1 February 2018 in Medical Engineering & Physics
Collagen hydrogels have been used ubiquitously as engineering biomaterials with a biphasic network of fibrillar collagen and aqueous-filled voids that contribute to a complex, compressible, and nonlinear mechanical behavior - not well captured within the infinitesimal strain theory. In this study, type-I collagen, processed from a bovine corium, was fabricated into disks at 2, 3, and 4% (w/w) and exposed to 0, 105, 106, and 107 microjoules of ultraviolet light or enzymatic degradation via matrix metalloproteinase-2. Fully hydrated gels were subjected to unconfined, aqueous, compression testing with experimental data modeled within a continuum mechanics framework by employing the uncommon Blatz-Ko material model for porous elastic materials and a nonlinear form of the Poisson's ratio. From the Generalized form, the Special Blatz-Ko, compressible Neo-Hookean, and incompressible Mooney-Rivlin models were derived and the best-fit material parameters reported for each. The average root-mean-squared (RMS) error for the General (RMS = 0.13 ± 0.07) and Special Blatz-Ko (RMS = 0.13 ± 0.07) were lower than the Neo-Hookean (RMS = 0.23 ± 0.10) and Mooney-Rivlin (RMS = 0.18 ± 0.08) models. We conclude that, with a single fitted-parameter, the Special Blatz-Ko sufficiently captured the salient features of collagen hydrogel compression over most examined formulations and treatments.
10 August 2018 in PLOS ONE
The prevalence of diverse animal models as surrogates for human vascular pathologies necessitate a comprehensive understanding of the differences that exist between species. Comparative passive mechanics are presented here for the common carotid arteries taken from bovine, porcine, ovine, leporine, murine-rat, and murine-mouse specimens. Data is generated using a scalable biaxial mechanical testing device following consistent circumferential (pressure-diameter) and axial (force-length) testing protocols. The structural mechanical response of carotids under equivalent loading, quantified by the deformed inner radius, deformed wall thickness, lumen area compliance and axial force, varies significantly among species but generally follows allometric scaling. Conversely, descriptors of the local mechanical response within the deformed arterial wall, including mean circumferential stress, mid-wall circumferential stretch, and mean axial stress, are relatively consistent across species. Unlike the larger animals studied, the diameter distensibility curves of murine specimens are non-monotonic and have a significantly higher value at 100 mmHg. Taken together, our results provide baseline structural and mechanical information for carotid arteries across a broad range of common animal models.
1 January 2019 in Theranostics
Background: Abdominal aortic aneurysms (AAA) are characterized by a progressive disruption and weakening of the extracellular matrix (ECM) leading to dilation of the aorta which can be fatal if not treated. Current diagnostic imaging modalities provides little insight on the varying degree of ECM degeneration that precedes rupture in AAAs. Targeted delivery of contrast agents such as gold nanoparticles (GNPs) that bind to degraded matrix could prove useful when combined with computed tomography (CT) to provide a non-invasive surrogate marker of AAA rupture potential.
4 November 2022 in Acta Biomaterialia
29 July 2020 in Annals of Biomedical Engineering
18 February 2020 in Computer Methods in Biomechanics and Biomedical Engineering
To measure the inhomogeneous 3D-strain fields present during inflation-extension testing of physiologically submerged micro-aneurysms, a Stereo Digital Image Correlation (StereoDIC) microscopy system is developed that revolves 15° stereo-angle cameras around a centrally-mounted target. Calibration is performed using submerged dot patterns and system accuracy verified using strain and deformation analyses for rigid body motions of speckle-patterned, micro-aneurysmal surrogates. In terms of the Green-Lagrange strain tensor and the 3D displacement fields, the results are stable even after 120 minutes, with maxima in both strain bias and strain standard deviation less than 2E-03 for all components, and micron-level displacement standard deviation.