An improved methodology of the Zr specimen preparation was developed which allows fabrication of stable Zr nanotips suitable for FIM and AP applications. Initial oxidation of the Zr surface was studied on a Zr nanotip by FIM and on a polycrystalline Zr foil by XPS, both at low oxygen pressure (10(-8)-10(-7)mbar). The XPS data reveal that in a first, fast stage of oxidation, a Zr suboxide interlayer is formed which contains three suboxide components (Zr(+1), Zr(+2) and Zr(+3)) and is located between the Zr surface and a stoichiometric ZrO2 overlayer that grows in a second, slow oxidation stage. The sole suboxide layer has been observed for the first time at very early states of the oxidation (oxygen exposure ≤ 4L). The Ne(+) FIM observations are in accord with a two stage process of Zr oxide formation.
It is well documented that different surface structures of catalytically active metals may exhibit different catalytic properties. This is typically examined by comparing the catalytic activities and/or selectivities of various well-defined smooth and stepped/kinked single crystal surfaces. Here we report the direct observation of the heterogeneity of active polycrystalline surfaces under reaction conditions, which is manifested by multifrequential oscillations during hydrogen oxidation over rhodium, imaged in situ by photoemission electron microscopy. Each specific surface structure, i.e. the crystallographically different µm-sized domains of rhodium, exhibits an individual spiral pattern and oscillation frequency, despite the global diffusional coupling of the surface reaction. This reaction behavior is attributed to the ability of stepped surfaces of high-Miller-index domains to facilitate the formation of subsurface oxygen, serving as feedback mechanism of the observed oscillations. The current experimental findings, backed by microkinetic modeling, may open an alternative approach towards addressing the structure-sensitivity of heterogeneous surfaces.
The catalytic H2 oxidation reaction on stepped Rh surfaces in the 10−6 mbar pressure range was studied in situ on individual high-Miller-index domains of a polycrystalline Rh foil by PEEM (photoemission electron microscopy) and on a Rh nanotip by FIM/FEM (field-ion/field-emission microscopy). The activity, particularly the tolerance to poisoning by oxygen, was found to strongly depend on the density of steps and defects, as well as on the size of the catalytically active surfaces. Graphical Abstract
Spatially- and component-resolved kinetic measurements and resulting phase diagrams for CO oxidation on a model catalyst consisting of Pd powder agglomerates supported by a polycrystalline Pt foil are reported. The kinetic data for the micrometer-sized Pt(100) and Pt(110) domains and for the different Pd powder agglomerates of similar dimensions were obtained by local analysis of PEEM video-sequences recorded in situ during the ongoing CO oxidation reaction. Individual domains of the supporting Pt foil as well as the µm-sized Pd powder agglomerates behave in the combined Pdpowder/Ptfoil sample independently from each other with respect to CO oxidation, at least in the 10−5 mbar pressure range. The propagating reaction fronts move within grain boundaries for Pt domains and also remain confined to the Pd agglomerates.
5 February 2026 in Journal of Materials Chemistry C
Upon EUV irradiation, n -butyltin–oxo cages release butene, butane and octane with an initial quantum yield of 5 Sn–C bond breaks per absorbed photon (92 eV). To render the resist film insoluble only 2 Sn–C bonds (on average) need to be broken.