute alloy component, could serve as a “surfactant” that segregates to the surface and is capable of enhancing the nucleation density.