This study aimed to investigate the impact of mesa geometry on the light output characteristics of AlGaN-based 275 nm deep ultraviolet light-emitting diodes (DUV-LEDs). By dividing the original single-junction mesa into four parts and connecting them serially (four-in-one), high-voltage (HV) DUV-LEDs with rectangular, hexagonal, circular, triangular, and square submesas were realized, achieving significant enhancement of the light output power (LOP) and wall-plug efficiency (WPE). The LOP of HV DUV-LEDs with hexagonal submesas has been promoted substantially compared to that of the original DUV-LEDs. Among the investigated five different types of submesas, hexagonal-type HV DUV-LEDs can achieve the highest LOP and WPE due to the higher sidewall light extraction. Furthermore, it is also demonstrated that pulse current driving can reduce the self-heating effect of HV DUV-LEDs.
By using microscopic hyperspectral imaging, the inhomogeneous electroluminescence (EL) across the mesa of blue vertical micro-LEDs has been investigated. The sidewall emission dominates the EL of micro-LEDs under higher current injections and that bright circular light emission from the sidewall region possesses larger peak energy due to the strain relaxation. The multi-channel radiative recombination leads to the high-energy peaks in the EL spectra of the inner and dim regions of mesa. The photons, which are generated in the inner region of mesa and transported to sidewall after experiencing multiple reflections, act as the indispensable component for sidewall emissions. This work emphasizes the importance of spatially resolved spectral characterization in revealing the mechanisms of light emission from sidewall of micro-LEDs.
This study delves into the degradation mechanism of AlGaN-based UV-C light-emitting diodes (LEDs) subjected to continuous current stress while maintaining a constant heat sink temperature over a 500-hour duration. Utilizing Raman spectroscopy, we observe the relaxation of strain at various stages of degradation. This is exemplified by the blue shift of the ${\text {E}_{{2}}}^{\text {H}}$ phonon peak from the P-GaN layer of AlGaN-based LEDs, measured from different orientations: back, front, and side views, throughout each degradation phase. Raman spectroscopy allows us to comprehensively explore the relaxation of stress specifically under the P-metal of the AlGaN-based UVC LEDs, while the N-metal remains unchanged. This comprehensive investigation sheds light on the intricate degradation mechanism of UV-C LEDs, providing valuable insights into their performance under prolonged stress conditions.
3 August 2023 in IEEE Photonics Technology Letters
AlGaN-based UVC LEDs have encountered a problem of low reverse Electro-Static Discharge (ESD) and low light efficiency due to the high Al composition in their epitaxial structure, which results in low reliability and lifetime degradation. In this study, a reverse diode (ESD device) was added to the device fabrication of the AlGaN-based flip-chip UVC LED to improve the negative ESD capability. By optimizing the design of the ESD protection diode and the N contact, the negative ESD capability can be significantly increased from −150V to −1800V, effectively solving the problem of weak ESD in AlGaN-based UVC LEDs. Additionally, the Light Output Power (LOP) and Wall-Plug Efficiency (WPE) can be increased by 10-18%.
27 September 2024 in IEEE Transactions on Electron Devices
This study delves into the intricate behaviors of degradation in AlGaN-based UV-C light-emitting diodes (LEDs) undergoing constant current stress and maintaining a constant heat sink temperature over a 500-h period. Employing 2-D cathodoluminescence (CL) at each degradation stage, we meticulously analyze the emissions from the multiple quantum wells (MQWs) layer and the N-AlGaN layer. The inclusion of peak wavelength mapping images and intensity distribution pseudo-color images adds depth to our understanding of defect generation and the decline of intensity across different layers throughout the degradation process. Complementing this analysis, the utilization of a focused ion beam and scanning electron microscope (FIB/SEM) allows us to visually inspect defects and observe the deterioration of the Cr/Al layer of the P-metal after 48 h of degradation. The results from CL emission align seamlessly with SEM images, offering a comprehensive visual methodology to pinpoint defect locations and analyze the failure mechanisms of ultraviolet-C (UVC) LEDs.