Efforts to meet regulations ensuring the safety of lithium-ion battery (LIB) modules in electric vehicles are currently limited in their ability to provide sufficient safe escape times in the event of thermal runaway (TR). Thermal runaway occurs when the heat generation of a battery module exceeds its heat removal capacity, leading to a rapid increase in temperature and uncontrolled heat release. To address this issue, this study focuses on evaluating the cascading thermal failure characteristics of six-cell LIB modules under an air environment in an experimental combustion chamber. Sensors are strategically placed at advantageous locations to capture changes in various characteristic parameters, including LIB temperature, module voltage, module mass, and the concentrations of venting gases in the combustion chamber. Analysis of the variations in these characteristic parameters over time aims to identify effective signals that can predict thermal failure conditions with a maximum warning time. The results demonstrate that monitoring LIB temperature provides the shortest advance warning of TR propagation within the module. However, module voltage measurements offer a warning that is approximately 2% earlier on average. On the other hand, measurements of the module mass and concentrations of venting gases in the combustion chamber allow for warnings of thermal failure that are, on average, approximately 2 min earlier than those based solely on LIB temperature. These findings can serve as guidance for improving the safety of LIBs, enhancing the reliability of fault detection systems, and exceeding the safe escape time requirements set by current global regulations.
With the widespread application of lithium-ion batteries (LIBs) energy storage stations in high-altitude areas, the impact of ambient pressure on battery thermal runaway (TR) behavior and venting flow characteristics have aroused wide research attention. This paper conducts a lateral heating experiment on 280 Ah lithium iron phosphate batteries (LFPs) and proposes a method for testing battery internal pressure using an embedded pressure sensor. This paper analyzes the battery characteristic temperature, internal pressure, chamber pressure, and gas components under different chamber pressures. The experiment is carried out in a N2 atmosphere using a 1000 L insulated chamber. At 40 kPa, the battery experiences two instances of venting, with a corresponding peak in temperature on the battery’s side of 136.3 °C and 302.8 °C, and gas generation rates of 0.14 mol/s and 0.09 mol/s, respectively. The research results indicate that changes in chamber pressure significantly affect the center temperature of the battery side (Ts), the center temperature of the chamber (Tc), the opening time of the safety valve (topen), the triggering time of TR (tTR), the time difference (Δt), venting velocity, gas composition, and flammable limits. However, the internal pressure and gas content of the battery are apparently unaffected. Considering the TR characteristics mentioned above, a safety assessment method is proposed to evaluate the TR behavior and gas hazard of the battery. The results indicate that the risk at 40 kPa is much higher than the other three chamber pressures. This study provides theoretical references for the safe use and early warning of energy storage LIBs in high-altitude areas.
Trigger selection underpins thermal runaway (TR) and thermal propagation (TP) testing of lithium-ion batteries, yet its influence on the TR response is rarely quantified, and data for a cell with manganese-based composite cathode (MCC) material are scarce. Here, a fully charged 130 Ah prismatic cell using MCC was driven into TR by high-frequency electromagnetic induction heating and by lateral plate heating in identical fixtures, and each response was resolved into four stages. A 12-s induction pulse initiated TR from a local nucleus: flame ejection followed venting by 9 s, the trigger-point temperature peaked at 682.6 °C, and the voltage collapsed in two stages with a ~3.0-V, ~14-s plateau, the signature of an expanding local short circuit. Lateral heating required 273 s of whole-cell preheating and produced a faster, hotter event: a jet flame ~20 s after venting, whole-cell involvement within 10.4 s, a 775.4 °C peak, and a single-stage ~20-s collapse. Induction heating thus provides rapid, position-selectable initiation with minimal additional energy input, which is well suited to propagation testing, whereas standard-compliant lateral heating represents external-fire abuse; these results provide the first cell-level reference data for MCC thermal runaway, quantify how the triggering method alone alters the TR response, and identify the voltage-collapse morphology as a diagnostic of the initiation mode.