29 September 2026 in SERIES CHEMISTRY AND TECHNOLOGY
The conversion of renewable biomass waste into porous carbon materials is a promising approach for both efficient waste valorization and the development of environmentally sustainable electrode materials for modern electrochemical energystorage systems. Food waste, particularly orange peel, is of considerable interest as an abundant, renewable, and carbon-rich precursor. This study aimed to synthesize porous carbon materials from orange peel waste and to determine the effects of carbonization and chemical activation temperatures on their structural, elemental, and electrochemical properties. Porous carbon materials were prepared using a two-step process consisting of pre-carbonization followed by chemical activation. Carbonization was performed at 500, 600, and 700 °C, while activation was conducted at 700, 800, and 900 °C. The morphology and elemental composition of the resulting materials were characterized using scanning electron microscopy (SEM) and energy-dispersive X-ray spectroscopy (EDX), respectively, while their carbon structure was investigated by Raman spectroscopy. The electrochemical characteristics and specific capacitance of the prepared electrode materials were also evaluated. SEM analysis revealed that increasing the activation temperature promoted the development of a heterogeneous and well-developed porous structure. EDX analysis confirmed carbon as the predominant element (83–90 wt%), with an oxygen content of 10–14 wt% and a small amount of residual potassium. Raman spectroscopy demonstrated that the carbon structure varied depending on the synthesis conditions. Among the investigated materials, OPA500/700 exhibited the best electrochemical performance, delivering a specific capacitance of 367.5 F g-1 at 0.1 A g-1 and 259.6 F g-1 at 2 A g-1, corresponding to retention of more than 70% of the initial value. The results demonstrate that orange peel waste is a promising, readily available, and renewable precursor for producing high-capacitance porous carbon electrodes for supercapacitor applications.
30 September 2026 in Reports of the NAS RK
This study examined the feasibility of recycling wood waste to produce organosolv lignin suitable as a precursor for carbon fibers. Mixed wood waste, pine, and elm sawdust were used as feedstock. Lignin was isolated using an organosolv method with a mixture of formic and acetic acids, which reduced the use of aggressive reagents and facilitated environmentally friendly biomass processing. The structural, morphological, and thermal properties of the resulting lignin samples were analyzed using scanning electron microscopy, infrared spectroscopy, nuclear magnetic resonance spectroscopy, thermogravimetric analysis, and Raman spectroscopy. The isolated lignin contained aromatic, phenolic, hydroxyl, methoxyl, and methyl functional groups. Nuclear magnetic resonance spectroscopy revealed a predominance of syringyl structural fragments over guaiacyl ones, indicating favorable thermal stability for subsequent carbonization. Composite fibers were fabricated from the resulting lignin using polyacrylonitrile as the electrospinning polymer. The influence of the spinning solution composition and heat treatment conditions on the fiber morphology and structure was studied. A lignin to polyacrylonitrile ratio of 30:70 proved optimal, ensuring the production of continuous, defect-free fibers with an average diameter of approximately 97 nm. After carbonization at 800 °C under a nitrogen atmosphere, carbon nanofibers with an average diameter of approximately 47 nm and a developed porous structure were obtained. These results demonstrate the potential of organosolv lignin obtained from wood waste as a renewable precursor for carbon nanofibers and electrode materials for energy storage systems. The carbonized fibers exhibited a developed specific surface area of 549.7 m2/g, while the sample carbonized at 800 °C showed the highest electrochemical performance, with a specific capacitance of 136.4 F/g for supercapacitors and a discharge capacity of 797 mAh/g for lithium-ion batteries.